  #1  
Old 09-21-2018, 12:10 PM
Chris Lowry Chris Lowry is offline
Registered User
 
Join Date: Oct 2003
Posts: 252
Chris Lowry is on a distinguished road
Hxtal

So is hxtal good with glass to steel?
Reply With Quote
  #2  
Old 09-21-2018, 12:30 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,748
Pete VanderLaan is on a distinguished road
I have never bonded glass to steel but I have done hxtal to aluminum on a number of occasions. Once, I dropped a piece bonded like that and it indeed broke but the piece did not break at the joint, it broke up about an inch from it.
Just have the surface clean and try to make the joint right around 100F. It will need clean up with acetone at about 24 hours. Wait longer at your own peril.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 09-21-2018, 12:49 PM
Chris Lowry Chris Lowry is offline
Registered User
 
Join Date: Oct 2003
Posts: 252
Chris Lowry is on a distinguished road
I was thinking stainless but aluminum might work. I guess Iíll do a test.
Reply With Quote
  #4  
Old 09-21-2018, 01:13 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,748
Pete VanderLaan is on a distinguished road
the point there was that the glass was not as strong as the hxtal joint.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #5  
Old 09-21-2018, 01:50 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,448
Eben Horton is on a distinguished road
I think that the only time you would have to worry is with quick temp changes related to being outside. If the work is going inside it should be totally fine. The COE of steel is much much less than soda lime glass.
__________________
<eben epoiese>
Reply With Quote
  #6  
Old 09-21-2018, 02:02 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,748
Pete VanderLaan is on a distinguished road
I failed to mention that the piece had been out in the weather in winter colorado.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #7  
Old 09-21-2018, 02:06 PM
Art Freas Art Freas is offline
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 523
Art Freas is on a distinguished road
Is there a reference anywhere that would give the rough linear expansion of glass to steel, aluminum, .....
Reply With Quote
  #8  
Old 09-21-2018, 02:39 PM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is offline
PotatoFish
 
Join Date: Jan 2007
Location: Charlotte, NC
Posts: 2,021
Greg Vriethoff is on a distinguished road
Here's one.

Don't know how precise it is, or helpful.
__________________
"Technique is just a means of arriving at a statement." - Jackson Pollack
Reply With Quote
  #9  
Old 09-21-2018, 02:51 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,748
Pete VanderLaan is on a distinguished road
It shows plate glass around 3.3, steel at 7.5 and aluminum at about 13. I think the issue is over what distance and standard is applied. Aluminum is clearly the highest value. Much would depend on the area being covered .

In glass, the ASTM standard is expanding from 19.1C to 300C over a 4.000 inch test rod. So, you can do that math. If the joint was 2 inches in our soft glass, it would be 96/2 ten thousandths. You would want to take into account the fact that the steel is expanding as well to determine what kind of strain to expect. My non scientific observation with aluminum ( expanding at twice the steel specs) did not cause fracture at the joint. What usually actually is important in stuff like this is surface preparation and that is inevitably where joint failure occurs and I have seen it more times than I can count in glass on glass even with the same formulation. I have never seen a hxtal joint fail in the same way as I've seen UV adhesives fail. In UV, sometimes the joint simply peels away.

Don't use windex. Don't use 70% isopropyl. Pure Xylene in a 90% isopropyl solution gives some tooth to the venture. Don't breathe the xylene.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #10  
Old 09-21-2018, 06:04 PM
Peter Bowles Peter Bowles is offline
Registered User
 
Join Date: Sep 2002
Location: Breadalbane, Tasmania
Posts: 628
Peter Bowles is on a distinguished road
I've always thought the units of expansion bizarrely funny.
Perhaps they were made by a delegation of Liberians, Americans, Germans and Indians at a scientific conference in Myanmar.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 04:36 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.