Turning powders into paint

Anyone done this? My experience so far is that CMC/Tylose thickener is like trying to paint with ketchup/catsup. Lol literally using a ketchup dispenser. If you spell it catsup, don't talk to me.
My generation kinda missed Paradise paints, whatta loss. I mean, I got my hands on some and somehow lost it. Lol.
I just tried a 50/50 ratio of powder to Lyndsay Doyle and yeah, you still have to shove it around instead of painting with it, but man I can get great lines with it. Much finer than PP.
Only problem is the oil kinda yellows everything.

Anyone pursuing oil on glass? Or maybe there's a super clear oil you can think of off the cuff, one that burns off clean and clear?

Last edited by Mike McCain; 02-19-2018 at 02:18 AM. Reason: Update?
Reply With Quote
  #2  
Old 02-19-2018, 02:20 AM
Mike McCain
Guest
 
Posts: n/a
Selfish. I wanted this to show up before my response to the diy response.

Last edited by Mike McCain; 02-19-2018 at 02:21 AM. Reason: .4:20 a.m. just to make Pete question me
Reply With Quote
  #3  
Old 02-19-2018, 08:57 AM
Tony Serviente Tony Serviente is offline
Registered User
 
Join Date: Mar 2005
Location: Ithaca, NY
Posts: 155
Tony Serviente is on a distinguished road
What are you trying to do Mike? Paint flat glass and fire I assume?
Reply With Quote
  #4  
Old 02-19-2018, 10:53 AM
Randy Kaltenbach's Avatar
Randy Kaltenbach Randy Kaltenbach is online now
Registered DancingChicken
 
Join Date: Aug 2003
Location: Calgary, Canada
Posts: 951
Randy Kaltenbach is on a distinguished road
I've used gum arabic as a binder with Reusch and similar powders. Thinned with either water, vinegar, or antifreeze. Never tried it with glass powders like Gaffer or Reichenbach.
Reply With Quote
  #5  
Old 02-19-2018, 11:56 AM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is offline
(((0)))
 
Join Date: Jan 2007
Location: Charlotte, NC
Posts: 1,920
Greg Vriethoff is on a distinguished road
You may be in over your head.
__________________
"It's such a fine line between stupid and clever." - David St. Hubbins
Reply With Quote
  #6  
Old 02-19-2018, 12:40 PM
Dan Vanantwerp Dan Vanantwerp is offline
Registered User
 
Join Date: Apr 2017
Location: Bozeman, MT
Posts: 222
Dan Vanantwerp is on a distinguished road
I've used liquid stringer and powdered glass with some success. I even took out a loan and bought some dichro powder to use as accent in some graal pieces. Just have to find the right ratio. I believe the stuff is pretty cheap.
There are also some glass paints you can buy from fusing places that work ok. I like the liquid stringer/powder combo best though...
__________________
My furnace setting: 2112
Reply With Quote
  #7  
Old 02-19-2018, 01:15 PM
Steven O'Day Steven O'Day is offline
Registered User
 
Join Date: Jun 2002
Location: portland oregon
Posts: 282
Steven O'Day is on a distinguished road
Reusche sells a bunch of different mediums. Gum arabic works well but tends to dry quickly.

The main issue with painting with blowing colors is that they are too coarse, they really need to be ground finer to work.

Reusche also sells a line of enamels for hot glass, I haven't tried them and am curious if anyone has experience with them.
Reply With Quote
  #8  
Old 02-19-2018, 04:53 PM
Mike McCain
Guest
 
Posts: n/a
Thanks for the advice.
Reply With Quote
  #9  
Old 02-19-2018, 07:38 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,212
Eben Horton is on a distinguished road
Paradise paints used pine oil I believe
__________________
<eben epoiese>
Reply With Quote
  #10  
Old 02-20-2018, 06:24 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,008
Pete VanderLaan is on a distinguished road
just keep in mind that it won't ever go into solution. You need a far finer ground powder than the color companies will provide, more around the level of German aluminum for explosives.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #11  
Old 02-21-2018, 03:57 AM
Michael Ahlefeldt-Laurvig Michael Ahlefeldt-Laurvig is online now
Registered User
 
