Just curious how much power people use... always wondered how smaller furnaces run.

We run a Stadelman furnace 400lbs, melt Spruce Pine once a week and use around 9400KWH in 31 days. That is strictly the furnace.

On a side note electricity is around $.33 a KWH here.
Reply With Quote
  #2  
Old 09-30-2018, 12:30 PM
Mark Rosenbaum's Avatar
Mark Rosenbaum Mark Rosenbaum is offline
Registered User
 
Join Date: Apr 2002
Location: New Orleans, LA
Posts: 1,001
Mark Rosenbaum is on a distinguished road
Hard to tell unless you have separate meters. I think my AC takes as much power as my furnace! :O
Reply With Quote
  #3  
Old 10-01-2018, 10:03 AM
David Hopman David Hopman is online now
Registered User
 
Join Date: Mar 2009
Location: Sutter Creek, CA
Posts: 429
David Hopman is on a distinguished road
I'm using an average of 7000 kwh an hour for my entire building, running a 230 lb Electroglass furnace, electric glory hole, 1 annealer, charging once every 3 weeks and blowing 2 days a week.

Shop closed, only electricity use is the furnace: 170 kwh per day.
Blowing day, all equipment and gallery lighting running: 370 kwh per day
Shop open, not blowing: 190 kwh per day.
Average cost: .23 per kwh.

Last edited by David Hopman; 10-01-2018 at 10:08 AM.
Reply With Quote
  #4  
Old 10-01-2018, 06:20 PM
Max Epstein Max Epstein is online now
Registered User
 
Join Date: Sep 2016
Location: Tallahassee, FL
Posts: 250
Max Epstein is on a distinguished road
Damn, maybe I should get on the electric bandwagon. My electric rates are cheaaaap.

.06 per kWh
.38-.70 per CCF nat gas (not sure, haven't fired up yet)
Reply With Quote
  #5  
Old 10-01-2018, 06:49 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,748
Pete VanderLaan is on a distinguished road
Look at the entire bill, not just the KWH per hr. Currently, in NH my costs of power are lower than the delivery charge. Take the bottom line.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #6  
Old 10-22-2018, 11:45 PM
Max Epstein Max Epstein is online now
Registered User
 
Join Date: Sep 2016
Location: Tallahassee, FL
Posts: 250
Max Epstein is on a distinguished road
Customer Charge: $37.86
Energy Charge - kWh at $0.05556
Fuel & Purch Pwr - kWh at $0.035
+tax

So... worst case 170 kWh x 31 x $0.0556 + $37.86

...is $330.


I don't envy your power bill Chris.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 05:35 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.