Controller

I was running my annealer with a partlow 1166. It died on me. I have a Watlow F4 and wanted to run my annealer with it. I had my electrician wire it up and things turned on but the contact points didn't click. The contact points still are good as far as I have tested. Anyone have suggestions or a affordable replacement for the partlow 1166
Reply With Quote
  #2  
Old 03-04-2020, 05:33 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,022
Pete VanderLaan is on a distinguished road
Charlie Correll seems to have a lot of partlows. A call there might be worth it.

Otherwise, I am beginning to think the entire crop is worth shit compared to the older ones.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 03-04-2020, 05:42 PM
Eric Trulson Eric Trulson is offline
Young Turk
 
Join Date: Sep 2014
Location: Stanwood, WA
Posts: 137
Eric Trulson is on a distinguished road
My two go-to brands for annealer controllers are Aubers or SOLOs.

They both strike a good balance between value (prices range from $50-$150) and reliability. I have used them on several kilns & ovens and have never run into issues, although I'd probably go a little more upmarket if I was buying a controller for a furnace.

Aubers are a little funnier to use, you set temperatures digit-by-digit instead of changing things a degree at a time like most controllers. Not too bad once you get used to it though. SOLOs handle similarly to most other controllers.
Reply With Quote
  #4  
Old 03-04-2020, 06:08 PM
Art Freas Art Freas is offline
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 665
Art Freas is on a distinguished road
Sounds like the controller output isn't correct for the relay. When I went to the Bartlett for my one annealer I had to change the relay as the input was different. I am still in my first year with the bartletts.

1) Love the number of programs.
2) Love how easy they are to program.
3) It is great having the phone app to check the annealer.
4) It is handy to be able to download the 30 second by 30 second view of actual and target temps.
5) Wish they ramped a bit faster when you open the door.
6) Wish they had an honest soak step.
7) They program by rate and temp not time. Would be nice to have a time and target option.
Reply With Quote
  #5  
Old 03-04-2020, 07:31 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,022
Pete VanderLaan is on a distinguished road
Give me a straight shot lining up these aubers and I'll pull the trigger on them in a heartbeat.
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 11:11 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.