So I've got my color unit up again and I would like to do some phosphate melts in this new pot I threw in there. I'm going to be working off a formula we used at John's class which used SP batch with erbium as the base. I have that here, it's what I use for my clear, but I also brought some bags of the 87 plain (no erbium) that I picked up from the batch plant down there. I've used the plain a lot in the past so as to not waste erbium on some of the colors I've done where I'm just adding colorants to their base, and save a bit of money as I think it's a bit less expensive. Question is, without the decolorant, does anyone think I'd see a greenish tint to the opaline white I'm looking for? I'm prob overthinking this as is usually my MO, but if there were any objections based on experience that could potentially save me a wasted test melt.

Also, one more, someone recommended not letting the temp get below 2150 for phosphates. Any truth to this? Just asking because that's a bit warmer than my usual gathering/idle temps.

Thanks
__________________
www.jmbglass.com
instagram.com/joshbernbaum_glass
Reply With Quote
  #2  
Old 05-16-2019, 07:05 PM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,717
Jordan Kube is on a distinguished road
I wouldn't worry about the erbium. Keep the phosphate opal hot. I have experienced snot and crystal formation at lower temps.
__________________
WWUD? Think for yourself.
Reply With Quote
  #3  
Old 05-17-2019, 09:18 AM
Josh Bernbaum Josh Bernbaum is online now
Registered User
 
Join Date: Feb 2009
Location: Brattleboro, VT
Posts: 736
Josh Bernbaum is on a distinguished road
Okay thanks Jordan
__________________
www.jmbglass.com
instagram.com/joshbernbaum_glass
Reply With Quote
  #4  
Old 05-17-2019, 09:46 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,369
Pete VanderLaan is on a distinguished road
While I don't have the recipe John wanted to use , it will be the case that calcium will cause a lot of issues from the SP. The new silica is remarkable in its clarity if the stuff you purchased is in fact new stock.

Phosphates don't do well if cooled down much. That's true of a lot of glasses. I tend to think the lumps in lead arsenates are caused by overcooling the melts to make rods. In general, glass doesn't want to be in a rod form anyways. The attempts we made up here with Marks TIT series turned to glasscrete when cooled. We kept the calcium out of those glasses and replaced with Strontium.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #5  
Old 05-17-2019, 09:32 PM
Shawn Watt Shawn Watt is offline
Registered User
 
Join Date: May 2010
Location: Branson, MO
Posts: 101
Shawn Watt is on a distinguished road
I also mix my phosphate in spruce with erbium. I have to melt pretty hot and long 2385 for 7 hours and then I take it down the the “squeeze “ 2185 and work it from there. It will get snotty if it gets much lower than that. I also have to use it up within a couple days otherwise it’s gets chunky and starts to creep Coe. I was bummed I didn’t end up making it to the class. It sounded like a great experience.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 10:58 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.