CraftWEB Hot Glass Talk  

Go Back   CraftWEB Hot Glass Talk > Hot Glass > General Hot Glass Discussion

Reply
 
Thread Tools Display Modes
  #1  
Old 04-28-2018, 01:24 PM
Brian Graham's Avatar
Brian Graham Brian Graham is offline
Registered Abuser
 
Join Date: Mar 2004
Location: Canal Fulton - Ohio
Posts: 500
Brian Graham is on a distinguished road
Question on cremains in glass

Ok collective hive...I have a few questions:
What is your earliest recollection of any glass artist placing human ashes into glass to create a memorial piece? Is it the 70's or 80's?

One final related question - What is the earliest company set up to offer this class of goods to market? websites, company name, etc.
__________________
The revolution will not be televised.
Reply With Quote
  #2  
Old 04-28-2018, 09:01 PM
Michael Ahlefeldt-Laurvig Michael Ahlefeldt-Laurvig is offline
Registered User
 
Join Date: Apr 2010
Location: Sweden
Posts: 726
Michael Ahlefeldt-Laurvig is on a distinguished road
I dont know, but why do you want to know?
Reply With Quote
  #3  
Old 04-28-2018, 11:48 PM
Charles Friedman Charles Friedman is offline
Registered User
 
Join Date: Apr 2002
Location: Seattle Wa
Posts: 569
Charles Friedman is on a distinguished road
I was doing a little with clay with glass inlays with ashes, late Sixties early Seventies. Made a bunch of urns with ashes in the glazes.
What's the point?
__________________
"Glass will save the world from ourselfs" CharlesF
Reply With Quote
  #4  
Old 04-29-2018, 07:52 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,101
Pete VanderLaan is on a distinguished road
I would have immediately suspected Rob Adamson.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #5  
Old 04-29-2018, 04:40 PM
Art Freas Art Freas is online now
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 543
Art Freas is on a distinguished road
Wouldn't surprise me to see it in 1800's paperweights but that just a hunch.
Reply With Quote
  #6  
Old 04-29-2018, 06:50 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,101
Pete VanderLaan is on a distinguished road
I'm thinking real reliquaries, not junk rolled in a paperweight.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #7  
Old 04-29-2018, 09:37 PM
Michael Ahlefeldt-Laurvig Michael Ahlefeldt-Laurvig is offline
Registered User
 
Join Date: Apr 2010
Location: Sweden
Posts: 726
Michael Ahlefeldt-Laurvig is on a distinguished road
My guess would be Murano, as soon as they got clear glas figured out
Reply With Quote
  #8  
Old 04-30-2018, 01:13 AM
John Croucher's Avatar
John Croucher John Croucher is offline
Registered User
 
Join Date: Jul 2003
Posts: 60
John Croucher is on a distinguished road
Phosphate opal glasses are thought to have originated in 14th Century Persia and recipes began circulating among German alchemists in the 17th century, including the famous glass maker Johannes Kunckel.

I've always thought it bit bogus that current glass reliquary trade entails just rolling up human ashes into a crude paperweight. In my opinion it's much classier and more appropriate and professional to melt the bone ashes into a bespoke batch along with perhaps a colorant of the family's choice that can add an extra emotional and spiritual element.

On an interesting historical side note one of Kunckel's alchemist contemporaries, Johann Becher, was overawed by the fact that human bones could render glass milky and in his book with the wonderful title "Subterranean Physics" he noted:
Oh, how it should be of custom that I would have friends to serve my dry bones, exhausted of all of life's work, this last of all duties, and transform them into this never changing timeless substance, glass, the softest color of its kind...,the trembling Narcissus' milky reflection, possible to be done in some few hours only. so as to become evidence of God's almighty power on the day of resurrection and illumination".

Becher was reluctant to make the secret known for fear such an awful revelation may lead to its misuse!
Reply With Quote
  #9  
Old 04-30-2018, 09:47 AM
Max Epstein Max Epstein is offline
Registered User
 
Join Date: Sep 2016
Location: Tallahassee, FL
Posts: 290
Max Epstein is on a distinguished road
I'd be curious to see how to incorporate ashes into glass without being a "stupid paperweight".

Every person who has come in and made their own has had a spiritual experience... which I'm glad I can provide. And I can charge good money for them, so it's a win-win
Reply With Quote
  #10  
Old 04-30-2018, 09:55 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,101
Pete VanderLaan is on a distinguished road
John says "Crude", I say "Junk". What do you expect from people that make the actual glass bodies.? Elation brought about through ignorance usually depresses me. I go to great lengths to keep junk out of my glasses. But then again my dog loves to roll in Horse shit.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #11  
Old 04-30-2018, 11:38 AM
Eben Horton Eben Horton is online now
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,507
Eben Horton is on a distinguished road
I refuse to make glass from ashes but I have done it a few times just to see how it all works. I made a beautiful cobalt twisty cane pull out of Fred and then cut the cane into small lengths that were made into pendants. I think 1 TSP of fred made 20 pendants. I added a little dicro frit to give it some sparkle.
The big personal realization I had was I was desecrating human remains and scratch my head on the morality of it all and definitely do t want trace amounts of someone’s ashes in my studio and ending up on my sandwich.
__________________
<eben epoiese>

Last edited by Pete VanderLaan; 04-30-2018 at 11:52 AM. Reason: spelling, demon spelling
Reply With Quote
  #12  
Old 04-30-2018, 11:54 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,101
Pete VanderLaan is on a distinguished road
we sprinkled Mary Beth's furniture teacher's ( a true master) ashes in our woodshop here in the barn. We don't eat sandwiches off the floor. Well, not very often anyways.

