parallel concentrators

I am trying to parallel two concentrators and when I turn them on the ball in the visionaire drops to about 2 from 5 the other one (Devilbliss) is ok. Devill bliss and visionaire output pressure set at 8.4psig. Before paralleling pressure steady .
output pressure after paralleling is steady at 8.4psi.
I was thinking about increasing the pressure of the visionaire until the ball raises. But then with no load the pressure will be high.
Adding an external one way valve.
So anyone tried paralleling? What happened?
Franklin
Reply With Quote
  #2  
Old 05-29-2017, 07:02 PM
Peter Bowles Peter Bowles is offline
Registered User
 
Join Date: Sep 2002
Location: Breadalbane, Tasmania
Posts: 638
Peter Bowles is on a distinguished road
You might have to do a bit of trawling - but I'm sure you will find what you're after here.

http://www.isgb.org/forum/
Reply With Quote
  #3  
Old 05-29-2017, 07:59 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,776
Eben Horton is on a distinguished road
Everyone I know who uses concentrators has them feeding a compressor, which fills a k tank. This way they have no limitations.
Reply With Quote
  #4  
Old 05-29-2017, 09:23 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 4,049
Franklin Sankar is on a distinguished road
Thanks for the replies. I may have to go for the compressor but would like to fix this first. The good thing about this board is that you get good advice.
Interesting problem to solve. I like.
Franklin
Reply With Quote
  #5  
Old 05-29-2017, 11:35 PM
David Hopman David Hopman is offline
Registered User
 
Join Date: Mar 2009
Location: Sutter Creek, CA
Posts: 442
David Hopman is on a distinguished road
I run 3 parallel concentrators and haven't noticed any problems like you are having, unless the flow of the units are being restricted in some way. Make sure the O2 valve on the torch is open all the way and always stays open. See if that fixes it.
Reply With Quote
  #6  
Old 05-30-2017, 06:25 AM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 4,049
Franklin Sankar is on a distinguished road
I reconfigured the hoses to try and balance the flow and now both flows are dropping when I block the output tube with my finger but one drops much faster than the other. I will live with this and see what happens later.
David or anyone do you have a one way valve on the outputs of the concentrator.
Thanks
Franklin
Reply With Quote
  #7  
Old 05-30-2017, 06:33 AM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 4,049
Franklin Sankar is on a distinguished road
water in the air is a killer for the concentrator.
Does anyone have moisture problems.
Franklin
Reply With Quote
  #8  
Old 05-31-2017, 12:41 PM
David Hopman David Hopman is offline
Registered User
 
Join Date: Mar 2009
Location: Sutter Creek, CA
Posts: 442
David Hopman is on a distinguished road
I do not have any one way valves on my system. I'm in CA so I don't have a humidity problem. Back pressure is really bad for the units, avoid it at all costs and keep the O2 valve always wide open. If you have trouble just regulating your flame with the gas valve because of too much O2 flow, add another bleed valve somewhere on the line to reduce the flow to the torch without reducing the outflow from the concentrators.
Reply With Quote
  #9  
Old 05-31-2017, 10:00 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 4,049
Franklin Sankar is on a distinguished road
Thanks David. I need all the oxygen I can get. Glass turning brown with too much propane or not enough oxy.
Using a mega minor with 2 conc if I can parallel them without back pressure caused by one unit pushing into the other.hoping a little difference in pressure between the units will be ok.
Franklin
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 09:47 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.