Don't...

So, I ran out of beeswax. I've made some candles before and dropped a little wad of soy wax onto the jacks. Every time I went back to the glory my vessel would ignite from the inside. While a neat trick it also left some nasty residue on the piece. I suppose it also could have been the vanilla scented oil I melted into the wax

I started thinking about a "sounds reasonable but don't try it" thread. Anyone care to share?

I can borrow another one...don't use cat litter to line the bottom of your glory hole.
Reply With Quote
  #2  
Old 03-27-2018, 03:08 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,927
Pete VanderLaan is on a distinguished road
don't use an aluminum tray for shoving cullet into your furnace. ( Peet Robison and the case of the missing tray, 1988)

Bad move. Really expensive mistake.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 03-27-2018, 03:10 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,927
Pete VanderLaan is on a distinguished road
Mark your bags for batch. Don't get silica confused with porcelain. ( Al Leedom, my shop, 1984.)

Well that pot is gone...
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #4  
Old 03-27-2018, 04:05 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,474
Eben Horton is on a distinguished road
When making snorkel cane, DONT inhale before you are sure that your snorkel is completely submerged. Eben Horton 1999
__________________
<eben epoiese>
Reply With Quote
  #5  
Old 03-27-2018, 04:11 PM
Dan Vanantwerp
Guest
 
Posts: n/a
I was sandblasting near my cullet supply...a little sand won't hurt. It doesn't blend in like you think it would. That glass had a lot of texture.
Reply With Quote
  #6  
Old 03-27-2018, 04:14 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,927
Pete VanderLaan is on a distinguished road
Don't ever run a body grinder near finished glass
*****
Me several times.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #7  
Old 03-27-2018, 04:23 PM
Dan Vanantwerp
Guest
 
Posts: n/a
Ditto on the grinder Pete. I need a bigger shop.

Don't use vegetable oil instead of linseed oil when making a cork mold.

Don't forget to add a hole to said mold to allow expulsion of gases. (Sorry, George...his front tooth paid dearly for that one)
Reply With Quote
  #8  
Old 03-27-2018, 11:10 PM
Bill Worcester Bill Worcester is online now
Registered User
 
Join Date: Apr 2009
Location: Maui, HI
Posts: 55
Bill Worcester is on a distinguished road
Exclamation Donít spit Pepsi in your blowpipe

Had a closed off bubble, pissed off, well just thought just put liquid in pipe and cap off and make steam.Not good, so hot so fast.
Reply With Quote
  #9  
Old 03-28-2018, 01:50 AM
Max Epstein Max Epstein is offline
Registered User
 
Join Date: Sep 2016
Location: Tallahassee, FL
Posts: 284
Max Epstein is on a distinguished road
Don't hang a kiln controller by copper wire near a 240v outlet.
Reply With Quote
  #10  
Old 03-28-2018, 07:50 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,927
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Max Epstein View Post
Don't hang a kiln controller by copper wire near a 240v outlet.
********
This one I don't really understand.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #11  
Old 03-28-2018, 07:58 AM
Brennan VanderLaan Brennan VanderLaan is offline
Registered User
 
Join Date: Mar 2018
Location: Massachusetts
Posts: 1
Brennan VanderLaan is on a distinguished road
Don't guess that you know which kind of grit a lapping machine is running

Don't add grit to a running lapping machine based on said assumption

Don't try to make the lapping process faster

(~96 - Pete's shop)
Reply With Quote
  #12  
Old 03-28-2018, 08:55 AM
Nick Delmatto Nick Delmatto is offline
Registered User
 
Join Date: Feb 2010
Location: Logan, OH
Posts: 44
Nick Delmatto is on a distinguished road
When using coffee cups like crucibles to melt glass, don't use the ones marked Corning on the bottom. They melts just like glass.
Reply With Quote
  #13  
Old 03-28-2018, 09:21 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,927
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Brennan VanderLaan View Post
Don't guess that you know which kind of grit a lapping machine is running

Don't add grit to a running lapping machine based on said assumption

Don't try to make the lapping process faster

(~96 - Pete's shop)
*****
Spoken like a helpful very young son
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #14  
Old 03-28-2018, 10:43 AM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,474
Eben Horton is on a distinguished road
Quote:
Originally Posted by Brennan VanderLaan View Post
Don't guess that you know which kind of grit a lapping machine is running

Don't add grit to a running lapping machine based on said assumption

Don't try to make the lapping process faster

(~96 - Pete's shop)

hey Bren! welcome!
__________________
<eben epoiese>
Reply With Quote
  #15  
Old 03-28-2018, 11:39 AM
James Ennis James Ennis is offline
Registered User
 
Join Date: Oct 2004
Location: seattle
Posts: 328
James Ennis is on a distinguished road
don't leave your tools in your car........every new to Seattle glassblower.
Reply With Quote
  #16  
Old 03-28-2018, 12:19 PM
Dan Vanantwerp
Guest
 
Posts: n/a
From Ed Schmidt...don't lap glass with stones. Especially if you are in a hurry.
Reply With Quote
  #17  
Old 03-28-2018, 12:27 PM
Dan Vanantwerp
Guest
 
Posts: n/a
Don't use aluminum parts with stannous chloride sprayers.
Reply With Quote
  #18  
Old 03-28-2018, 03:45 PM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is offline
PotatoFish
 
Join Date: Jan 2007
Location: Charlotte, NC
Posts: 2,040
Greg Vriethoff is on a distinguished road
...try to wipe clean the lenses of your prescription glasses with the front of your dampened t shirt after lapping on a grit wheel.
__________________
"Technique is just a means of arriving at a statement." - Jackson Pollack
Reply With Quote
  #19  
Old 03-28-2018, 04:24 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,474
Eben Horton is on a distinguished road
Donít make pumpkins
__________________
<eben epoiese>
Reply With Quote
  #20  
Old 03-28-2018, 06:50 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,927
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Greg Vriethoff View Post
...try to wipe clean the lenses of your prescription glasses with the front of your dampened t shirt after lapping on a grit wheel.
***
I keep a spare pair of older glasses at the machine to exchange.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #21  
Old 03-28-2018, 06:51 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,927
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Eben Horton View Post
Donít make pumpkins
***
If you do, you simply are damned for eternity. Everyone knows this at this point.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #22  
Old 03-28-2018, 07:23 PM
Art Freas Art Freas is offline
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 530
Art Freas is on a distinguished road
Rush removing a door casting from a mold.
Reply With Quote
  #23  
Old 03-29-2018, 03:23 AM
Rich Samuel's Avatar
Rich Samuel Rich Samuel is online now
Registered User
 
Join Date: Apr 2002
Location: Seattle, WA
Posts: 2,425
Rich Samuel is on a distinguished road
"Sure, I can make one to match the other five."
Reply With Quote
  #24  
Old 03-29-2018, 11:24 AM
Paul Thompson Paul Thompson is offline
Registered User
 
Join Date: Apr 2007
Location: Hygiene CO
Posts: 189
Paul Thompson is on a distinguished road
Don't mess with the settings on someone else's garage.
__________________
"You don't have to be a very good glassblower when you can fix stuff" -- Richard Royal
Reply With Quote
  #25  
Old 03-29-2018, 11:53 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,927
Pete VanderLaan is on a distinguished road
Don't ever take work to a selling show which requires orders for a piece you just developed in the last ten days.
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 11:55 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.