Mono T 9 replacement

For those of you who actually build furnaces, or make replacement parts and are old enough to remember Mono T 9, this is for you!

Mono T 9 was this indestructible plastic refractory that a lot of us used in the 1970's and '80's. It was withdrawn from the market in 1988 when the clay pit ran out. There was virtually no comparable replacement. For those of you who draw back from the word "plastic", that means unfired clay and you literally pound it into place with either a hammer or a pneumatic device, the latter being preferable. The product fired is indestrucible.

Peiser and I have been going around with each other since after 13 years, Mark's crown has to go and it is so complex that he doesn't think it to be a candidate for castables. We have really been scouring the mines and fields and finally Missouri Refractories company has an intelligent thinking PHD who listens and then responds and he has made a recommendation for a similar mine run about forty five miles from the old site that National refractories was using for the Mono T 9.

Mno T 9 was never particularly high in alumina. It's about 45% and the bulk of the remainder is rotted silica ( AKA Clay) at 48 % or so. It varies in the deposit. There are trace amounts of iron, titanium and alkaline fluxes in the goop, This is true not just of the old stuff but the new stuff is strikingly similar. I had thought that given the geology, there was a great likelyhood of it being just the same.

"Not so" says our Ceramic Engineer at High Temp. He said that even though compound clays can have virtually identical analysis, it doesn't mean squat. What does mean squat is the "modulus of rupture" and in both materials, if you get it good and hot, it gets really strong.

Let me show what that means: In a bonded clay or castable fired to 200F, the modulus is around 200PSI which means it can break pretty easily. From here on, I will look just at the clays. Fire to 2000F, the modulus goes up to about 1000PSI. Fire to 2750F, it jumps to over 1300PSI and once at 2910, it's amazingly over 3000PSI.

Of course the rest of your furnace just melted and went down the drain, so compromise. There is a point here in this educational little tirade and that is to fire your new furnace as hot as you can before actually putting glass in it. This works for gas units and decidedly does not work for small electric kilns which whimper and die tragically. . This is a lot of the reason why you can't make your own crucibles out of greencast 97. You actually probably could if you fired them to 2750F but you can't or don't.

Coming to the endgame here, This material super plastic A looks to be really nice stuff. The plastics have always been very cheap for what they do. Mark and I both recall $16.00 for 100lb box but that was back when we were broiling dinosaur meat on the grill. I can say that they make the best floors you could ever build. Mark is making his crown out of the stuff. Thank You Missouri Refractories Co! You can get their products from High Temp in Fenton Missouri and I wasn't paid a dime for this post. You can also go to :


Missouri Refractories
1198 Mason Circle Drive North
Pevely, MO 63070-1635
(636) 479-7770
(573) 368-7628 cell and sms
(636) 479-7773 fax
bill@morco.us or bill_headrick@hotmail.com personal
morco@morco.us company
http://www.refractories.net/


Learn this stuff. It will save you from eternal ignorance. Tell them all that I sent you.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #2  
Old 08-05-2014, 08:16 PM
Victor Chiarizia Victor Chiarizia is offline
Registered User
 
Join Date: Sep 2005
Location: fairview, NC
Posts: 612
Victor Chiarizia is on a distinguished road
i used low alumina ram for my bread oven. it's suppose to take cycling very well. true for this new ram? and it's name is plastic A? Vic
Reply With Quote
  #3  
Old 08-06-2014, 06:56 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 23,876
Pete VanderLaan is on a distinguished road
Super plastic A. Mark is going to be ordering it I think. I could ask him to get some extra if you want to get it at the same time. It might cut shipping some.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #4  
Old 08-06-2014, 07:52 AM
Victor Chiarizia Victor Chiarizia is offline
Registered User
 
Join Date: Sep 2005
Location: fairview, NC
Posts: 612
Victor Chiarizia is on a distinguished road
not ready yet..think the last plastic was a franco product. i did use mono t 9 on my very first furnace i made. pounding that stuff isn't ez so i bought an air impact and that was the ticket. v
Reply With Quote
  #5  
Old 08-06-2014, 08:08 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 23,876
Pete VanderLaan is on a distinguished road
Smooth it's not. I could rip up my hands on the alumina chunks. It comes in fifty lb boxes with four 12.5 lb slabs about two inches thick.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #6  
Old 08-07-2014, 08:56 AM
Glenn Randle's Avatar
Glenn Randle Glenn Randle is offline
Registered User
 
Join Date: Apr 2002
Location: Boone,NC
Posts: 968
Glenn Randle is on a distinguished road
I remember Mono t-9 coming as either an "air-set" or a "heat set", right? Can't remember which was preferred, but seems like the heat set would have a longer shelf life.

After beating on a crown for hours & hours with a hammer I discovered that Walmart sold air hammers for about $15.... They turn " hard labor" into "play time".
Reply With Quote
  #7  
Old 08-07-2014, 09:00 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 23,876
Pete VanderLaan is on a distinguished road
you can reconstitute the stuff. Just stand an unfired slab in an inch of water and it gradually wicks up the clay. Ultimately, it's all heat set. In sintering materials, essentially the hotter you get it on the first firing , the stronger it will be up to about 2900F in this case. 2500F would make a very strong crown.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #8  
Old 08-07-2014, 12:33 PM
David Hopman David Hopman is offline
Registered User
 
Join Date: Mar 2009
Location: Sutter Creek, CA
Posts: 473
David Hopman is on a distinguished road
The air hammer works pretty well as a mold vibrator too.


Quote:
Originally Posted by Glenn Randle View Post
After beating on a crown for hours & hours with a hammer I discovered that Walmart sold air hammers for about $15.... They turn " hard labor" into "play time".
Reply With Quote
  #9  
Old 08-10-2014, 11:09 AM
Glenn Randle's Avatar
Glenn Randle Glenn Randle is offline
Registered User
 
Join Date: Apr 2002
Location: Boone,NC
Posts: 968
Glenn Randle is on a distinguished road
Quote:
Originally Posted by David Hopman View Post
The air hammer works pretty well as a mold vibrator too.
They are handy tools. I sharpened a cold chisel and used it to carve Locust (super hard wood) like butter. The body panel cutter is a great for cutting metal roofing.

This is one of the rare times when an "el cheapo" tool is great.
Reply With Quote
  #10  
Old 08-11-2014, 06:51 PM
Lowell Duell Lowell Duell is offline
Registered User
 
Join Date: Jan 2006
Location: Glide, Oregon
Posts: 44
Lowell Duell is on a distinguished road
Mono t 9 is great stuff, I must of got the last batch in 1999 used most of it in my furnace but put the rest in a bucket with a lid and forgot about it. Pete, Good thing to know it can be reconstituted, probably dry by now.
Reply With Quote
  #11  
Old 08-21-2014, 06:01 AM
Victor Chiarizia Victor Chiarizia is offline
Registered User
 
Join Date: Sep 2005
Location: fairview, NC
Posts: 612
Victor Chiarizia is on a distinguished road
pete....can i get some of the super plastic. just shut down for maintenance and need to replace a few things. v
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 11:59 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2022, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.