Diamond bandsaw blades

I searched the archives and spent the day calling around.
I'm looking for a source for 93.5 x 1/4" blades.

The only supplier I have found for this size is Denver glass machinery. I'm sure they don't manufacture the blade themselves. I'm in the middle of a job that requires literally thousands of cuts that can only be achieved using a bandsaw. I will go thru some blades for this job and would love to find a better source with possible multi blade discounts.

Thanks for any help!
Reply With Quote
  #2  
Old 07-31-2013, 05:29 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,609
Pete VanderLaan is on a distinguished road
Did you try North Jersey Diamond?
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 07-31-2013, 10:20 PM
Patrick Casanova Patrick Casanova is offline
Registered User
 
Join Date: Apr 2002
Location: Western Wisconsin
Posts: 289
Patrick Casanova is on a distinguished road
Sky,
I have been pleased with the blades that I have gotten from these folks.

http://www.bandsawbladesdirect.com/b...and-saw-blades
Reply With Quote
  #4  
Old 08-01-2013, 10:20 AM
Sky Campbell's Avatar
Sky Campbell Sky Campbell is offline
Registered User
 
Join Date: May 2002
Location: Gainesville FL
Posts: 1,032
Sky Campbell is on a distinguished road
Thanks

I tried jersey diamond and although they don't normally sell bandsaw blades Mark said he would look into for me. Still it would be weeks out.

Bandsaw direct only sell 1/2" I really need 1/4" for this application.
Reply With Quote
  #5  
Old 08-01-2013, 10:39 AM
George Vidas George Vidas is offline
Registered User
 
Join Date: Jun 2012
Location: Detroit, MI
Posts: 194
George Vidas is on a distinguished road
Are diamond bandsaw blades welded like normal metal/wood bandsaw blades?

Seems like the process would have to be slightly more precise to avoid having a bump or divot at the weld, since the diamond is more continuous and less textured than saw teeth.

But I wonder if there's somewhere that would sell a bunch of 1/4" diamond coil stock, and then you could take it to your local bandsaw guys and have them weld it for you.
Reply With Quote
  #6  
Old 08-01-2013, 12:23 PM
Patrick Casanova Patrick Casanova is offline
Registered User
 
Join Date: Apr 2002
Location: Western Wisconsin
Posts: 289
Patrick Casanova is on a distinguished road
Sky,
I don't know of anyone that makes a 1/4" bandsaw blade. How thick a piece do you need to cut? And how many? I believe most Ring Saws only have a 1.5" throat height, and at that thickness I think it would be really slow going.

George... "some wheels are best left round!"
Reply With Quote
  #7  
Old 08-01-2013, 02:57 PM
Tom Fuhrman Tom Fuhrman is offline
Registered User
 
Join Date: Apr 2002
Location: Lakeland, Florida
Posts: 1,500
Tom Fuhrman is on a distinguished road
have you tried www.kentsupplies.com they list a 94.1" X 1/3" for $146.
Reply With Quote
  #8  
Old 08-01-2013, 05:00 PM
Hugh Jenkins Hugh Jenkins is offline
Registered User
 
Join Date: Sep 2006
Location: Honoka'a, HI
Posts: 1,025
Hugh Jenkins is on a distinguished road
www.ukam.com/diamond_band_saw_blades.htm
__________________
Aloha, Hugh
Reply With Quote
  #9  
Old 08-02-2013, 06:21 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,609
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by George Vidas View Post
Are diamond bandsaw blades welded like normal metal/wood bandsaw blades?

Seems like the process would have to be slightly more precise to avoid having a bump or divot at the weld, since the diamond is more continuous and less textured than saw teeth.

