Ceramic blow-molds?

So I've got a question for the hivemind. Does anybody have experience with attempting to use ceramic blow-molds? (Successfully or not. Even knowing about previous attempts and failures would be helpful)

To the best of my knowledge, the standard blow-mold materials for glass tend to be hardwoods, graphite, and metals (mostly cast-iron). One of the common downsides with all of those materials is the need to start from a solid billet and remove material to form the mold cavity, which tends to push individual mold price fairly high once you account for material cost and CNC machine time.

I'm compelled to try and figure out a good workflow for 3D printing a PLA/foam positive of the form to be blown, casting around it with some type of ceramic to form the actual mold, then burning out the PLA/foam positive to leave the cavity.

Doesn't need to survive for huge production runs, but a single-use mold doesn't solve the problems I'm going after. Ideally, this would be suited for doing small-volume production runs, say around 10-30 pieces before the mold fails. This would be for turn molds only.

The two biggest issues I see are lubrication/cooling (keeping the mold surface cool enough to stop hot glass from sticking to it), and avoiding cracking or thermal shock in the ceramic (minor surface cracking might be fine, but as soon as things shift enough to expose a jagged edge to the glass, that mold is toast). My initial instinct would be to use a fine-grained high-alumina castable with a decently thick wall (1"+), and use a combination of wax and graphite powder for the lubrication.

Any stories of past attempts at this, or thoughts for better approaches?
Reply With Quote
  #2  
Old 09-28-2018, 04:24 PM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,646
Jordan Kube is on a distinguished road
In my travels down the PLA/foam core with ceramic overlay I ran into problems with the clay shrinking and cracking around the form. You would probably want a castable type product with low setting shrinkage.
__________________
WWUD? Think for yourself.
Reply With Quote
  #3  
Old 09-28-2018, 04:28 PM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,646
Jordan Kube is on a distinguished road
Might be best to go from foam or PLA to plaster, then to clay.
__________________
WWUD? Think for yourself.
Reply With Quote
  #4  
Old 09-28-2018, 06:42 PM
Mark Rosenbaum's Avatar
Mark Rosenbaum Mark Rosenbaum is offline
Registered User
 
Join Date: Apr 2002
Location: New Orleans, LA
Posts: 978
Mark Rosenbaum is on a distinguished road
Why not plaster?
Reply With Quote
  #5  
Old 09-28-2018, 09:21 PM
Rosanna Gusler Rosanna Gusler is offline
Registered Fuser
 
Join Date: Mar 2003
Location: Wanchese, NC
Posts: 916
Rosanna Gusler is on a distinguished road
Research quartz inversion temp when thinking about using ceramic.
Reply With Quote
  #6  
Old 09-30-2018, 12:25 AM
Steven O'Day Steven O'Day is offline
Registered User
 
Join Date: Jun 2002
Location: portland oregon
Posts: 301
Steven O'Day is on a distinguished road
If it is a blow mold you will need to be able to remove the glass piece so you should be able to get the PLA out without burning it out. Like Jordan said ceramic would not work because it shrinks as it dries and will crack around the mold.

I would try plaster, make sure the PLA is sprayed with mold release or vaseline.

Metal casters use a material referred to as ceramic shell. It is much tougher but requires a setup to keep it in suspension then it is fired.

Jewelers us a plaster/refractory mix that is more heat resistant than pottery but is more expensive.
Reply With Quote
  #7  
Old 09-30-2018, 01:28 PM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is offline
PotatoFish
 
Join Date: Jan 2007
Location: Charlotte, NC
Posts: 2,007
Greg Vriethoff is on a distinguished road
Ancient blow molds are thought to have been made out of terracotta. If your mold shrinks and/or cracks then the clay body has not been properly fired.

Some blowing with terracotta molds.
__________________
"It's such a fine line between stupid and clever." - David St. Hubbins
Reply With Quote
  #8  
Old 09-30-2018, 02:12 PM
Rich Samuel's Avatar
Rich Samuel Rich Samuel is offline
Registered User
 
Join Date: Apr 2002
Location: Seattle, WA
Posts: 2,402
Rich Samuel is on a distinguished road
Those "bench" rails are wild!
Reply With Quote
  #9  
Old 10-01-2018, 02:53 AM
Peter Bowles Peter Bowles is offline
Registered User
 
Join Date: Sep 2002
Location: Breadalbane, Tasmania
Posts: 627
Peter Bowles is on a distinguished road
I've made one piece, two piece, turn and still molds using all sorts of refractory castables. Often cast into a plywood box to give structure and to allow hinges, handles, latch clamps and wheels to be easily mounted. I lined them all with cork powder and pva. Works fine, no need to overthink this stuff.
Reply With Quote
  #10  
Old 10-01-2018, 03:45 PM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,646
Jordan Kube is on a distinguished road
If you make a refractory blow mold, as Peter suggests, you could burn out the PLA without worrying about release agents, etc. I would still seal the PLA first with some shellac or similar product.
__________________
WWUD? Think for yourself.
Reply With Quote
  #11  
Old 10-01-2018, 04:33 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,399
Eben Horton is on a distinguished road
If the romans did it...you can do it.
__________________
<eben epoiese>
Reply With Quote
  #12  
Old 10-01-2018, 07:39 PM
Peter Bowles Peter Bowles is offline
Registered User
 
Join Date: Sep 2002
Location: Breadalbane, Tasmania
Posts: 627
Peter Bowles is on a distinguished road
Learning to blow nicely into molds is a whole skill set in itself and can challenge your normal ways of setting up bubbles, gathers and timing greatly. Give some real thought to how you intend to finish the work (hot or cold) when you are designing the mold.
One of the secrets of blowing into molds is to go in with the glass as cool as you can get away with - not as hot as you can.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 04:56 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.