Question DIY Blowing molds

I've been asked to make several identical (or nearly so) blown glass flames. I'd like to help, but I'm stumped.
I don't have access to a woodworker. I do have access to clay & plaster. I am open to any ideas or suggestions of how to make a mold.
Reply With Quote
  #2  
Old 02-18-2018, 11:13 AM
Dan Vanantwerp Dan Vanantwerp is offline
Registered User
 
Join Date: Apr 2017
Location: Bozeman, MT
Posts: 246
Dan Vanantwerp is on a distinguished road
Both Glass Notes and Ed Schmidt's books have DIY sections on this.

There was also a huge list of retired Fenton molds that became available and were posted some time ago. May have been a flame in there, but besides the recent posting in the classified section I don't know what is still available, if anything. They were pricey but did get positive reviews from those who picked up a few.
__________________
My furnace setting: 2112
Reply With Quote
  #3  
Old 02-19-2018, 12:32 AM
Gail Obendorf Gail Obendorf is offline
Registered User
 
Join Date: Jul 2016
Location: Oregon
Posts: 7
Gail Obendorf is on a distinguished road
Thanks Dan, I will look into it
Reply With Quote
  #4  
Old 02-19-2018, 03:02 AM
Mike McCain
Guest
 
Posts: n/a
Carve graphite blocks with Dremel tools and core drill bits. Buy hinges. Wear protection.
Reply With Quote
  #5  
Old 02-23-2018, 10:57 PM
Gail Obendorf Gail Obendorf is offline
Registered User
 
Join Date: Jul 2016
Location: Oregon
Posts: 7
Gail Obendorf is on a distinguished road
Thanks Mike Not sure where to find graphite blocks, but I'm hoping that Google will be able to help me out
Reply With Quote
  #6  
Old 02-24-2018, 08:42 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,507
Pete VanderLaan is on a distinguished road
I used HGL Carbon in the past. High quality stuff.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #7  
Old 02-24-2018, 10:24 AM
Scott Mitchell Scott Mitchell is offline
Registered User
 
Join Date: Jun 2013
Location: Springfield, VA
Posts: 29
Scott Mitchell is on a distinguished road
Is there a school nearby that does metal casting (Technical, Engineering, or Art school)? Perhaps you could get a mold into it when they do an aluminum pour.
Reply With Quote
  #8  
Old 02-24-2018, 01:25 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,379
Eben Horton is on a distinguished road
I had a commission once to reproduce some chandelier flame globes. I made a rubber mold of a flame, and then another rubber of that mold to give a rubber positive. Then I placed that inside a plastic painters pail and filled that with wax on its side. I then removed that wax and carefully made another wax up to the line I had made of the first wax. I then carved some fred flintstone looking hinges in it that accepted a 1/4 rod and sent them to a foundery. A lot of work but I was compensated nicely.

Ransom and randolf sells a good rubber
__________________
<eben epoiese>
Reply With Quote
  #9  
Old 02-26-2018, 08:59 AM
Art Freas Art Freas is offline
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 504
Art Freas is on a distinguished road
how do you put hinges on the graphite? Just screws?
Reply With Quote
  #10  
Old 02-26-2018, 06:12 PM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,633
Jordan Kube is on a distinguished road
Art, you typically want to use something with a coarse thread and treat it nice.
__________________
WWUD? Think for yourself.
Reply With Quote
  #11  
Old 02-26-2018, 07:31 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,379
Eben Horton is on a distinguished road
Quote:
Originally Posted by Jordan Kube View Post
Art, you typically want to use something with a coarse thread and treat it nice.
And use a tap and die.
__________________
<eben epoiese>
Reply With Quote
  #12  
Old 02-27-2018, 12:54 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,507
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Jordan Kube View Post
Art, you typically want to use something with a coarse thread and treat it nice.
****
I have a carbon cone attached to my airline gun for puffing out a piece. It's tapped and you do have to treat it nice.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #13  
Old 02-27-2018, 01:13 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,747
Franklin Sankar is on a distinguished road
Eben so you made a wax negative. Why did you not use the rubber positive.
What did the foundry do with the wax mold you sent them?
Franklin
Reply With Quote
  #14  
Old 02-27-2018, 01:21 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,379
Eben Horton is on a distinguished road
Quote:
Originally Posted by Franklin Sankar View Post
Eben so you made a wax negative. Why did you not use the rubber positive.
What did the foundry do with the wax mold you sent them?
Franklin
The wax gets invested in a ceramic shell mold and then they burn out the wax.


You make a rubber and then a wax because you can make more waxes down the road if you have to, plus its easier to make a rubber mold of a wax than it is to make a rubber of a rubber.
__________________
<eben epoiese>
Reply With Quote
  #15  
Old 02-27-2018, 01:30 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,747
Franklin Sankar is on a distinguished road
Ok so you made a ceramic object not a mold to cast glass.
I thought you were making a mold.
Thanks
Franklin
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 04:29 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2018, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.