CraftWEB Hot Glass Talk  

Go Back   CraftWEB Hot Glass Talk > Hot Glass > General Hot Glass Discussion

Reply
 
Thread Tools Display Modes
  #1  
Old 02-22-2018, 09:49 AM
Ralph Laborde Ralph Laborde is offline
Registered User
 
Join Date: Jan 2010
Location: San Antonio, TX
Posts: 83
Ralph Laborde is on a distinguished road
G-Tec Gas Booster 30 for bench torch

Does anyone use a natural gas pressure intensifier for a bench fluffy torch? We're thinking of getting one, setting up multiple bench torches and doing away with the hand MAPP bottle torches and propane tanks.
Reply With Quote
  #2  
Old 02-22-2018, 05:07 PM
Charles Friedman Charles Friedman is offline
Registered User
 
Join Date: Apr 2002
Location: Seattle Wa
Posts: 544
Charles Friedman is on a distinguished road
It should be fine. just mind your PSI requirements for the said torch.


Get yours self a Oxygen Generator while you are at it. Charles
__________________
"Glass will save the world from ourselfs" CharlesF
Reply With Quote
  #3  
Old 02-24-2018, 03:53 PM
Max Epstein Max Epstein is offline
Registered User
 
Join Date: Sep 2016
Location: Tallahassee, FL
Posts: 189
Max Epstein is on a distinguished road
Unhappy

I saw that very model posted on a Boro group on Facebook!

I couldn't believe it! I've been trying to find something like this for years to no avail. Is this the solution to the mobile glass rig?

http://www.gas-tec.com/cylinders.html
*130 cubic feet cylinder, 25-500psi, up to 500schf (1schf = 1020BTUs, so 500schf= 510,000 BTU?)
*will not freeze like propane
*can be transported laying down, and has "been shot with a bullet near an open flame" and not exploded.

The Giberson 255 burner is 150k BTU. I am having trouble finding the psi requirements, but I know it is low pressure.

Soooo.... is there anything preventing me from running "Gloria" on this for mobile gigs? Is this a dream come true...? How long would 130 cubic feet last? Not long, right? I suck with propane/gas conversions. Maybe the dream ain't quite the reality here.
Reply With Quote
  #4  
Old 02-24-2018, 04:13 PM
Max Epstein Max Epstein is offline
Registered User
 
Join Date: Sep 2016
Location: Tallahassee, FL
Posts: 189
Max Epstein is on a distinguished road
So, if I'm reading this right, 100 ccf of natural gas = 100,000btu = 1 therm.

So that means this 130 ccf cylinder is about equal to 1 gallon propane = 1 therm.

Or, 1 hour of operation. thought I was onto something here for a second. All the other solutions are giant mostly carbon fibre DOT tanks for big trucks which is easily $5,000-20,000.
Reply With Quote
  #5  
Old 02-26-2018, 05:20 PM
Jordan Kube Jordan Kube is online now
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,617
Jordan Kube is on a distinguished road
You're doing kind of an apples to oranges comparison. The natural gas is a gas and the propane is in liquid form. A 20lb BBQ propane tank gets you about 138 cuft of propane gas. You would have to liquefy your natural gas to get the same performance as propane.
__________________
WWUD? Think for yourself.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 04:31 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2018, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.