Kiln tranfering heat down - how to stop?

I have a Paragon fiberfuse 16 in my classroom. The counters in my art room are all fire proof - the heavy black type that would also be used in a chemistry lab - not stone, but some other man made material. I have fired the kiln once and it made the counter top very hot. I was still able to touch it with my glass blowers hands...but the temp has me worried - pyrolysis to the wooden counter base. What can I do to insulate the kiln from the counter top? The kiln comes factory with riser legs and rubber feet. If I set it on a layer of thin fire brick or kiln shelves, it will still radiate heat out to all of that potential thermal mass and still transfer the heat into the counter below it.....
__________________
The revolution will not be televised.
Reply With Quote
  #2  
Old 03-15-2018, 08:05 PM
Ted Trower's Avatar
Ted Trower Ted Trower is offline
Registered User
 
Join Date: Apr 2002
Location: Ann Arbor, Michigan
Posts: 554
Ted Trower is on a distinguished road
If the countertop is truly the same as a chemistry lab then it is likely to be soapstone and very tolerant of high temperature. The wood underneath would be the only concern. As you indicated.
__________________
"It appears to me that glass men are the most given to drunkeness of any class of men I know" Peter Burt, recruiter in Europe, in a letter to Deming Jarves of the Boston and Sandwich glass company. -1826
Reply With Quote
  #3  
Old 03-15-2018, 08:46 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,918
Pete VanderLaan is on a distinguished road
Multiple dead air spaces, try two or three, then stick a probe in there at the bottom. If it's over 135F, it's still too hot.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #4  
Old 03-16-2018, 06:45 AM
Rosanna Gusler Rosanna Gusler is offline
Registered Fuser
 
Join Date: Mar 2003
Location: Wanchese, NC
Posts: 995
Rosanna Gusler is on a distinguished road
Concrete blocks laid on their side make a nice kiln stand. You can store props and stuff in the holes.
Reply With Quote
  #5  
Old 03-16-2018, 11:08 AM
Brian Graham's Avatar
Brian Graham Brian Graham is offline
Registered Abuser
 
Join Date: Mar 2004
Location: Akron - Ohio
Posts: 559
Brian Graham is on a distinguished road
Dead air spaces

Pete - any recommendation on the minimum height for a unit of "dead air space"? I am thinking about using sheets of thin concrete backer board.
__________________
The revolution will not be televised.
Reply With Quote
  #6  
Old 03-16-2018, 01:42 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,918
Pete VanderLaan is on a distinguished road
Make each one an inch, use two. Then feel it out. A lot depends on the firing cycle. If it's continuous it needs more. Aluminum foil on the top one will really help.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #7  
Old 03-16-2018, 01:52 PM
Art Freas Art Freas is offline
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 808
Art Freas is on a distinguished road
I think you are fusing, so if you have 1/4 fiber paper maybe a layer of that under the foil on the top layer. That gives an immediate air layer under the foil limiting the conduction to the feet.
Reply With Quote
  #8  
Old 03-16-2018, 03:40 PM
Brian Graham's Avatar
Brian Graham Brian Graham is offline
Registered Abuser
 
Join Date: Mar 2004
Location: Akron - Ohio
Posts: 559
Brian Graham is on a distinguished road
Thank you for the suggestions. I am guessing shiny side up on the foil to reflect the most heat?
__________________
The revolution will not be televised.
Reply With Quote
  #9  
Old 03-16-2018, 04:40 PM
Sky Campbell's Avatar
Sky Campbell Sky Campbell is offline
Registered User
 
Join Date: May 2002
Location: Gainesville FL
Posts: 1,035
Sky Campbell is on a distinguished road
I might try a couple metal 2x4 studs cut to length and lie them flat. That should provide adequate air space and suport the kiln evenly. Whatever you use its going to be the air space that stops the heat transfer.
Reply With Quote
  #10  
Old 03-16-2018, 06:45 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,918
Pete VanderLaan is on a distinguished road
Brian, just run the thing and monitor what it really does in real time. Then do the corrections, monitor them. Pyrolisis is a slow motion machine based in ambient temps. My take in all the fires I 've looked at is 135F is as high as you want it to get if it's continuous. Other wise, you have to look at the materials.

I'm basing my findings on Weinberg, Chiarizia, Bissett, Keckic and my own studio and bathroom ( which never lit off) and a number of pottery fires which had pyrolitic deterioration along with my dear departed mentor Tom Langhorst's observations from the New Mexico State Fire Marshal's office at whose feet I studied the issue. He taught me to look and think. Rare in the arts. RIP Tom. I miss your wit in the night.

