Old 06-13-2016, 11:09 AM
Randy Kaltenbach's Avatar
Randy Kaltenbach Randy Kaltenbach is offline
Registered DancingChicken
 
Join Date: Aug 2003
Location: Calgary, Canada
Posts: 973
Randy Kaltenbach is on a distinguished road
So i spoke to a number of folk at GAS Corning who are convinced that Spectrum will continue production. Nobody gave me any details so now i wonder whether they were optimistic, delusional, or "know something". Any thoughts?
Reply With Quote
  #177  
Old 06-13-2016, 11:16 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,072
Pete VanderLaan is on a distinguished road
well, the furnaces are shot. Did you see the nuggets that I had with the stones and other inclusions in them from Spectrum? They were the ones Pringle had gotten in late april. When she complained she was told they met the QC standards. I was told that actually the property was being sold off. Those furnaces won't move.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #178  
Old 06-13-2016, 12:26 PM
Randy Kaltenbach's Avatar
Randy Kaltenbach Randy Kaltenbach is offline
Registered DancingChicken
 
Join Date: Aug 2003
Location: Calgary, Canada
Posts: 973
Randy Kaltenbach is on a distinguished road
Quote:
Originally Posted by Pete VanderLaan View Post
Did you see the nuggets that I had with the stones and other inclusions in them from Spectrum?
Yes, I did see them and thanks for having them at the conference. Many blowers I spoke to seemed to think that that was acceptable, too
Reply With Quote
  #179  
Old 06-13-2016, 12:52 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,072
Pete VanderLaan is on a distinguished road
we have really fallen from grace.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #180  
Old 06-20-2017, 02:26 PM
Mike Kaplan Mike Kaplan is offline
Registered User
 
Join Date: Apr 2002
Location: cleveland ohio
Posts: 217
Mike Kaplan is on a distinguished road
So who has got some cullet for sale?
Reply With Quote
  #181  
Old 06-20-2017, 03:00 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,072
Pete VanderLaan is on a distinguished road
you are in an outdated thread. Spectrum and Spruce Pine both have cullet. The prices have gone up just a smidge.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #182  
Old 06-20-2017, 04:50 PM
Mike Kaplan Mike Kaplan is offline
Registered User
 
Join Date: Apr 2002
Location: cleveland ohio
Posts: 217
Mike Kaplan is on a distinguished road
So who has got some cullet for sale?
Reply With Quote
  #183  
Old 06-20-2017, 05:22 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,072
Pete VanderLaan is on a distinguished road
Spectrum and Spruce Pine
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #184  
Old 06-21-2017, 12:17 AM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is offline
PotatoFish
 
Join Date: Jan 2007
Location: Charlotte, NC
Posts: 2,053
Greg Vriethoff is on a distinguished road
Try here for Spectrum.

Since your profile says you're in Cleveland, I would guess the closest distributor is Ed Hoy's.

Cristalica from Spruce Pine.
__________________
"Technique is just a means of arriving at a statement." - Jackson Pollack
Reply With Quote
  #185  
Old 06-15-2019, 01:00 PM
Mark Rosenbaum's Avatar
Mark Rosenbaum Mark Rosenbaum is offline
Registered User
 
Join Date: Apr 2002
Location: New Orleans, LA
Posts: 1,024
Mark Rosenbaum is on a distinguished road
bringing this thread back around...
It seems like Oceanside is producing cullet again.
They are 96 Studio Nuggets. I assume that this is the old system 96 and not the 2.0. Is that the correct assumption?
on another note....
Pete or someone who has more knowledge than me.... I don't understand where/when a cullet like Crystallica melts does the borax leave the already once-melted glass to eat away furnace refractory. It's not like it is in batch form.... I am not a chemist, and don't pretend to be, so a layman's explanation would be welcome.... TIA
Reply With Quote
  #186  
Old 06-15-2019, 04:07 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,072
Pete VanderLaan is on a distinguished road
Boron gasses off readily, even from cullet and many materials do and can be assessed at micrograms loss per hour. It always goes up with temperature.

