Fuming

Has anyone found that atmospheric conditions can change your fuming. I can use the same mixture and get great results and at other times I have a harder time. The only difference I can think of is atmospheric.
Same colors, same process, same mixture with the same freshness of the mixture.
Reply With Quote
  #2  
Old 10-01-2018, 06:48 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,748
Pete VanderLaan is on a distinguished road
fuming with stannous chloride in reduction as opposed to oxidation indeed produce quite different results.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 10-01-2018, 06:52 PM
George Tessman George Tessman is offline
Registered User
 
Join Date: Jun 2004
Location: Highland, IN
Posts: 233
George Tessman is on a distinguished road
When I say atmospheric I am referring to the weather. Some days it goes great other days it is just a struggle.
Reply With Quote
  #4  
Old 10-01-2018, 07:06 PM
Ron Mynatt Ron Mynatt is offline
Registered User
 
Join Date: Apr 2008
Location: Springdale Arkansas
Posts: 148
Ron Mynatt is on a distinguished road
A question I would ask is how hot is your object you are spraying too hot or too cold will give different effects?Also how long you keep in in the spray pattern.I have found the first few seconds on a blue silver will give me a electric blue silver finish next comes a golden finish then a purple then a green.It seems if I go beyond that ,the color starts to go bad.That may because the object has gotten too cold.If you reheat and then go back you will be might be able to get another finish but those 4 colors work for me.
Reply With Quote
  #5  
Old 10-02-2018, 05:11 PM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is offline
PotatoFish
 
Join Date: Jan 2007
Location: Charlotte, NC
Posts: 2,021
Greg Vriethoff is on a distinguished road
This is such a touchy process, and there are too many variables to nail it down to any one thing. If you're trying to achieve consistent results, good luck. Down this road lies madness.

As to your specific question, my position is that atmospheric conditions can, and do affect glass making processes. Barometric pressure sure does.
__________________
"Technique is just a means of arriving at a statement." - Jackson Pollack
Reply With Quote
  #6  
Old 10-02-2018, 06:15 PM
Larry Cazes Larry Cazes is offline
Registered User
 
Join Date: Feb 2006
Location: San Jose, CA
Posts: 884
Larry Cazes is on a distinguished road
I fume borosilicate. Yes atmospheric humidity does play a role.
Reply With Quote
  #7  
Old 10-02-2018, 06:16 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,748
Pete VanderLaan is on a distinguished road
15 F affects it
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 05:30 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.