#1
|
|||
|
|||
Bomma and Sp wer compatibility
Has anyone used cane and murrine made with bomma with SP87 wer? Any info would be great. I have used SP and crystalica with out any problems but never bomma. I am always curious other peoples experience.
Thanks Aron |
#2
|
|||
|
|||
You should be fine !
__________________
<eben epoiese> |
#3
|
|||
|
|||
To be safe, do a test by incorporating some of the two (Bomma murrini and SP) in the same small piece. Then try to saw through it with a wet saw after annealing. See what happens. If it saws cleanly, then great, but if not, then no bueno. What color(s) are in the cane could be an additional variable.
__________________
www.jmbglass.com instagram.com/joshbernbaum_glass |
![]() |
Thread Tools | |
Display Modes | |
|
|