Shut down

I am about to shut my furnace off and rebuild. Looking for opinions i have a thermjet 250 my question is should I pull the head hot or wait till it cools to pull it. Just seeing what experiences people have had. Thank you
Reply With Quote
  #2  
Old 03-25-2020, 01:44 AM
Bill Worcester Bill Worcester is offline
Registered User
 
Join Date: Apr 2009
Location: Maui, HI
Posts: 64
Bill Worcester is on a distinguished road
Is it likely stuck in place?

If you think it will come out easily when cold, leave it in place. If not pull out hot and wrap ceramic part of the burner in flax to cool slowly.
Reply With Quote
  #3  
Old 03-25-2020, 06:50 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,819
Pete VanderLaan is on a distinguished road
spell check strikes again; "Flax".

Frax I suspect. It will burn up linen after all.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #4  
Old 03-25-2020, 08:47 AM
Art Freas Art Freas is offline
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 794
Art Freas is on a distinguished road
Ours came out easy after we were cold. Though it didn't really matter as ours was trashed and needed to be replaced.
Reply With Quote
  #5  
Old 03-25-2020, 12:07 PM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,751
Jordan Kube is on a distinguished road
Don't pull it out hot.
__________________
WWUD? Think for yourself.
Reply With Quote
  #6  
Old 03-25-2020, 07:54 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,883
Eben Horton is on a distinguished road
Quote:
Originally Posted by Jordan Kube View Post
Don't pull it out hot.
Correct. itís only 80% effective in unwanted problems.
__________________
<EBEN EΠOIESEN >
Reply With Quote
  #7  
Old 03-26-2020, 12:28 PM
Art Freas Art Freas is offline
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 794
Art Freas is on a distinguished road
Don't do anything to put it at risk, those things are expensive. We had to replace ours in our rebuild (it was 12 years old).
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 12:03 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.