Pete VanderLaan is on a distinguished road
500 belts

So, when I used to make the cut forms, I worked the inside edge with 1/2x24" belts on the dyna file. I'm going back to using those tools again and find my old supplier sold out about five years ago. I did find a new one for 180 belt and 320 belts but I have not been able to find a 500 grit Aluminum oxide. I used to see that 3M made them. Any ideas?
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #2  
Old 03-09-2018, 05:47 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,379
Eben Horton is on a distinguished road
My 500 belts are simply worn out 300 belts. I know... I know....but.....
__________________
<eben epoiese>
Reply With Quote
  #3  
Old 03-09-2018, 06:07 PM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,633
Jordan Kube is on a distinguished road
https://www.amazon.com/Inch-Silicon-...00DH0ESGM?th=1

They got 400 and 600 grit. I just use the worn out 400's.
__________________
WWUD? Think for yourself.
Reply With Quote
  #4  
Old 03-09-2018, 06:30 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,507
Pete VanderLaan is on a distinguished road
I can get 320's and that's a good jump from the 180. Going to 400 is too little a jump and I would have to cut every belt by hand from the ones you put out there. I actually have cork belts this size but ten years is a long time to lose track of a market . I still need a 500 1/2 x 24. On the cut forms, it is really the perfect stupid finish. I used to be able to get 9 micron! ( Still have a few!). I'll try cutting my own 600 belts so that was great! Now I need to rebuild a dynafile from 1987. It has no plastic parts.

I am such a dinosaur...

I ran my bigger gloryhole today after a year away. That was really fun.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #5  
Old 03-10-2018, 05:02 PM
Steve Beckwith Steve Beckwith is offline
Registered User
 
Join Date: Feb 2007
Location: Cocoa Beach, Florida
Posts: 87
Steve Beckwith is on a distinguished road
www.supergrit.com. These guys say they make custom belts. I've dealt with them and they were good to me
Reply With Quote
  #6  
Old 04-07-2018, 02:18 AM
neil duman neil duman is offline
Registered User
 
Join Date: May 2015
Location: VA
Posts: 26
neil duman is on a distinguished road
Quote:
Originally Posted by Pete VanderLaan View Post
So, when I used to make the cut forms, I worked the inside edge with 1/2x24" belts on the dyna file. I'm going back to using those tools again and find my old supplier sold out about five years ago. I did find a new one for 180 belt and 320 belts but I have not been able to find a 500 grit Aluminum oxide. I used to see that 3M made them. Any ideas?
I keep forgetting to get my belt suppliers name while at the studio.
They will custom make almost anything if they don't already have it in stock. If you still need them, give me a call monday midday. Memory just keep getting worse and worse.
804 334 8462
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 04:40 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2018, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.