My belief about the cullets in particular that we've seen such damage from is that the quick process from batch to barrel leaves the chemical process incomplete and it outgasses once melted the second time. Spectrum was really bad at this. Also, those formulas are not really stable durable glasses. When you want soft low melt, it's achieved at a cost. Couple that with non AZS refractories and you have your answer.
__________________
Where are we going and why am I in this basket?

Last edited by Pete VanderLaan; 06-15-2019 at 05:51 PM. Reason: spelling
Reply With Quote
  #187  
Old 06-15-2019, 04:10 PM
Mark Rosenbaum's Avatar
Mark Rosenbaum Mark Rosenbaum is offline
Registered User
 
Join Date: Apr 2002
Location: New Orleans, LA
Posts: 1,024
Mark Rosenbaum is on a distinguished road
Is it done off-gassing once it is flat?
From what I have read, it is better to melt at a lower temp than to run it up and down like batch.
Reply With Quote
  #188  
Old 06-15-2019, 06:00 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,072
Pete VanderLaan is on a distinguished road
It's rather dependent on the temps you run at. Again, it's not built to be durable and a lot of the problem is right there. They have given you most everything you asked for, low melt.. cheap.. convenient. But I don't think trash glass gets kinder with age. I do after all sell a really fine batch glass thru SP.

When I melt, I'm no longer running a shop that has to have output. You are. I can wait days to see the glass where I want it and you can't. My pot now, at fifteen months still looks brand new. I have all the time in the world as long as you note that isn't very long at all for me.

My biggest worry about the long term is what will happen with this stuff in a number of decades. The glass flowers at Harvard are disintegrating before the curator's eyes. I hate to think that this instant gratification in studio glass is going to yield very little to the big picture. I still view being in the group at Corning to be the best honor I'll ever get. Being put along side glass from 1000AD will shake you should it happen.

I well recognize what a pain in the ass I am to so many here. I'm a two edged sword. I want to see everyone who is blowing off the earth's resources to have done it for a grand reason.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #189  
Old 06-15-2019, 07:40 PM
Mark Rosenbaum's Avatar
Mark Rosenbaum Mark Rosenbaum is offline
Registered User
 
Join Date: Apr 2002
Location: New Orleans, LA
Posts: 1,024
Mark Rosenbaum is on a distinguished road
I am running at 2050 and not going up or down. I only charge in 50 pounds each night in a 400# crucible.... I have clean glass in the morning. This has worked for me, so why change it. My crucible has lasted 2.5 years so far (knock wood).
Yes, I do not have the luxury of waiting for batch to cook out. That extra day to charge and fine will cost me $$$. I melted batch for years and have found that cullet is better suited for my situation....
Pain in the ass??? Hardly. Opinionated, yes, but you are consistent in your love of making your artwork to be the best that you feel it can be.
Reply With Quote
  #190  
Old Yesterday, 08:05 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,072
Pete VanderLaan is on a distinguished road
If it's working for you, I can't see any reasons to change. I think the Bomma cullet will be the best offering seen in some time. It needs to be worked for evaluation. Hopefully it will not have borax in it.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #191  
Old Yesterday, 01:44 PM
Mark Rosenbaum's Avatar
Mark Rosenbaum Mark Rosenbaum is offline
Registered User
 
Join Date: Apr 2002
Location: New Orleans, LA
Posts: 1,024
Mark Rosenbaum is on a distinguished road
Yup, just have to see what the beta testers are saying and what the pricing is.... I just wish that Mark at Olympic would have given me the option for Bomma when I ordered cullet
Reply With Quote
  #192  
Old Yesterday, 07:01 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,072
Pete VanderLaan is on a distinguished road
These guys continue to operate in their own interests, not in yours.
Price will be much higher and will go up I expect. The reason is that it costs more to make decent materials which should be no surprise. The concern? Will supply be exceeded by demand.
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 04:37 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.