My blower has announced that it is going to be dead soon. High pitch wailing is not a good thing. I use it for two glory holes. One is 20 x 30 with two large Giberson heads on it and the other is 16 x 24 with one large Giberson burner on it. I want to split these up to run on independent blowers. The blower that I use is this one:
https://optimaldist.com/products/119...bypass-mech-cl
It is over $1000! I thought that I could get two blowers at a much better price. These are the ones that I am thinking of:
https://www.amazon.com/Outlet-Electr...4135260&sr=8-3
They have more CFM, but not as much WCI. Would they still work for my application? I am running on natural gas.

Last edited by Mark Rosenbaum; 07-07-2020 at 11:21 AM.
Reply With Quote
  #2  
Old 07-07-2020, 11:57 AM
Josh Bernbaum Josh Bernbaum is offline
Registered User
 
Join Date: Feb 2009
Location: Brattleboro, VT
Posts: 706
Josh Bernbaum is on a distinguished road
Dudley probably knows how much water column inches his burners need, I bet if you give him a call he'd have an answer on that. I'm not sure the price of the expensive blowers is warranted, but my guess is the pricier ones are designed to run longer with continuous use, which I suppose is more of a consideration for a furnace blower. But that cheap one is so much cheaper that maybe you should get 2 or 3 of them to have as backups and then it's a non-issue.
__________________
www.jmbglass.com
instagram.com/joshbernbaum_glass
Reply With Quote
  #3  
Old 07-07-2020, 01:58 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,057
Pete VanderLaan is on a distinguished road
I have a few eight inch paddle type blowers from Graingers I could let you have Mark. They will not be shy about producing the volume and WC you would need. I always used to cut them down with a big gate valve. Noisy. They're just lying around from the earlier days.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #4  
Old 07-07-2020, 02:02 PM
Eben Horton Eben Horton is online now
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,743
Eben Horton is on a distinguished road
I use a variable trinity blower. Charlie Correll sells them. Dial it down to exactly how much pressure you need and viola! You are using just as much electricity as you can get away with.
__________________
<eben epoiese>
Reply With Quote
  #5  
Old 07-07-2020, 02:41 PM
Mark Rosenbaum's Avatar
Mark Rosenbaum Mark Rosenbaum is offline
Registered User
 
Join Date: Apr 2002
Location: New Orleans, LA
Posts: 1,076
Mark Rosenbaum is on a distinguished road
Quote:
Originally Posted by Pete VanderLaan View Post
I have a few eight inch paddle type blowers from Graingers I could let you have Mark. They will not be shy about producing the volume and WC you would need. I always used to cut them down with a big gate valve. Noisy. They're just lying around from the earlier days.
Thanks for the offer Pete, but I think that noise is a factor too because they are in the same room as us behind the shields. We have lots of fans going and its hard enough to hear now....
Reply With Quote
  #6  
Old 07-07-2020, 03:09 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,057
Pete VanderLaan is on a distinguished road
well, eventually you won't be able to hear them at all.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #7  
Old 07-07-2020, 03:45 PM
Mark Rosenbaum's Avatar
Mark Rosenbaum Mark Rosenbaum is offline
Registered User
 
Join Date: Apr 2002
Location: New Orleans, LA
Posts: 1,076
Mark Rosenbaum is on a distinguished road
Quote:
Originally Posted by Eben Horton View Post
I use a variable trinity blower. Charlie Correll sells them. Dial it down to exactly how much pressure you need and viola! You are using just as much electricity as you can get away with.
I looked at that also.... can I run both GHs on it? How does it dial down? A valve? I have everything piped in for one blower on two GHs, so if that will work, I may just go that route. How loud is it?
Reply With Quote
  #8  
Old 07-07-2020, 03:46 PM
Mark Rosenbaum's Avatar
Mark Rosenbaum Mark Rosenbaum is offline
Registered User
 
