Oceanside frit for blowing

Has anyone used the new(?) Oceanside frit? I see they make a green, blue, and black aventurine and that has me curious.

Guessing it would only be compatible with their glass, given that it's based off the old Spectrum formula.
Reply With Quote
  #2  
Old 01-06-2020, 04:20 PM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 459
Shawn Everette is on a distinguished road
I've gotten away with using some spectum(uroboros) in the past with system premium, but yes, it shouldn't actually be compatible with a 96. The blue adventuring is particularly finicky. The other big issue that you're going to run into is that they're also not formulated to be stretched, the colors are "thin" and are really only good for solid work.
Reply With Quote
  #3  
Old 01-06-2020, 09:21 PM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is offline
rEgisturd Spelunker
 
Join Date: Jan 2007
Location: USSA
Posts: 2,144
Greg Vriethoff is on a distinguished road
Aventurine is always a question mark with compatibility. If you can test you should.

All System 96 aventurine was produced at Spectrum's facility. Crushing, packaging, and labeling were done at Uroboros. As I've stated several times in the forums, about 75% of the glass for frit, stringers, noodles, and rods (and other miscellaneous components) were processed at Uroboros from cullet shipped from Spectrum.

The actual bright spot in all of this is with one entity handling the entire manufacturing process there should be more consistency to all products (whatever ends up surviving). I'm skeptical about the blowing nuggets/cullet/whatever surviving.
__________________
I loves Dale gilhooly
Reply With Quote
  #4  
Old 01-06-2020, 11:18 PM
Gabriel Greenlaw Gabriel Greenlaw is offline
Registered User
 
Join Date: Feb 2015
Location: Bay Area, CA
Posts: 11
Gabriel Greenlaw is on a distinguished road
Do you think this is old stock that Oceanside got when they purchased the Spectrum line or are they actually making it themselves now?
Reply With Quote
  #5  
Old 01-06-2020, 11:47 PM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,702
Jordan Kube is on a distinguished road
New stock.
__________________
WWUD? Think for yourself.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 08:29 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.