Powder with dust

How do you or can you wash/ clean powder or frit contimanited with dust . The dust got in by leaving the glass open for far too long.
Franklin
Reply With Quote
  #2  
Old 02-25-2018, 08:49 AM
Rosanna Gusler Rosanna Gusler is offline
Registered Fuser
 
Join Date: Mar 2003
Location: Wanchese, NC
Posts: 916
Rosanna Gusler is on a distinguished road
Google " how to wash enamel powder "
Reply With Quote
  #3  
Old 02-25-2018, 09:24 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,659
Pete VanderLaan is on a distinguished road
I do wash frit and powder after making color and running the chunks through the crusher. I could own a second crusher that does ultra fines but that's another 6K, so I capture the stuff that broke up that way in the first place.

First the ore is run through screens from Gilson. I have about ten differing meshes in 18 x 18 drawers. It used to be automated with one on top of the other but I stopped that after leaving Santa Fe. Now it's hand work. The ore separates into varying grit sizes and than goes in a big stainless food prep tray from the navy.It has water added, it's stirred and the residue is discarded unless I think there's some valuable fines in it in which case it's evaporated.

I usually put about 20 lbs of ore in the tray at a time, stir constantly, and rinse as necessary until the water comes clear. Then it is allowed to evaporate on the burners until totally dry. Then it goes into bags marked with the frit size.

It's simple. You just have to be anal retentive and compulsive to do it. The crusher sadly is not actually a low maintenance machine. It chews up parts. Mine needs a few replaced that are hard to get to. Essentially, it's a beastly Archimedian wedge.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #4  
Old 02-25-2018, 02:48 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,755
Franklin Sankar is on a distinguished road
Thanks
Hopefully the dust can dissolve or mix in with the water
Franklin
Reply With Quote
  #5  
Old 02-25-2018, 04:22 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,659
Pete VanderLaan is on a distinguished road
the dust can't dissolve if it's glass dust.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #6  
Old 02-26-2018, 04:08 AM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,755
Franklin Sankar is on a distinguished road
Itís powder or frit I left open for a long while. Dust from the air is the worst. I did not realize It gets on everything even if you donít notice it.
Franklin
Reply With Quote
  #7  
Old 02-26-2018, 08:38 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,659
Pete VanderLaan is on a distinguished road
zip loc bags are your friend.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #8  
Old 02-26-2018, 08:51 AM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,422
Eben Horton is on a distinguished road
Quote:
Originally Posted by Franklin Sankar View Post
It’s powder or frit I left open for a long while. Dust from the air is the worst. I did not realize It gets on everything even if you don’t notice it.
Franklin
When you are food shopping, always buy food that comes in a clear plastic jar with a screw on lid. For example, peanut butter, honey roasted peanuts, jelly beans, etc.

I bought cases of jars like that from the container store and they last a life time.

Ziplock bags work but can end in disaster
__________________
<eben epoiese>
Reply With Quote
  #9  
Old 02-26-2018, 01:00 PM
Cecil McKenzie Cecil McKenzie is offline
Registered User
 
Join Date: Feb 2011
Location: Emporia, KS
Posts: 488
Cecil McKenzie is on a distinguished road
Franklin I have used a shallow sided pan to clean fit that has been contaminated. Put some frit in the pan with the water swish the water around to get the smaller dust particles in suspension then pour the water off but not pouring off frit, this is how small time prospectors panned for gold. Put the dirt in the pan swish it around and the heavier material settles to the bottom.

i adopted a stray brittany spaniel that made a sleeping place in a wooden box that had maybe 10 kilos of white fit breaking open every bag and contaminating it with clay like mud. She was an expensive dog. Prior to that she had made a bed in two 24 by 36 by 6 inch pieces of fiberfrax even though I did not discover that until later.

Hope this helps.
Reply With Quote
  #10  
Old 02-27-2018, 01:50 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,755
Franklin Sankar is on a distinguished road
Thanks I have hope now.
Franklin
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 03:55 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.