Join Date: Apr 2002
Location: New Orleans, LA
Posts: 1,076
Mark Rosenbaum is on a distinguished road
Quote:
Originally Posted by Pete VanderLaan View Post
well, eventually you won't be able to hear them at all.
WHAT????? Speak up!!! We just put a hand to our ear and shake our heads.... one of the disadvantages of a large, loud studio....
Reply With Quote
  #9  
Old 07-07-2020, 05:04 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,057
Pete VanderLaan is on a distinguished road
Charlie's blowers are not quiet. I have one and it drives me out of the room. I am simply offering up a blower at zip for cost. It ran one of our big color melters for years. A real horse.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #10  
Old 07-07-2020, 09:45 PM
Eben Horton Eben Horton is online now
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,743
Eben Horton is on a distinguished road
I mounted my blower in an electrical box and then added a few layers of mineral wool board to sound deaden it. Itís not that loud.
__________________
<eben epoiese>
Reply With Quote
  #11  
Old 07-08-2020, 05:51 AM
Victor Chiarizia Victor Chiarizia is offline
Registered User
 
Join Date: Sep 2005
Location: fairview, NC
Posts: 579
Victor Chiarizia is on a distinguished road
spencer turbine made in windsor, CT
true combustion air blowers but expensive
Reply With Quote
  #12  
Old 07-08-2020, 10:31 AM
Mark Rosenbaum's Avatar
Mark Rosenbaum Mark Rosenbaum is offline
Registered User
 
Join Date: Apr 2002
Location: New Orleans, LA
Posts: 1,076
Mark Rosenbaum is on a distinguished road
Quote:
Originally Posted by Eben Horton View Post
I mounted my blower in an electrical box and then added a few layers of mineral wool board to sound deaden it. Itís not that loud.
We have ours mounted in a box also, but the noise that it is making now is just too much. I'm wondering if it just needs a good cleaning and greasing...
Reply With Quote
  #13  
Old 07-08-2020, 03:49 PM
Art Freas Art Freas is offline
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 684
Art Freas is on a distinguished road
Quote:
Originally Posted by Pete VanderLaan View Post
well, eventually you won't be able to hear them at all.
Air Force Audiologists can tell what plan folks flew back when by what frequencies they have hearing loss at.
Reply With Quote
  #14  
Old 07-08-2020, 04:15 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,057
Pete VanderLaan is on a distinguished road
Mine is more credited to my time in the fire service with the big pumps. It was all before hearing protection was viewed as really important.

I really miss it.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #15  
Old 07-11-2020, 10:36 AM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is offline
Broken Clock
 
Join Date: Jan 2007
Location: Aarde
Posts: 2,221
Greg Vriethoff is on a distinguished road
My left ear has gotten noticeably worse the last couple of years. I know when the damage occurred. A certain rock concert about 40 years ago had me too close stage right. Bothered me since. Had my hearing checked by the blacksmith/fab shop I worked for in Seattle 20 years ago. Noted the loss in that ear. Not too bad, but now the tinnitus has gotten to the point that I can't ignore it when there's not enough ambient sound.
Reply With Quote
  #16  
Old 07-11-2020, 10:50 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,057
Pete VanderLaan is on a distinguished road
Get a hearing aid. Once the follicles start to die, the brain stops checking in and then getting the aid does you little good. There's a lot of very good hearing aids coming on the market that are a fraction of what ones like mine cost. You'll never get rid of the tinnitus.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #17  
Old 07-15-2020, 02:18 PM
Jon Myers's Avatar
Jon Myers Jon Myers is offline
Registered User
 
Join Date: Apr 2002
Location: Portland OR
Posts: 630
Jon Myers is on a distinguished road
those Busch variable speed blowers are small and quiet and cheap and strong...
Reply With Quote
  #18  
Old 07-16-2020, 01:59 AM
Scott Benefield Scott Benefield is offline
Registered User
 
Join Date: Apr 2002
Location: Ballintoy, Northern Ireland
Posts: 89
Scott Benefield is on a distinguished road
Do you have a part number(s) for variable speed Busch blowers? On a quick Google search I could only find Busch vacuum pumps
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 04:46 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.