But I wonder if there's somewhere that would sell a bunch of 1/4" diamond coil stock, and then you could take it to your local bandsaw guys and have them weld it for you.
***********
I would be inclined to try to remember that the goal here is to make glass with the limited time we have. It's easy to go off on tangents.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #10  
Old 08-02-2013, 08:52 AM
Tom Fuhrman Tom Fuhrman is offline
Registered User
 
Join Date: Apr 2002
Location: Lakeland, Florida
Posts: 1,500
Tom Fuhrman is on a distinguished road
Quote:
Originally Posted by Pete VanderLaan View Post
***********
I would be inclined to try to remember that the goal here is to make glass with the limited time we have. It's easy to go off on tangents.
That may be true for some but I am certain it has now become more critical just to survive and pay the bills than worrying about making glass. Life has changed for many of us that attempted to do this glass stuff as a full time lifetime endeavor and actually tried to make some "art". Some sell crucibles and some may want to make saw blades. I just want to keep paying my health insurance and avoid the pains that come with getting old. Glass making has become a real luxury.
Reply With Quote
  #11  
Old 08-02-2013, 03:50 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,609
Pete VanderLaan is on a distinguished road
I don't think having diamond saw blades made falls in the survival category. I do think that taking that time and making products that are pretty sure to sell . I think the observation about not rediscovering the wheel is on the money. Time is important and getting to use it blowing glass is even more so.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #12  
Old 08-02-2013, 04:33 PM
Sky Campbell's Avatar
Sky Campbell Sky Campbell is offline
Registered User
 
Join Date: May 2002
Location: Gainesville FL
Posts: 1,032
Sky Campbell is on a distinguished road
Well I ordered a blade from Denver glass. I'll let you know about quality later. It meets my requirements for now. It was $180

George the blades are pre welded then electroplated. It is the only way it works. I wish you could weld them as I have several new blades that are to long or old blades that have one chip in them.


For the record Denver has the blades and Mark from jersey diamond came back with a source for less money but weeks out before they are made.

Tom I tried them no such luck on my size. I considered a small riser block on the throat of the saw but more work that doesn't pay

Hugh I did originally look on there web page and didn't find what I needed. Called them after your post and yes they can but at $230 each I don't know if it's worth the extra dough.

Last edited by Sky Campbell; 09-03-2013 at 02:29 PM. Reason: Where my manners? Big thanks to everyone! I owe you all a beer.
Reply With Quote
  #13  
Old 08-02-2013, 10:11 PM
Doug Randall's Avatar
Doug Randall Doug Randall is offline
Registered User
 
Join Date: Jun 2004
Location: Portland, Oregon
Posts: 114
Doug Randall is on a distinguished road
Kingsley North has a 94" x 1/4" blade that fits the DL 7000 bandsaw. $125. on sale.
__________________
To review my newest book: http://www.blurb.com/bookstore/detail/256039
Reply With Quote
  #14  
Old 08-03-2013, 12:00 AM
Sky Campbell's Avatar
Sky Campbell Sky Campbell is offline
Registered User
 
Join Date: May 2002
Location: Gainesville FL
Posts: 1,032
Sky Campbell is on a distinguished road
Thanks Doug. Even if I knew 94.25" blade would fit I still never would have found it there. Great price I'll order one on Monday and let you know what I think of the quality.

The Denver blade is .020 thick and is listed at 180 grit $179
The Kingsley blade is .026 and listed as 140 to 170 grit sale $125
Normal price of $184

I'm sure anyone selling a blade for a machine and doesn't list it as being American made will be an import. Quality is all over the board and I hate spending money on what may be garbage. That said next time around after these two blades die I'll bite the bullet and spend the extra money with Jersey diamond and see if the price is made up in quality. Mark at Jersey can deliver a blade at the thickness you want with the grit you want. Consistant grit size I'm sure will reduce chip out but maybe the varying size grit will speed up production. I'm lumping this all up as a learning process.
Reply With Quote
  #15  
Old 08-03-2013, 05:30 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,609
Pete VanderLaan is on a distinguished road
The differences are hard to see in the ads. Diamond concentration per sq inch is really important and how the diamond is bonded to the metal- either resin or sinter metal bond. I don't actually know if Jersey makes a band saw blade but if they do you have to check out process either way. Either way it's a very useful thread and I'm going to move it to "classics" since it's such a persisting search.
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is On
Forum Jump


All times are GMT -5. The time now is 05:57 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.