Join Date: Apr 2010
Location: Sweden
Posts: 661
Michael Ahlefeldt-Laurvig is on a distinguished road
This is a glass pigment muller
https://goo.gl/images/E3Yg5G
It is used to fine grind pigments and enamels- even commercially bought enamels perform better when they are ground finer. The enamel is mixed with water or oil on a piece of sandblasted plate glass and the muller is moved in a circular motion until desired consistency is reached. I have made several through the years, for stained glass painters and porcelain painters
Reply With Quote
  #12  
Old 02-21-2018, 12:15 PM
Mike McCain
Guest
 
Posts: n/a
I was going to try mortar and pestle, but this seems like a neat way to go. Thanks Michael.
Reply With Quote
  #13  
Old 02-21-2018, 12:34 PM
Michael Ahlefeldt-Laurvig Michael Ahlefeldt-Laurvig is online now
Registered User
 
Join Date: Apr 2010
Location: Sweden
Posts: 661
Michael Ahlefeldt-Laurvig is on a distinguished road
No no, this how its done. Think a couple of teaspoons at the most and 20 min grinding, add water or oil as needed. Arabic gum is also good to make it dry to the glass and stick
Reply With Quote
  #14  
Old 02-21-2018, 01:10 PM
Michael Ahlefeldt-Laurvig Michael Ahlefeldt-Laurvig is online now
Registered User
 
Join Date: Apr 2010
Location: Sweden
Posts: 661
Michael Ahlefeldt-Laurvig is on a distinguished road
Bloody hell Pete, can you make aluminum explode? I still want to know how to make good whiskey!
Reply With Quote
  #15  
Old 02-21-2018, 01:44 PM
Charles Friedman Charles Friedman is offline
Registered User
 
Join Date: Apr 2002
Location: Seattle Wa
Posts: 536
Charles Friedman is on a distinguished road
Add some glycerin. It will smooth things out.
__________________
"Glass will save the world from ourselfs" CharlesF
Reply With Quote
  #16  
Old 02-21-2018, 02:41 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,008
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Michael Ahlefeldt-Laurvig View Post
Bloody hell Pete, can you make aluminum explode? I still want to know how to make good whiskey!
********
Aluminum powder was banned for sale in the US for about 8 years after 9/11. My kid used to make stuff that blew stumps using that with potassium per Chlor ate. Straight Clor ate is far more unstable.
I'm talking a fine grade where it just looks like shiny silver paint on your fingers. Profoundly dangerous stuff. You can buy it on Amazon these days in small quantities. It certainly doesn't take much. Most of his loads were 35 grams or less. Don't get confused with charles stuff. glycerine is a serious hydrocarbon and really is dangerous to handle.

He made flash powder as well. That was entertaining. I haven't made any single malts in a while. It's just really time consuming.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #17  
Old 02-21-2018, 04:30 PM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is offline
(((0)))
 
Join Date: Jan 2007
Location: Charlotte, NC
Posts: 1,920
Greg Vriethoff is on a distinguished road
Aluminum dust is quite combustible. The first metal fab shop I worked in in Seattle we had a heavy door/gate thing made out of copper plate with an aluminum support/frame. The guy that was making the aluminum frame was working on a vented table. He'd been dressing (grinding) the finished welds on the same surface, and the dust had built up in the catchment below the table. He went to do some touch-up work, and a spark from the welding ignited the pile of dust below. The added oxygen from the air being pulled into the chamber made things get exciting really fast.

He's really lucky it didn't actually explode.
__________________
"It's such a fine line between stupid and clever." - David St. Hubbins
Reply With Quote
  #18  
Old 02-22-2018, 07:11 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,008
Pete VanderLaan is on a distinguished road
It needs to be really fine , around 9-10 micron. Then watch it.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #19  
Old 02-25-2018, 05:25 AM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,696
Franklin Sankar is on a distinguished road
I assume that you can make your own muller with furnace glass? Or is it something special.
Franklin
Reply With Quote
  #20  
Old 02-26-2018, 01:19 PM
Michael Ahlefeldt-Laurvig Michael Ahlefeldt-Laurvig is online now
Registered User
 
Join Date: Apr 2010
Location: Sweden
Posts: 661
Michael Ahlefeldt-Laurvig is on a distinguished road
Yes, normal glass, any glass
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 10:41 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2018, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.