Basalt

Has anyone used basalt fiber as a liner to their lehrs?
I currently use refrasil and it breaks down quickly and becomes dusty and airborne.
Basalt is made from volcanic rock and has a melting point of 2600 degrees F with an application temperature of 1800 degrees. It comes in lots of weave patterns and densities....
It can also be used to minimize thermal transfer in lehrs and furnaces, but that is for another day...
Reply With Quote
  #2  
Old 01-26-2021, 10:53 PM
Sky Campbell's Avatar
Sky Campbell Sky Campbell is offline
Registered User
 
Join Date: May 2002
Location: Gainesville FL
Posts: 1,026
Sky Campbell is on a distinguished road
I ordered a bunch of basalt samples that came in 10” squares. All the weaves I used turned brittle when fired. Basalt is not a new material it’s been used for muffler packing for a long time. That said I found ceramic fiber that has served me very well for many years. I bought cheap welding blankets from harbor freight that held up far better then brand name refrasil. I think refrasil is made from silica not a ceramic. I’ll be honest I’m not sure what the difference is but I do know some of the ceramic fiber cloth I use lasts years longer then silica based cloth. I cut and hem pads with staples that get layered in between blown ware. You would be amazed at how much I can stack in a annealer.
Reply With Quote
  #3  
Old 01-27-2021, 11:08 AM
Mark Rosenbaum's Avatar
Mark Rosenbaum Mark Rosenbaum is offline
Registered User
 
Join Date: Apr 2002
Location: New Orleans, LA
Posts: 1,091
Mark Rosenbaum is on a distinguished road
Quote:
Originally Posted by Sky Campbell View Post
I ordered a bunch of basalt samples that came in 10” squares. All the weaves I used turned brittle when fired. Basalt is not a new material it’s been used for muffler packing for a long time. That said I found ceramic fiber that has served me very well for many years. I bought cheap welding blankets from harbor freight that held up far better then brand name refrasil. I think refrasil is made from silica not a ceramic. I’ll be honest I’m not sure what the difference is but I do know some of the ceramic fiber cloth I use lasts years longer then silica based cloth. I cut and hem pads with staples that get layered in between blown ware. You would be amazed at how much I can stack in a annealer.
Thanks Sky.... are the Harbor Freight blankets ceramic?
Reply With Quote
  #4  
Old 01-27-2021, 08:46 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,799
Eben Horton is on a distinguished road
You can spend a lot of time going down a rabbit hole or you can fill a cookie sheet full of sand.
__________________
<EBEN EΠOIESEN >
Reply With Quote
  #5  
Old 01-27-2021, 10:03 PM
bob gent bob gent is offline
Registered User
 
Join Date: Oct 2016
Location: lawrence, ks
Posts: 17
bob gent is on a distinguished road
I've always used plaster, without adding water, of course
Reply With Quote
  #6  
Old 01-27-2021, 11:39 PM
Sky Campbell's Avatar
Sky Campbell Sky Campbell is offline
Registered User
 
Join Date: May 2002
Location: Gainesville FL
Posts: 1,026
Sky Campbell is on a distinguished road
Quote:
Originally Posted by Eben Horton View Post
You can spend a lot of time going down a rabbit hole or you can fill a cookie sheet full of sand.
I’d like to see how you use layers of sand to stack work in the annealer.

As far as the harbor fright welding blanket. I would guess they constantly change suppliers. They buy whatever they can get the best deal on. I wouldn’t count on anything from there being consistent. I bought one to try years ago when it held up I bought a bunch of them. I have plenty of pads to use for stacking wares and separating hot things in hot places. The ones that I’m using now are labeled ceramic welding blanket.
Reply With Quote
  #7  
Old 01-27-2021, 11:49 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,799
Eben Horton is on a distinguished road
Sky, I have a metal rack in my annealer that I welded up that is the same width as the cookie sheets.
__________________
<EBEN EΠOIESEN >
Reply With Quote
  #8  
Old 01-28-2021, 11:09 AM
Mark Rosenbaum's Avatar
Mark Rosenbaum Mark Rosenbaum is offline
Registered User
 
Join Date: Apr 2002
Location: New Orleans, LA
Posts: 1,091
Mark Rosenbaum is on a distinguished road
Quote:
Originally Posted by Eben Horton View Post
You can spend a lot of time going down a rabbit hole or you can fill a cookie sheet full of sand.
Yes, but with tall flattened work, I want some stability at the bottom. A layer of sand doesn't provide that. I need something solid so when I open and close the door, the piece doesn't fall over. i use sand trays for weights and marbles
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 05:12 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.