Old 01-02-2005, 06:35 PM
Todd Nelson Todd Nelson is offline
Registered User
 
Join Date: Feb 2004
Location: Spokane, Missouri
Posts: 97
Todd Nelson is on a distinguished road
Allan; you didn't say what type of welder you have. If it's the lincoln tombstone it's an AC welder. 6011 rod will weld very nicely on this machine or any machine or polarity but 7018 is a DC reverse polarity rod and won't weld worth a crap. You can buy 7018 that will run on straight polarity and a DC machine. If your rod boxes are unopened and not rusted thru the rods are probably alright!

Last edited by Todd Nelson; 01-02-2005 at 06:49 PM.
Reply With Quote
  #52  
Old 01-02-2005, 07:29 PM
Ben Rosenfield's Avatar
Ben Rosenfield Ben Rosenfield is offline
Registered User
 
Join Date: Sep 2003
Location: Cincinnati, OH
Posts: 2,554
Ben Rosenfield is on a distinguished road
Quote:
Originally posted by Todd Nelson
.if you want to keep your rods fresh keep them in a warm, dry environment, like an old frig(with a light bulb on inside) or maybe in the corner of an annealer. You could take them out the day b/4 you need them and they won't have soaked up all that humidity!
Along those lines, you could add one of these to the storage space. The 900-gram unit handles 66 cubic feet.
Reply With Quote
  #53  
Old 01-02-2005, 08:29 PM
Allan Gott Allan Gott is offline
Registered User
 
Join Date: Apr 2002
Location: Youbou, Vancouver Island
Posts: 659
Allan Gott is on a distinguished road
Well that could be the trouble right there Todd. Thanks. Who would use rod like that???

......and yes, Lincoln tombstone about 10 yrs new.
Reply With Quote
  #54  
Old 01-02-2005, 09:56 PM
Scott Dunahee's Avatar
Scott Dunahee Scott Dunahee is offline
Registered User
 
Join Date: Apr 2002
Location: Madison, WI
Posts: 645
Scott Dunahee is on a distinguished road
115V Millers

I have a Miller 130 (?) or 135 and I love it. It's easy to use with the gas and I get clean penetrating welds every time. It's really only good to about 3/16" for mild steel and I've never tried Stainless, but I'm told it'll do that, too.

I've built an entire hot shop with this little guy and he keeps going. If you're not going for portability, which was of concern to me, I'd go with a 220 unit though.

BSD
Reply With Quote
  #55  
Old 01-03-2005, 08:19 AM
Rick Schneider
Guest
 
Posts: n/a
Tech Schools

I am glad Todd weighed in on the numbers of Sticks. Too often we think we can do something properly just because it happens to work. I have always been an advocate of taking a class at a community college. I was able to take Stick welding and a TIG MIG class for $95 each from professional welders. You will learn what all those stick numbers mean, what the uses for DC - /DC+/ AC are really for. Most of you probably set your welder on one of them and leave it forever not knowing which one will really do a better job. One of these settings will give you better penetration. Go find out. You will be the better for it.

Before any of you say I do just fine and welding isn't that hard and my equipment is built tough, I want to say that welding is a pretty easy thing to just get the hang of, but for the cheap price of a CC class you will learn it right and it will be better. You will get more out of your $100 Welding class than you will out of a $1000+ summer glass class.
Reply With Quote
  #56  
Old 01-03-2005, 10:37 AM
Andrew Brott Andrew Brott is offline
Registered User
 
Join Date: Dec 2002
Location: New Orleans
Posts: 213
Andrew Brott is on a distinguished road
Saving rods

Live in the swamplands; we save ours by putting them in a open soup can on top of a running day tank, or pipe warmer.
Ab
Does anybody have any experience with this machine: Delta 20-330 5" X 6" Horizontal Band Saw with Blade.... and it's cheap.
http://www.toolking.com/delta/view.asp?id=3182
Reply With Quote
  #57  
Old 01-03-2005, 11:17 AM
Alexander Adams's Avatar
Alexander Adams Alexander Adams is offline
www.artistadams.com
 
