Sugar glass

I want to make a big pot of sugar glass to practice gathering when the melter is off. I’m sure poor gathering is at the root of most of my problems. I don’t have a good mental picture of the dynamics of the process.
So I boiled up 5kg of sugar and water on the stove (when my wife was out) and kept going to evaporate the water. Jim McKelvey’s book says to take it up to 338oF for realistic glass like viscosity.
Well, I got to 280oF and the bubbles turned to foam with crystals in! I then realised I’d forgotten to put the cream of tartar in but it was too late anyhow. The whole lot suddenly doubled in volume, recrystallised and started to burn. What a mess!
Does anyone have any experience with this stuff? 338oF seems too high and what is cream of tarter doing in there?
Reply With Quote
  #2  
Old 05-02-2019, 11:36 AM
Charles Friedman Charles Friedman is offline
Registered User
 
Join Date: Apr 2002
Location: Seattle Wa
Posts: 580
Charles Friedman is on a distinguished road
Use honey instead. Going from warm to colder. Use a chop-stick or drinking straw to gather with. The colder the honey the bigger the gathers. Use a small bowl as the crucible.
__________________
"Glass will save the world from ourselfs" CharlesF
Reply With Quote
  #3  
Old 05-02-2019, 04:47 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,250
Pete VanderLaan is on a distinguished road
I've never tried it. It strikes me as being an unlikely way to learn much about gathering. I know at Steuben they taught new workers to gather miscible oil before they ever let them near open pots. Steuben was never really big on gathering conventionally anyways.
Maybe STP in a cold container with something that sticks to STP, but Sugar glass? Really? Or, a pot of real glass in a small electric kiln.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #4  
Old 05-02-2019, 05:19 PM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is offline
PotatoFish
 
Join Date: Jan 2007
Location: Charlotte, NC
Posts: 2,092
Greg Vriethoff is on a distinguished road
Sugar blowing is a different animal. The material is stiffened first before being pulled, and manipulated by hand. There isn't any "gathering" as is done with glass blowing.

A friend of mine did this, and discovered how differently the materials behaves. Search the archives for more info.

I think Charlie's suggestion for an analog is the closest you'll get.
__________________
"Technique is just a means of arriving at a statement." - Jackson Pollack
Reply With Quote
  #5  
Old 05-02-2019, 11:11 PM
Charles Friedman Charles Friedman is offline
Registered User
 
Join Date: Apr 2002
Location: Seattle Wa
Posts: 580
Charles Friedman is on a distinguished road
I forgot to say...place one bowl of honey in hot water and other in crushed ice water. You can even make a cut out of your furnace door with sill. This way you can have a sideways look at your gathering and see what is really going on.
__________________
"Glass will save the world from ourselfs" CharlesF
Reply With Quote
  #6  
Old 05-03-2019, 02:30 AM
rodman gilder miller rodman gilder miller is offline
Registered User
 
Join Date: Aug 2014
Location: seattle
Posts: 68
rodman gilder miller is on a distinguished road
Sucrose glucose and fructose....I think that the real key is the ratio between glucose and fructose. That ratio determines when things go crystalline. In the stores, sugar is sucrose. Add a bit of acid and sucrose breaks down to glucose and fructose. Honey is almost any ratio between the two, dependent upon the species of the flowers' nectar. High fructose is what is usually heralded as the best for "blowing" sugar.

But "blowing" sugar is not very similar to "blowing" glass. A number of years ago, at a GAS conference in Seattle, I arranged for a demo of sugar blowing. It was a disappointment: not many blowers showed up and although the pastry chief was more than good, it really seemed of little relevance to blowing glass.
__________________
You have to dance with the glass
Reply With Quote
  #7  
Old 05-03-2019, 10:08 AM
Rich Samuel's Avatar
Rich Samuel Rich Samuel is offline
Registered User
 
Join Date: Apr 2002
Location: Seattle, WA
Posts: 2,475
Rich Samuel is on a distinguished road
The one of the Chinese guy is the most impressive.

https://www.google.com/search?q=blow...hrome&ie=UTF-8
Reply With Quote
  #8  
Old 05-03-2019, 11:43 AM
Art Freas Art Freas is offline
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 558
Art Freas is on a distinguished road
But the key question is - Did you get it cleaned up before she got back...
Reply With Quote
  #9  
Old 05-03-2019, 12:41 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,537
Eben Horton is on a distinguished road
Offer to help a local glass blower for free.
Buy him or her lunch, brush his or her dog,
Bring beer for the end of the day, sweep the floor..
There’s your gathering practice.
__________________
<eben epoiese>
Reply With Quote
  #10  
Old 05-03-2019, 02:26 PM
Eric Trulson Eric Trulson is online now
Young Turk
 
Join Date: Sep 2014
Location: Boston
Posts: 113
Eric Trulson is on a distinguished road
Quote:
Originally Posted by Eben Horton View Post
Offer to help a local glass blower for free.
Buy him or her lunch, brush his or her dog,
Bring beer for the end of the day, sweep the floor..
There’s your gathering practice.
Seconding this. If you can assist another glassblower, especially one who's doing production work rather than large sculptural pieces, odds are you'll get a whole lot of practice taking first gathers quickly, and some verbal feedback on each gather (whether that feedback is obscenity-laden or not depends on the glassblower)
Reply With Quote
  #11  
Old 05-03-2019, 02:55 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,250
Pete VanderLaan is on a distinguished road
I've noticed that bringing a bottle of a nice single malt helps too.
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 10:07 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.