Is anyone using a white flourine.

If anybody is using a white fluorine Glass I have a customer i can pass to you. Call me 216-533-2116 mike
Reply With Quote
  #2  
Old 11-06-2017, 06:18 PM
George Tessman George Tessman is offline
Registered User
 
Join Date: Jun 2004
Location: Highland, IN
Posts: 240
George Tessman is on a distinguished road
if you are. I could use some cullet if it fits 96. Have a 4 pot electric color furnace. Looking for a milk white.
Reply With Quote
  #3  
Old 11-06-2017, 11:02 PM
Mike Kaplan Mike Kaplan is offline
Registered User
 
Join Date: Apr 2002
Location: cleveland ohio
Posts: 231
Mike Kaplan is on a distinguished road
I have been told it is very dangerous to use so I am trying to avoid it. Is that the consensus with the board here?
Reply With Quote
  #4  
Old 11-07-2017, 12:01 AM
George Tessman George Tessman is offline
Registered User
 
Join Date: Jun 2004
Location: Highland, IN
Posts: 240
George Tessman is on a distinguished road
I've heard the same thing . But at my age and good ventilation not much of a concern for me anymore . I just want A good strong white that I can dip a hot gather. When I was making my own batch I loved my Fenton white. I have a dead on 96 milk white formula but I just don't want to mix batch anymore . So I'm using Spruce Pine . And while the clarity is not as good as the old batch I used to make myself it's convenient and does a nice job . I do hate buying white rod at such high price and I miss having a pot to dip on. I do know that when you first open the furnace of milk white you don't want to be breathing it in right off the bat . But @52 I don't really care anymore LOL .
Reply With Quote
  #5  
Old 11-07-2017, 07:02 AM
Eben Horton Eben Horton is online now
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,604
Eben Horton is on a distinguished road
George does not care. George wants to blownglass!

I like it.
Reply With Quote
  #6  
Old 11-07-2017, 07:29 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,663
Pete VanderLaan is on a distinguished road
George will fry his electrical elements if he puts a fluorine in the pots. If you think it no longer matters at 52, I'd reconsider that.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #7  
Old 11-07-2017, 09:18 AM
Eben Horton Eben Horton is online now
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,604
Eben Horton is on a distinguished road
Quote:
Originally Posted by Pete VanderLaan View Post
George will fry his electrical elements if he puts a fluorine in the pots. If you think it no longer matters at 52, I'd reconsider that.
I wonder if one couldn’t make a sealed element inside quartz tubing. Considering flourines melt so low.
Reply With Quote
  #8  
Old 11-07-2017, 10:05 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,663
Pete VanderLaan is on a distinguished road
Fluorine would still attack the quartz. I think anything that can isolate the element from the gas would help. The white is not much of an issue to melt. Doing Cad sel stuff is more problematic. Cad sulfide always resisted complete melting, always from the cadmium compound side. Drawn from the pot at 200 F it looked a lot like crabs legs. It did melt in eventually and resisting turning it up to do so was a fine tightrope to walk. Too hot, the pot dissolved. Too cold, hard to get the melt just right.

I think the furnaces which are essentially muffle furnaces work best with a seal around the top of the pot at the door. Then, the elements are isolated. At that point the heat has to come through the pot walls and you are back to what Durk described with Anti''s melt problems. But it's still better.

Ideally, I'd melt fluorines with gas. After all those years of the moly, I confess it's really nice to be back to serious horsepower from propane. Nat gas would be even nicer.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #9  
Old 11-07-2017, 10:16 AM
Eben Horton Eben Horton is online now
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,604
Eben Horton is on a distinguished road
Quote:
Originally Posted by Pete VanderLaan View Post
Fluorine would still attack the quartz. I think anything that can isolate the element from the gas would help. The white is not much of an issue to melt. Doing Cad sel stuff is more problematic. Cad sulfide always resisted complete melting, always from the cadmium compound side. Drawn from the pot at 200 F it looked a lot like crabs legs. It did melt in eventually and resisting turning it up to do so was a fine tightrope to walk. Too hot, the pot dissolved. Too cold, hard to get the melt just right.

I think the furnaces which are essentially muffle furnaces work best with a seal around the top of the pot at the door. Then, the elements are isolated. At that point the heat has to come through the pot walls and you are back to what Durk described with Anti''s melt problems. But it's still better.

Ideally, I'd melt fluorines with gas. After all those years of the moly, I confess it's really nice to be back to serious horsepower from propane. Nat gas would be even nicer.
I converted to Nat gas 6 years ago... what a clean burning flame. I see a difference in my melts.
Reply With Quote
  #10  
Old 11-07-2017, 11:14 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,663
Pete VanderLaan is on a distinguished road
Propane is quite interesting to watch burning. It has all these yellow flares in the combustion. Nat gas doesn't do that. Propane really makes clinkers as well. I find them in my BASO value output.
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 06:09 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.