Devit?

I've been opening some enameled bottles into tall cups. But I keep getting a haze in the glass. See the attached pic of one. I'm guessing this is devitrification.

It happens about half the time; and usually it's visible on the glass within the first couple heats. Washing the bottles with soap and water isn't helping. Should I be using nastier solvents? The last one got the haze on the inside, instead of the outside like this example. What am I missing?
Attached Images
File Type: jpg devit.jpg (28.5 KB, 77 views)
Reply With Quote
  #2  
Old 10-27-2017, 07:55 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 19,557
Pete VanderLaan is on a distinguished road
where is the enamel applied? What is the enamel? What is the base glass?
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 10-27-2017, 09:28 PM
Scott Mitchell Scott Mitchell is offline
Registered User
 
Join Date: Jun 2013
Location: Springfield, VA
Posts: 25
Scott Mitchell is on a distinguished road
It's all commercial glass. I have no idea.
Reply With Quote
  #4  
Old 10-28-2017, 06:29 AM
Rosanna Gusler Rosanna Gusler is offline
Registered Fuser
 
Join Date: Mar 2003
Location: Wanchese, NC
Posts: 885
Rosanna Gusler is on a distinguished road
Be aware that those enamel are not food safe and may contain heavy metals.
Reply With Quote
  #5  
Old 10-30-2017, 12:13 PM
James Ennis James Ennis is offline
Registered User
 
Join Date: Oct 2004
Location: seattle
Posts: 303
James Ennis is on a distinguished road
those might have been sprayed with titanium, they use it to prevent scratching,
i dont know any way to remove it.
Reply With Quote
  #6  
Old 10-31-2017, 10:46 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 19,557
Pete VanderLaan is on a distinguished road
actually, titanium is now a regular additive to enamels for density and whiteness.
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 02:04 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2018, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.