bomma cullet

So, John Croucher tells me that the Bomma cullet is in from the Czech republic. They tested it in his Penland Class and he said it's dead on Sp87. So that is a good place to start. He did not comment on it beyond that.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #2  
Old 04-27-2019, 05:09 PM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 158
Shawn Everette is on a distinguished road
Supersacks were supposed to arrive this week. Any idea if they filled a pot or were just doing compatibility testing?

I'd be surprised of Penland did a full switch, they've been die hard Spruce for a while. Plus there's nothing like driving down the road for your glass.
Reply With Quote
  #3  
Old 04-27-2019, 06:35 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,023
Pete VanderLaan is on a distinguished road
I'm not saying that Penland switched at all. As a color rod maker, I'm sure John had an interest in the statistics. He was teaching the polarimeter and this would be a great example. My photos show small bags.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #4  
Old 04-27-2019, 10:04 PM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 158
Shawn Everette is on a distinguished road
whoa, got a hold of the actual bags, I wants the info!!!
Reply With Quote
  #5  
Old 04-28-2019, 07:41 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,023
Pete VanderLaan is on a distinguished road
the photos came from Charlie to me by email.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #6  
Old 04-28-2019, 08:42 AM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 158
Shawn Everette is on a distinguished road
Sounds like selective Beta testing, they picked a good standard bearer.
Reply With Quote
  #7  
Old 04-28-2019, 09:31 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,023
Pete VanderLaan is on a distinguished road
John's comments to me were solely based on the polarimetry. He has a lot invested in fitting the glasses being made. Spectrum simply ignored the elephant in the room (SP87) and it would seem that Oceanside will do that as well. Maybe Nic at Penland has gotten to use the cullet, I'm simply unaware of it.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #8  
Old 04-29-2019, 09:49 AM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 158
Shawn Everette is on a distinguished road
Spectrum and Oceanside probably ignored 87 because they're making too much money off fused glass and didn't see the need for the effort. Other than the limited Spruce run their only real competition was Cristalica, which had issues of its own. Enough people were buying it, guilty, so why change.

That may come back to haunt Oceanside if Bomma bodes well and has any type of capacity. The price discrepancy certainly isn't going to persuade me into a dusty glass that eats my furnace. What Oceanside possibly has in the plans may be better, but they're getting beat to the punch. The opacity of information certainly hasn't helped anything, the only updates I ever see are about the plate glass.
Reply With Quote
  #9  
Old 04-30-2019, 09:00 AM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 158
Shawn Everette is on a distinguished road
Gonna leave this here. Martin's quote is hilarious.
Reply With Quote
  #10  
Old 04-30-2019, 10:19 AM
James Burts James Burts is offline
Registered User
 
Join Date: Jul 2014
Location: Raleigh, NC
Posts: 40
James Burts is on a distinguished road
I was at the Penland class with John Croucher. Between John and Tom Littleton, they'd gotten their hands on a handful of pieces of the cullet and made up trident seals to test the compatibility between the Bomma cullet and the SP87 that Penland melts in their clear furnace.

As John indicated to Pete, the polarimeter showed the Bomma cullet to be right on for compatibility with Spruce Pine batch. With them only having 5-10 pieces of the Bomma cullet, we obviously didn't have enough material to be able to make any observations on the working qualities of the glass. That sort of information will have to come once people get a real quantity of the glass on hand to test with.
Reply With Quote
  #11  
Old 04-30-2019, 10:48 AM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 158
Shawn Everette is on a distinguished road
Janecky is probably one of the main people I'd trust for high praise of quality and workability. Might go to others in terms of what it's doing to your furnace. The verdict should be out fairly soon, should be stateside by now, but don't know who'll get it first. My order should be in around June, but I won't be really melting it til August or September.
Reply With Quote
  #12  
Old 05-01-2019, 08:18 PM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,678
Jordan Kube is on a distinguished road
Spectrum was right on, Bomma was right on. Old and new Cristalica were about half a point off from each other and around a point high. Kugler was also a point high. The Spectrum was the only one that worked nice in the torch. It was really a great glass formula. It may have been based on Spruce Pine at some point in the beginning but it ended up being much different in the end.
__________________
WWUD? Think for yourself.
Reply With Quote
  #13  
Old 05-02-2019, 06:19 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,023
Pete VanderLaan is on a distinguished road
In Harvey's words from many decades back "Now we have to throw it to the kids and see what they do with it."

It's such shiny promising stuff. Don't drop it.
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 02:52 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.