Copper ruby

Ran across this patent, they add a small amount of bismuth oxide to the formula. Anyone try this?

Manufacture of ruby glass
Reply With Quote
  #2  
Old 12-12-2017, 02:49 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,287
Pete VanderLaan is on a distinguished road
It's curious. Bismuth is really a heavy metal right there with lead. It also uses cyanide. It also wants to use stannic, not stannous oxide which is an opacifier and not a reducing agent.

Honestly, I think black tin will yield better results. Bismuth also is not cheap. If anyone tries it, let us know.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 12-12-2017, 05:00 PM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,717
Jordan Kube is on a distinguished road
The boro melters use it, I think. There's some stuff to learn from what they are doing.
__________________
WWUD? Think for yourself.
Reply With Quote
  #4  
Old 12-12-2017, 05:59 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,287
Pete VanderLaan is on a distinguished road
I think it's the zircon. Cyanide? no..
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #5  
Old 08-03-2019, 08:32 AM
Bradley Howes Bradley Howes is offline
Registered User
 
Join Date: Mar 2015
Location: Alfred University
Posts: 62
Bradley Howes is on a distinguished road
Bismuth and cyanide

Quote:
Originally Posted by Pete VanderLaan View Post
It's curious. Bismuth is really a heavy metal right there with lead. It also uses cyanide. It also wants to use stannic, not stannous oxide which is an opacifier and not a reducing agent.

Honestly, I think black tin will yield better results. Bismuth also is not cheap. If anyone tries it, let us know.
This is now definitely on my to do list once I get back to Alfred and can do my GAE work again. My experience with bismuth thus far has been in calcedony. I was taking inspiration from Antonio Neri from ~1660 AD. He used mercury in his calcedony melts. Bismuth and mercury are part of a family defined by Volf that goes to the tune of Hg-Tl-Pb-Bi (80-83 on the periodic table). I made my own bismuth oxide from bismuth metal by reacting it with nitric acid and reducing it to oxide with sodium hydroxide. The amounts I was using though was over the .31 wt.% limit specified in the patent that produces browns and blacks from the formation of bismuth metal particles. (Side note: I once saw a wonderful honey amber orange brown color made from bismuth by one of the Alfred undergrad engineering seniors.) It might be worth revisiting that avenue.

I’m very suspicious of the cyanide. I’ve never used it and I have no idea if it volatilizes from the melt somehow. I also have no idea what role the cyanide plays in the glass. Is it some kind of reducing agent?

Last edited by Bradley Howes; 08-15-2019 at 03:51 PM.
Reply With Quote
  #6  
Old 08-03-2019, 10:50 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,287
Pete VanderLaan is on a distinguished road
well, pick your poison, cyanide or mercury. the presence of arsenic in glass will certainly knock you on your can. Volf declares that Mercury has no role in glass on the one hand and in the other refers to distinct color changes in batches where it's present. I have had it suggested to me that bismuth could replace lead in whole or in part but at that time the price of bismuth was over eight times the price of lead.
Bismuth is certainly used mixed with silver salts to help keep them from oxidizing away as a surface treatment but conditionally in its nitrate form.

I think pursuit of the Neri observations regarding mercury are worth pursuit. Dino Rosin gets really wild chalcedonia effects and he doesn't talk much about his formulations.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #7  
Old 08-11-2019, 03:23 PM
Bradley Howes Bradley Howes is offline
Registered User
 
Join Date: Mar 2015
Location: Alfred University
Posts: 62
Bradley Howes is on a distinguished road
Just by pure chance, I was looking at the index of Weyl for aventurine, I saw a note for Bismuth Oxide, in Ruby Glass pg.343. It wasn't much but Weyl stated lead, bismuth, and tin are all metallophilic, with tin being the most effective (hence its use in ruby glasses). Again, it wasn't much, just another piece in the puzzle.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 06:22 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.