Peach silver opal

Does anybody know what the potential of this bar is? I've never used it but heard great things. If anyone has suggestions or photos of what it looks like I would very much appreciate to see them.
Thanks
Drew Hine
Attached Images
File Type: jpg IMG_4161.jpg (25.5 KB, 62 views)
Reply With Quote
  #2  
Old 05-04-2017, 01:26 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 19,443
Pete VanderLaan is on a distinguished road
I made that.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 05-04-2017, 02:47 PM
Dan Vanantwerp Dan Vanantwerp is offline
Registered User
 
Join Date: Apr 2017
Location: Bozeman, MT
Posts: 116
Dan Vanantwerp is on a distinguished road
Post #14:

http://talk.craftweb.com/showthread....ight=calcedony
Reply With Quote
  #4  
Old 05-04-2017, 07:24 PM
Scott Mitchell Scott Mitchell is offline
Registered User
 
Join Date: Jun 2013
Location: Springfield, VA
Posts: 25
Scott Mitchell is on a distinguished road
Silver Colors

Quote:
Originally Posted by Dan Vanantwerp View Post
I have some of that silver peach too. And to dredge up something from the other thread. How do you strike it? Maybe I'm not using enough.

The one piece I've made from the stuff is nice enough, but the character isn't there. The transmitted color is a nice light amber (and could probably use a nice white backing). The reflected color is a milky light yellow. Is it supposed to be uncased?

I also have some of the silver blue. It's acted similarly: Kind of a dark aqua reflected, with a pale green transmitted. It's a bit more opaque than the peach.
Reply With Quote
  #5  
Old 05-04-2017, 07:27 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 19,443
Pete VanderLaan is on a distinguished road
Use more. Keep it pretty cold.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #6  
Old 05-04-2017, 08:39 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,001
Eben Horton is on a distinguished road
As a rule of thumb, I use 4 times as much bar when I use silver opals or calcedony colors.

You will never get anything to look as good as it does in bar form though...
Reply With Quote
  #7  
Old 05-05-2017, 11:13 AM
Scott Novota's Avatar
Scott Novota Scott Novota is offline
AbbyNormal User
 
Join Date: Jan 2004
Location: Pensacola Florida
Posts: 2,079
Scott Novota is on a distinguished road
I am with Eben here on how much you use. If it thins out it turns a sort of dull pink without swirls...think it is all over the place swirl wise. Whatever you think is enough double it.

If I made a pint beer tumbler I would use about an and inch and half.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 08:07 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2018, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.