Pringle Teetor is on a distinguished road
Bubbles between cane

I have finally been doing some cane work (hard to do solar for the first time in a few years. Iím rolling up cane on a collar and for some reason yesterday I was getting bubbles between the canes here and there for the first time. Once I rolled up and went into heat, some canes became unfused in the middle. Was it not fused enough? Was my reheat too long? Any thoughts?
Reply With Quote
  #2  
Old 02-22-2018, 02:48 PM
David Russell David Russell is offline
Registered User
 
Join Date: Jul 2008
Location: South Carolina
Posts: 198
David Russell is on a distinguished road
When freshly rolled up (before you pinch the bottom) you can use your Jacks along the outside (sometimes at an angle) to help pinch all the canes together. This may be redundant but could help you out.
Reply With Quote
  #3  
Old 02-23-2018, 05:24 PM
Peter Bowles Peter Bowles is offline
Registered User
 
Join Date: Sep 2002
Location: Breadalbane, Tasmania
Posts: 626
Peter Bowles is on a distinguished road
Turning the plate a couple of times between heats and gently squeezing the canes together before rolling up will prevent bubbles. Just allow for the marginal loss in circumference when you make your collar.

Some do, some don't, but I'm an advocate of preheating everything to around 600 before going into the glory hole. It helps in that you have to do far less heating in the glory hole where the heat distribution across the plate is very uneven.
Reply With Quote
  #4  
Old 02-23-2018, 05:28 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,507
Pete VanderLaan is on a distinguished road
sounds dumb, but when was the last time those canes were really clean?
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #5  
Old 02-23-2018, 07:39 PM
David Patchen's Avatar
David Patchen David Patchen is offline
Registered User
 
Join Date: Sep 2005
Location: San Francisco, CA
Posts: 1,861
David Patchen is on a distinguished road
Quote:
Originally Posted by Pringle Teetor View Post
I was getting bubbles between the canes here and there
If you weren't gathering over them and they got bubbly as you heated them, I agree with Pete's suspicions--there must be some dirt/baking soda/ash/etc between the canes. That's the only thing I could imagine that would create bubbles between them.

Quote:
Originally Posted by Pringle Teetor View Post
Once I rolled up and went into heat, some canes became unfused in the middle. Was it not fused enough? Was my reheat too long? Any thoughts?
Definitely not well enough fused if they came apart in the hole. When picking up on a collar I have my assistant get them pretty toasty through 2-3 heats. They should have glowing, rounded ends but not melted flat--that's way too hot. Once they're flexible, we usually give it a good squeeze or two so they're well stuck together. Squeeze them too cold and you get pick-up sticks. Roll them up immediately after your assistant comes out of the gh while they're still flexible (but not floppy) and you're good. If you pick them up after your assistant has been out of the gh too long, they may have cooled and will crack and separate as you roll them up--that's a disaster. If they're still hot and moving after you pick up, you can quickly close them and brush them. If they're feeling stiff after rolling up, take a short flash, then close them and brush them. Once they're closed and brushed, then take a short heat and use your jacks on the outside (vertically like you're putting in a neckline) to squeeze them all together. Then they should be quite stable and ready for whatever you want to do.

Do it a few dozen/hundred times and you'll get a good feel for the heats.
Reply With Quote
  #6  
Old 02-24-2018, 08:56 AM
Pringle Teetor's Avatar
Pringle Teetor Pringle Teetor is offline
Registered User
 
Join Date: Jul 2003
Location: Chapel Hill, NC
Posts: 632
Pringle Teetor is on a distinguished road
Cleaning them as they go on the plate. Probably not squeezing enough on the last two where I had the problems. I do the jacks around the roll up but I think I waited too long on the ones in question. These are great tips so thanks!
Reply With Quote
  #7  
Old 02-24-2018, 09:22 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,507
Pete VanderLaan is on a distinguished road
I spent my first real time making cane with Gary Beecham at Pilchuck in 76 I recall. As quickly as he made cane, he put it in PVC tubes. It could not get dirty or dusty that way. Fine glass powder on a cane can cause bubbles. Cleaning cane after it has been out in the studio for a while is problematic.

Bubbles caused otherwise would suggest that the cane was not the same diameter yet was laid on the ferro quite close but also not necessarily straight.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #8  
Old 02-24-2018, 05:56 PM
Peter Bowles Peter Bowles is offline
Registered User
 
Join Date: Sep 2002
Location: Breadalbane, Tasmania
Posts: 626
Peter Bowles is on a distinguished road
Not likely, but also a possibility, is that if you have any residual texture on the cane from marvering before running the cane out you can trap micro bubbles between, particularly if you are making twisted cane.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 04:49 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2018, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.