uv delamination

Hey ya'll. So I'm trying to help out my partner on a restoration project at a museum. She's got an assembled cut and polished piece that is starting to get the tell tale delam ferns growing at the seams. There's an odd oil slick look to part of it, which I haven't come across before. We think that it was bonded with a UV, which I know is not our favorite. Anybody have experience on how long to expect complete failure?
Attached Images
File Type: jpg CON_2018.239_nt_001.jpg (15.3 KB, 59 views)
File Type: jpg CON_2018.239_nt_003.jpg (21.5 KB, 55 views)
File Type: jpg CON_2018.239_nt_005.jpg (32.8 KB, 56 views)
Reply With Quote
  #2  
Old 12-05-2019, 04:14 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,711
Pete VanderLaan is on a distinguished road
Complete failure? It probably won't but it will continue to look worse and worse. The "artifact" or the fern is the result of inadequate exposure to the UV source. The ring may well indicate how flat the two surfaces were at the time of joining them. Newton rings sugggest very close fits.
During the period when I was trying to use UV before abandoning it was that the light source needs to be warmed up. We finallly kept our light under a cardboard box running all day. If you don't warm them up, the filament develops a coating that interfers with the bonding.

I've taken them apart using Methyl Chloride ( Toxic) but it's a lot faster to bite the bullet and saw them, resurfacing everything and this time doing it in Hxtal.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 12-05-2019, 04:44 PM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 518
Shawn Everette is on a distinguished road
Any chance you could manage to properly cure what hasn't started to come apart. Given the dogma of museum conservation disassembly probably isn't happening, certainly not with a saw.
Reply With Quote
  #4  
Old 12-05-2019, 06:59 PM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,706
Jordan Kube is on a distinguished road
Quote:
Originally Posted by Shawn Everette View Post
Any chance you could manage to properly cure what hasn't started to come apart.
My gut feeling says no but that's the easiest place to start. Won't cost anything. If it doesn't work you're still at present condition.

I know it's not your problem but I would recommend they contact the artist and try to work out a remedy. Museums should have museum quality work, which this piece is not at this point. If the artist isn't interested(I'm assuming they are still around) stick it in a box in back and let it fall apart out of public view.
__________________
WWUD? Think for yourself.
Reply With Quote
  #5  
Old 12-05-2019, 10:23 PM
Scott Dunahee's Avatar
Scott Dunahee Scott Dunahee is offline
Registered User
 
Join Date: Apr 2002
Location: Madison, WI
Posts: 640
Scott Dunahee is on a distinguished road
can't you bring it up to temp and burn out the uv glue connections then reassemble after cleaning with hxtal?

Just asking.

BSD
__________________
That's all right. I never expected there to be a blue light special on enlightenment...
Reply With Quote
  #6  
Old 12-06-2019, 12:23 AM
David Patchen's Avatar
David Patchen David Patchen is offline
Registered User
 
Join Date: Sep 2005
Location: San Francisco, CA
Posts: 1,906
David Patchen is on a distinguished road
Quote:
Originally Posted by Scott Dunahee View Post
can't you bring it up to temp and burn out the uv glue connections then reassemble after cleaning with hxtal?
BSD
This is what the artist should do. If he won't, this is what I would do. I've taken pieces off of bases by bringing them up and down through another annealing cycle. The UV turns dark brown and fails. It isn't easy to get off but a super clean razor blade and some acetone should do the trick. Maybe a cork belt and cerium if it's really stubborn. Then re-assemble with hxtal.
Reply With Quote
  #7  
Old 12-05-2019, 06:30 PM
Larry Cazes Larry Cazes is offline
Registered User
 
Join Date: Feb 2006
Location: San Jose, CA
Posts: 958
Larry Cazes is on a distinguished road
Quote:
Originally Posted by Shawn Everette View Post
Anybody have experience on how long to expect complete failure?
Exactly 1 year 3 months and 10 hours. Thats give or take a few seconds of course.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 09:02 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.