I made reliquaries for his family.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #13  
Old 04-30-2018, 12:39 PM
Eben Horton Eben Horton is online now
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,507
Eben Horton is on a distinguished road
Sorry about the “demon spelling”. I posted that from my iPhone.
__________________
<eben epoiese>
Reply With Quote
  #14  
Old 04-30-2018, 03:31 PM
Larry Cazes Larry Cazes is offline
Registered User
 
Join Date: Feb 2006
Location: San Jose, CA
Posts: 921
Larry Cazes is on a distinguished road
Quote:
Originally Posted by Max Epstein View Post
I'd be curious to see how to incorporate ashes into glass without being a "stupid paperweight".

Every person who has come in and made their own has had a spiritual experience... which I'm glad I can provide. And I can charge good money for them, so it's a win-win
I make spheres with ashes incorporated into them. The white fluffy trail is human remains. Its an amazing experience to be part of someones healing.
Attached Images
File Type: jpg 17972427_10154481679598176_8551843996934637289_o.jpg (53.4 KB, 49 views)
Reply With Quote
  #15  
Old 04-30-2018, 03:59 PM
Dan Vanantwerp
Guest
 
Posts: n/a
Wow Larry. That's about the nicest looking cremains tribute I've seen. Well done!
Reply With Quote
  #16  
Old 04-30-2018, 04:17 PM
Larry Cazes Larry Cazes is offline
Registered User
 
Join Date: Feb 2006
Location: San Jose, CA
Posts: 921
Larry Cazes is on a distinguished road
Quote:
Originally Posted by Dan Vanantwerp View Post
Wow Larry. That's about the nicest looking cremains tribute I've seen. Well done!
Thanks Dan. Ive been doing them for a few years and it has changed my outlook on just how rewarding making art can be. The first ones I did were for my family after my father died. Making Those was a very powerful experience for me and it spread by referrals from those. Most folks ask for something small so that it can be carried in a pocket or purse so I suggest keeping them around 2".
Reply With Quote
  #17  
Old 04-30-2018, 04:50 PM
Larry Cazes Larry Cazes is offline
Registered User
 
Join Date: Feb 2006
Location: San Jose, CA
Posts: 921
Larry Cazes is on a distinguished road
Quote:
Originally Posted by Pete VanderLaan View Post
we sprinkled Mary Beth's furniture teacher's ( a true master) ashes in our woodshop here in the barn. We don't eat sandwiches off the floor. Well, not very often anyways.

I made reliquaries for his family.
We spread my father in laws on the 18th hole of a golf course he loved and played regularly.
Reply With Quote
  #18  
Old 04-30-2018, 05:41 PM
Dan Vanantwerp
Guest
 
Posts: n/a
I'll keep that in mind. I have a hard time with the idea. John Croucher's entry on phosphate opals is also interesting as I have recently melted my first batch of this glass. I'd be interested in using animal bone ash to find a recipe that would work. Pete warned that it is difficult, but perhaps using a small amount (<0.5%) to the total phosphate (3-4%) would be feasible.
I really respect that you used your Father's ashes before moving on to other people's loved ones. I imagine that gave both you and your customers a level of comfort in the process.
Reply With Quote
  #19  
Old 04-30-2018, 06:19 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,101
Pete VanderLaan is on a distinguished road
you don't actually need the calcium. replace it with Strontium unless you like above 2500F.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #20  
Old 04-30-2018, 06:48 PM
Marty Kremer Marty Kremer is offline
Registered User
 
Join Date: May 2004
Location: North Yarmouth ME
Posts: 459
Marty Kremer is on a distinguished road
Quote:
Originally Posted by Larry Cazes View Post
...... Most folks ask for something small so that it can be carried in a pocket or purse so I suggest keeping them around 2".
Reductio ad absurdum: "I don't know, let's ask Dad!"

I have more faith in the Magic 8 Ball.
I like knowing that my father is in one place, not on my person or spread out among relatives who may or may not have their own agendas.
Reply With Quote
  #21  
Old 04-30-2018, 10:12 PM
Michael Ahlefeldt-Laurvig Michael Ahlefeldt-Laurvig is offline
Registered User
 
Join Date: Apr 2010
Location: Sweden
Posts: 726
Michael Ahlefeldt-Laurvig is on a distinguished road
Without having thought much about it, I don't think I want to be a paperweight, but Larrys pictures look nice

Last edited by Michael Ahlefeldt-Laurvig; 04-30-2018 at 10:16 PM.
Reply With Quote
  #22  
Old 05-01-2018, 12:07 AM
Sky Campbell's Avatar
Sky Campbell Sky Campbell is offline
Registered User
 
Join Date: May 2002
Location: Gainesville FL
Posts: 942
Sky Campbell is on a distinguished road
I respect the living and if they tell me they don't want to be a paper weight I promise to do my best and not make them into a paper weight. Many states still insist on embalming before cremation. To me that's just silly. The best thing I see happening is a trend for green burials. No embalming wicker or wood casket no grave marker just returning to the earth in a most natural way. I was surprised when I found out I can be buried on my property. I don't have to go anywhere think of the money I'll save.
Reply With Quote
  #23  
Old 05-01-2018, 07:26 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,101
Pete VanderLaan is on a distinguished road
you can be buried in your front yard here too.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #24  
Old 05-01-2018, 09:51 AM
Eben Horton Eben Horton is online now
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,507
Eben Horton is on a distinguished road
I want Ed S to cremate me like he cremated that cat...
__________________
<eben epoiese>
Reply With Quote
  #25  
Old 05-01-2018, 03:27 PM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,679
Jordan Kube is on a distinguished road
You'll have to find him first.
__________________
WWUD? Think for yourself.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 01:31 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.