Casting Boro

Anyone know what it takes to melt boro glass for casting. 1700 lbs worth. CAn you even melt this stuff in a conventional moly furnace? Where would you get batch.

Crazy RFQ that came in.
Reply With Quote
  #2  
Old 05-22-2017, 02:26 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,289
Pete VanderLaan is on a distinguished road
Don't even think about it in your furnace. The crucible is not designed for Boro.There is enormous waste that has to be skimmed. Indeed a moly theoretically can do 2750F in terms of heat generated but your refractories will get even with you.

Boro cullet is being melted at 2380. For the most part it's very seedy stuff and not particularly fluid at 2380. It is melted.

I can refer you to the old boro formula for batch from 1915-1925 when it was being trademarked and patented.

It is also expensive as a cullet. There are lots of boro makers who would likely buy the cullet at well over a dollar a lb. Well over. That's where to make your money.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 05-22-2017, 02:36 PM
Brian Wong Shui Brian Wong Shui is offline
Registered User
 
Join Date: Oct 2002
Location: Atlanta, GA
Posts: 183
Brian Wong Shui is on a distinguished road
Pete, thanks for the facts to put beside the gut instinct to say no.
Reply With Quote
  #4  
Old 05-22-2017, 05:57 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,776
Eben Horton is on a distinguished road
Why boro ?
Reply With Quote
  #5  
Old 05-22-2017, 09:21 PM
Brian Wong Shui Brian Wong Shui is offline
Registered User
 
Join Date: Oct 2002
Location: Atlanta, GA
Posts: 183
Brian Wong Shui is on a distinguished road
No idea. Material was listed on the RFQ for a project. Sometimes I don't want to ask too much. I think that they are trying to do something like....

https://www.youtube.com/watch?v=3JwcKQRdJXA

on a much smaller scale.
Reply With Quote
  #6  
Old 05-23-2017, 06:05 AM
charlie jenkins charlie jenkins is offline
Registered User
 
Join Date: Nov 2015
Location: Dresden Maine
Posts: 36
charlie jenkins is on a distinguished road
Talk to this guy.
http://www.davidruth.com/

Oakland CA artist has (or had 12 years ago) a Boro casting furnace.
Really cool.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 01:30 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.