Hot shop stringer pulling apparatus

Does anyone have an image or design for a device to pull large quantities of stringer in the hot shop? I have seen images of said devices but cannot remember or source the literature or web site.

Thanks.
Reply With Quote
  #2  
Old 04-10-2018, 03:02 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,402
Eben Horton is on a distinguished road
Toots zynski has a set up for this. I donít have any pics
__________________
<eben epoiese>
Reply With Quote
  #3  
Old 04-10-2018, 03:05 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,598
Pete VanderLaan is on a distinguished road
we made a really large wheel and cranked it around. It worked better than just running into the wall but it wasn't great. Northstar as I understand it has a series of pulleys that apparently work well. Timing is everything.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #4  
Old 04-10-2018, 06:05 PM
Sky Campbell's Avatar
Sky Campbell Sky Campbell is offline
Registered User
 
Join Date: May 2002
Location: Gainesville FL
Posts: 893
Sky Campbell is on a distinguished road
I would think a large square wheel unless you want curved cane.
Reply With Quote
  #5  
Old 04-10-2018, 07:55 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,402
Eben Horton is on a distinguished road
Quote:
Originally Posted by Sky Campbell View Post
I would think a large square wheel unless you want curved cane.
A benson burner, two slow rotating wheels to grab the thread and pull and a chopper that chops every 30 seconds and a hopper underneath to catch the threads.
__________________
<eben epoiese>
Reply With Quote
  #6  
Old 04-10-2018, 08:25 PM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,647
Jordan Kube is on a distinguished road
Quote:
Originally Posted by Sky Campbell View Post
I would think a large square wheel unless you want curved cane.
It's cold by the time it hits the wheel. Square wheel would break everything. Do it too hot and it gets deformed.
__________________
WWUD? Think for yourself.
Reply With Quote
  #7  
Old 04-10-2018, 08:30 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,598
Pete VanderLaan is on a distinguished road
well, make the square sides the size you want the stringer. do it hot
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #8  
Old 04-10-2018, 08:51 PM
Rich Samuel's Avatar
Rich Samuel Rich Samuel is offline
Registered User
 
Join Date: Apr 2002
Location: Seattle, WA
Posts: 2,402
Rich Samuel is on a distinguished road
Something similar to an adjustable yarn skeiner should work. Easy to motorize, too.

https://www.google.com/search?q=yarn...w=1024&bih=483
Reply With Quote
  #9  
Old 04-10-2018, 08:58 PM
Sam Stang Sam Stang is offline
Registered User
 
Join Date: Feb 2018
Location: Augusta, Missouri
Posts: 11
Sam Stang is on a distinguished road
John Chiles made one for my wife, Kaeko almost 20 years ago. It uses the concept of chucking up a color bar in a lathe and uses a oxy/pro torch to melt the tip and rollers to pull a continuous thread. The operator has to control the torch, start the thread with tweezers and advance the color bar. John used side cutting pliers with a solenoid to cut 2 foot (or whatever you want) lengths and the threads drop into a pvc 1/2 round trough.
Reply With Quote
  #10  
Old 04-10-2018, 10:50 PM
Cecil McKenzie Cecil McKenzie is offline
Registered User
 
Join Date: Feb 2011
Location: Emporia, KS
Posts: 488
Cecil McKenzie is on a distinguished road
For what it is worth . A picture of a device I made many years ago. i heated up the bolt in the middle so that I could attach a hot bit then turned the device on a threading machine and made threads that were about 8 inches long with a little radius on the end. it worked fairly well but there was a problem. As the glass cooled it would shrink enough to break and the little threads would start flying through the air or falling on the floor. i thought that making the armature have a little flex would help, This is about the size of a blowpipe.
Attached Images
File Type: jpg IMG_3020.jpg (17.7 KB, 53 views)
Reply With Quote
  #11  
Old 04-11-2018, 01:08 AM
Michael Ahlefeldt-Laurvig Michael Ahlefeldt-Laurvig is online now
Registered User
 
Join Date: Apr 2010
Location: Sweden
Posts: 698
Michael Ahlefeldt-Laurvig is on a distinguished road
Ive made thin stringers with a bike. Take one junk bicycle, turn it upside down on the floor and cut off back tire. Cut an angled notch in the rim to accept the plier pinched tip of a hot color rod. Crank the pedals! You have to cool the glass violently with air before it spools on to the rim if you dont want it breaking when it shrinks as it cools.
Its best to be two people and the glass is spooled onto the rim from behind so you have to cut part of the brake or something or tack the gear to be able to crank it backwards.

If you want to go overboard in class then make a tiny little electric furnace with a hole in the bottom and a hole in the tiny crucible and mount it15 ft up in the air and and let gravity and temperature pull your stringers - perfect control of diameter of stringers with aperture diameter and temp variations. Thats one way that halogen bulbs and florescent lighting tubes are made
Reply With Quote
  #12  
Old 04-11-2018, 09:14 AM
Art Freas Art Freas is offline
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 512
Art Freas is on a distinguished road
fusers use a raised kiln with a hole in the bottom with a mold with a hole in it above the hole in the kiln. Look up vitragraph. once it starts to drip out the hole they grab it with tweezers and pull away. https://www.bing.com/videos/search?q...5037&FORM=VIRE

Last edited by Art Freas; 04-11-2018 at 09:16 AM.
Reply With Quote
  #13  
Old 04-11-2018, 04:14 PM
Charles Friedman Charles Friedman is offline
Registered User
 
Join Date: Apr 2002
Location: Seattle Wa
Posts: 556
Charles Friedman is on a distinguished road
cane pulling machine

Here is one I made.
Attached Images
File Type: jpg cane pulling machine 1.jpg (47.4 KB, 72 views)
File Type: jpg cane pulling machine 2.jpg (48.9 KB, 68 views)
File Type: jpg cane pulling machine 3.jpg (41.5 KB, 68 views)
__________________
"Glass will save the world from ourselfs" CharlesF
Reply With Quote
  #14  
Old 04-12-2018, 01:18 AM
Allan Gott Allan Gott is offline
Registered User
 
Join Date: Apr 2002
Location: Youbou, Vancouver Island
Posts: 659
Allan Gott is on a distinguished road
a looooong parking lot right outside the shop, running shoes, impeccable traffic control
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 07:19 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.