Anybody have a favorite binder or recipe for pate de verre? I'm going to be trying out that process for the first time soon. Some quick googling turned up methyl cellulose and gum arabic as potentially decent options, they both seem nontoxic, water-soluble, and relatively cheap to get a pound or so to play around with.
Reply With Quote
  #2  
Old 05-11-2020, 06:48 PM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is offline
Registered User
 
Join Date: Jan 2007
Location: Charlotte, NC
Posts: 2,239
Greg Vriethoff is on a distinguished road
I use gum arabic. It's such a staple in the fine arts it's good for me to keep some on hand. A multitude of uses.
Reply With Quote
  #3  
Old 05-11-2020, 07:33 PM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 696
Shawn Everette is on a distinguished road
The methyl cellulose is the stuff that they're selling as a "pmc" for glass, so I think it's a bit more elastic. Gum arabic is probably going to set up a bit faster. Any of the glass tacs for fusing should be fine. Elmers would also be an option, but only use the white stuff.
Reply With Quote
  #4  
Old 05-11-2020, 09:55 PM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is offline
Registered User
 
Join Date: Jan 2007
Location: Charlotte, NC
Posts: 2,239
Greg Vriethoff is on a distinguished road
I've used the clear Elmers to hold pieces for fusing. Seemed to burn out well. Does the clear stuff not work for patê de verre?
Reply With Quote
  #5  
Old 05-11-2020, 11:31 PM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 696
Shawn Everette is on a distinguished road
My students have experienced bad results with the "gel", cheap stuff works fine.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 12:43 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.