Tom and I were working a fire one night in the south county and we were running the sniffer and there was another guy from the Fire Marshal's office who really wanted to go home.It was around 2:00AM. We didn't like him much as we kicked the crap around just looking and mumbling. Dave asked Tom to tell him the cause and origin which is what we always want to know in an insurance case. We look at checks in the wood, both large and small and follow them. Little check are near the inception, big ones, it's ripping. Tom said "Residual Electricity" . Dave wrote it down and left. We were there another four hours. Dave got fired the next day.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #11  
Old 03-16-2018, 07:54 PM
Art Freas Art Freas is offline
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 808
Art Freas is on a distinguished road
"Residual Electricity"? That's a new one, up there with Douglas Adams' structural exasperation.
Reply With Quote
  #12  
Old 03-17-2018, 08:11 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,918
Pete VanderLaan is on a distinguished road
well maybe in an undischarged capacitor but you don't find them in mobile homes.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #13  
Old 03-17-2018, 10:03 AM
Eben Horton Eben Horton is online now
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,902
Eben Horton is on a distinguished road
Well... if you have let the national enquirer catch your eye in the check out lane at the grocery store, people can just spontaneously combust while chillaxing in their lazy boy recliner... so anything is possible.
__________________
<EBEN EΠOIESEN >
Reply With Quote
  #14  
Old 03-17-2018, 11:11 AM
Rich Samuel's Avatar
Rich Samuel Rich Samuel is offline
Registered User
 
Join Date: Apr 2002
Location: Seattle, WA
Posts: 2,595
Rich Samuel is on a distinguished road
You'll want to install a phlogiston suppressor, too.
Reply With Quote
  #15  
Old 03-17-2018, 12:35 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,918
Pete VanderLaan is on a distinguished road
you can't suppress phlogiston. That was the entire point.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #16  
Old 03-24-2018, 06:53 AM
Brian Graham's Avatar
Brian Graham Brian Graham is offline
Registered Abuser
 
Join Date: Mar 2004
Location: Akron - Ohio
Posts: 559
Brian Graham is on a distinguished road
Here is the kiln base that I came up with - old wall shelf hangers cut to length with a thin piece of hardie backer board attached. The single air space worked at maximum temperature (1500F). Between kiln and hardie board it was 140F - between base and table top it was 115F.
Attached Images
File Type: jpg kiln_base.jpg (28.1 KB, 32 views)
__________________
The revolution will not be televised.
Reply With Quote
  #17  
Old 03-25-2018, 11:42 PM
Art Freas Art Freas is offline
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 808
Art Freas is on a distinguished road
Concept is good, but find something other than the hardieboard. 140 is too hot for that board.
Reply With Quote
  #18  
Old 03-26-2018, 08:18 AM
Sky Campbell's Avatar
Sky Campbell Sky Campbell is offline
Registered User
 
Join Date: May 2002
Location: Gainesville FL
Posts: 1,035
Sky Campbell is on a distinguished road
Quote:
Originally Posted by Art Freas View Post
Concept is good, but find something other than the hardieboard. 140 is too hot for that board.
You might be thinking of some other type of board. Hardie board is cement board. It Will not burn and is well known for using it these type of aplacations. The caveat I see is the free silica the board is made from can be a respiratory hazard. Undisturbed I would think it's just fine.
Reply With Quote
  #19  
Old 03-26-2018, 09:04 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,918
Pete VanderLaan is on a distinguished road
I have used Hardiboard as the outside of a rectangular gloryhole. It lasted ten years and although it did eventually crack, it was never an issue. It's not an insulator but I don't think it's any significant hazard. 115F on the tabletop is not a risk in my mind. Keep in mind it's also periodic.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #20  
Old 03-26-2018, 10:22 AM
Cecil McKenzie Cecil McKenzie is offline
Registered User
 
Join Date: Feb 2011
Location: Emporia, KS
Posts: 503
Cecil McKenzie is on a distinguished road
1 inch of ceramic fiber equals something like 18 inches of hard brick. Put fiber of table top and metal studs flat on top of that.
Reply With Quote
  #21  
Old 03-26-2018, 11:50 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,918
Pete VanderLaan is on a distinguished road
While that's true, it is far more effective at higher performance temperatures than it is in the range Brain is using. Also, it is still obnoxious about fiber release. Brian has lowered the temperature at the hot face of the table to a very reasonable level. That was the goal.
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 04:19 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.