Do Gaffer's duro colours contain Pb?

Hey, just wondering if anyone knows if Gaffer's duros contain lead.
I was under the impression that enamels of course do but these duros
do not. Asking because I had some cane where some Se/Cd transparents
went dark after touching white duro underneath. I did not do a layer of
clear in between as I would have with what I was certain would contain
Pb. Cane in question still showed nice colors after first pull (filigrana) and second pull (flat cane), but then seemed to go dark when piece was made with the flat cane. Thanks.
__________________
www.jmbglass.com
instagram.com/joshbernbaum_glass
Reply With Quote
  #2  
Old 10-07-2017, 01:26 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,598
Pete VanderLaan is on a distinguished road
to the best of my knowledge, based on recent conversations with John, they do indeed contain lead. High Alumina makes this goop stiff. The EU has told Murano that in can no longer make the enamel with lead and arsenic they have made for centuries. It's a big deal over there.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 10-07-2017, 03:17 PM
Josh Bernbaum Josh Bernbaum is offline
Registered User
 
Join Date: Feb 2009
Location: Brattleboro, VT
Posts: 582
Josh Bernbaum is on a distinguished road
What are the LEC's of Murano glass like Pete? Are they anywhere near our 96 standard? Curious if they'd be buying bars now if they are no longer able to make their own.
__________________
www.jmbglass.com
instagram.com/joshbernbaum_glass
Reply With Quote
  #4  
Old 10-07-2017, 03:58 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,598
Pete VanderLaan is on a distinguished road
It's quite high. Effetre is between a 100- 104 .
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 03:58 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.