  #351  
Old 09-26-2014, 07:43 AM
Lawrence Duckworth Lawrence Duckworth is offline
Registered User
 
Join Date: Mar 2010
Location: usa
Posts: 685
Lawrence Duckworth is on a distinguished road
just completed the first pot change on the 200lb moly. I found 3 air tubes partially blocked with debris….(no inlet filter at blower)...something to keep an eye on in the future.

also was able to add 20 sq. ft. of insulation to the top

Last edited by Lawrence Duckworth; 02-05-2021 at 05:50 AM.
Reply With Quote
  #352  
Old 09-26-2014, 08:09 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 23,877
Pete VanderLaan is on a distinguished road
The air cooling methodology is pretty flakey. I think that using the copper buss bar for power distribution is better and keeps those things cooler. I am rebuilding mine this fall and expect to find my insulation to be in bad shape as well.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #353  
Old 06-14-2015, 06:33 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 23,877
Pete VanderLaan is on a distinguished road
Thanks Lawrence, I think that really helps. James Burt has bought the 22.5 KW electric package from me and I'm trying to convey how that front plate works. I've advised him to get the plate and then design around it since he wants to bring the 24 inch pot out the front ( What a concept) . Mine, on the 28 inch electric package tilts back a bit on the back of that casting but presents in essentially the same way as yours. That's a great sequence, thank you.

I really will miss my moly.

I'm about to start a medium size gas unit using an 80 lb pot and two 11 inch pots for the time Scott and I will melt enamels if there is an interest.I could use it as a permanent smaller furnace as opposed to the larger one. It will use a recuperation system Charlie Correll is building. I'll do it from the first weld if there is an interest.

Otherwise I'll just build it.
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 03:55 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2022, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.