Join Date: May 2003
Location: Philadelphia, PA/Coral Gables, FL
Posts: 595
Alexander Adams is on a distinguished road
You can get a very similar saw at Enco for $197.95+S&H actually it is on sale for $169.95. Or a similar saw at Grizzy Industrial for $287 S&H included. Harbour Freight has one listed for $169. McMaster-Carr has one listed for 271.95+S&H. These tool suppliers, even Delta, buy their tools from the same factories in Asia and we end up paying $100 extra dollars for a name brand sticker and special paint. Some tool suppliers will offer 3 identical tools but made in 3 different factories: China, Taiwan and North America, I came across this when I was shopping for a stomp shear. The Chinese Tool is the lowest priced and least reliable, Taiwan is better quality and a little more expensive, workmanship is increased i a place where one can be publically "caned" for vandalism. The tools in the made in the USA or Canada are twice as expensive and are sometimes the most reliable. If you do inquire where things were made, remember, "Made in the USA" and "Assembled in the USA" are two different things.

The Delta Model pictured on Toolking is okay. Depending on what you are cutting it can be loud and the blades often don't track straight when cutting several itmes at once. The other down side is the lack of a lube/coolant system and the belt drive can slip. It will be more accurate, smell better, safer and much more healthy to be around than an abrasive cut off saw.

-Alex
Reply With Quote
  #58  
Old 01-03-2005, 08:36 PM
Jon Myers's Avatar
Jon Myers Jon Myers is offline
Registered User
 
Join Date: Apr 2002
Location: Portland OR
Posts: 631
Jon Myers is on a distinguished road
what about a cold cut carbide saw? They are much faster than a bandsaw and much quieter than an abrasive saw and they have a stiff blade so the angles stay sharp (when you miter). I have been amazed by ours though the blades are expensive and don't cut stainless (knocks the teeth off). It cuts solid 1.5" as easy as our old cutoff abrasive cut 1/4" angle.
Reply With Quote
  #59  
Old 01-04-2005, 11:12 AM
Parker Stafford Parker Stafford is offline
Registered User
 
Join Date: Apr 2002
Posts: 254
Parker Stafford is on a distinguished road
I wouldn't own a stick welder. M.I.G. simply has greater flexibility and consistency. It is akin to going from a manual typewriter to a computer. I used to stick weld and I would never go back. I was in sculpture for ten years before I got side-swiped by glass. I would not get flux core but go with the gas unit. When I did stick weld, we used jet rod, the numbers for which I forget now, it has been so long ago.

For most welding around the hot shop you are not going to need a huge unit. I have a Lincoln SP-125 Plus, and it gives me all the penetration I need. You need to look closely at the specs and get a unit that is going to give you the penetration you think you are going to need and then get that. In eight years I have never once been in a situation where I was scratching my head and wishing I bought something heavier. I would buy from a welding shop with a fixed position in the physical universe.

Gas cutting in a ferrous situation is fine if you are making elaborate cuts, but most of my cuts are straight. But cutting is not welding, which is actually brazing, another animal, and one I would not use when I am joining ferrous with a MIG. I use a chop saw but wish I could get a well built band saw. The difference in the quality of the cut is noticable, but the chop saw I have is passable, and the price is right.

I'd love to hear from anyone who has a bandsaw that they love.

Parker S.
Reply With Quote
  #60  
Old 01-04-2005, 11:24 AM
Steve Stadelman Steve Stadelman is offline
Registered User
 
Join Date: Jun 2002
Location: Portland oregon area
Posts: 3,738
Steve Stadelman is on a distinguished road
A bandsaw that I like

This will sound absolutely crazy but I have the $189.00 harbor freight bandsaw and it works great.

You need to understand how to adjust the followers and rollers along with blade tension and tracking, but once that is accomplished it works great.

One point that people never get is that new bandsaw blades need to be "broken in".

You can do this by keeping a piece of 2"-3" round stock maybe 6"-8" long handy. When you get a new blade slowly lower the blade into the cut until more than an inch of blade is engaged in the cut. After you cut a slice off of your round store it until next time.

During my machine shop days we kept a piece of 6" cold rolled for this and just sliced off a 1/8 inch wafer every time.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is On
Forum Jump


All times are GMT -5. The time now is 06:31 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.