Elements not working

We have just rebuilt our 300# Stadelman furnace and have one bank (2) elements not working.
I have replaced those not working elements with two spares (Brand new) and replaced the element straps and everything seems right but they do not heat up. The welding leads on each side of the element bank that is out show around 290 amps. The welding leads to the working banks is at 220 amps.

Any suggestions on what my problem might be.
All help appreciated
Reply With Quote
  #2  
Old 07-06-2018, 04:02 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,660
Pete VanderLaan is on a distinguished road
Detach both sets of straps and run a continuity test on each element. They have to be detached.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 07-06-2018, 09:27 PM
Tim Bassett Tim Bassett is offline
Registered User
 
Join Date: Jun 2006
Location: melbourne australia
Posts: 77
Tim Bassett is on a distinguished road
When the bank was not working I replaced the elements with two new ones and checked continuity just before joining the straps together. Pretty sure I have some other problem that is yet to be determined.
Reply With Quote
  #4  
Old 07-06-2018, 10:12 PM
George Tessman George Tessman is offline
Registered User
 
Join Date: Jun 2004
Location: Highland, IN
Posts: 233
George Tessman is on a distinguished road
On trouble shooting. Start at the elements and work backwards.
Do you have voltage...Even if you have voltage you may not have the amps needed
If you have checked continuity and it is correct. connect wires that are feeding elements that are working and see if elements heat up.
If they heat up. you have a problem in the wires and connections on the bank that is not heating up. Work your way back and make sure all connections are tight. You should do this before the previous step.
Reply With Quote
  #5  
Old 07-07-2018, 08:34 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,660
Pete VanderLaan is on a distinguished road
I have seen elements break on installation. The trick here is to not assume anything.
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 12:41 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.