Sugar Acid

I was in Denmark talking to a guy about sugar acid. He uses it all the time and feels it is safe but it still scares me.

What do people think... is sugar acid any safer than others? Is acid just just to dangerous for small studios?
Reply With Quote
  #2  
Old 09-10-2017, 05:20 AM
Peter Bowles Peter Bowles is offline
Registered User
 
Join Date: Sep 2002
Location: Breadalbane, Tasmania
Posts: 615
Peter Bowles is on a distinguished road
There is a lot of misinformation about sugar acid in the glass community, I'd be wary of any information offered up however well meaning it is intended.

Ammonium bifluoride still gives ions of HF.

Getting rid of the stuff responsibly once you're done with it might make you rethink the whole thing. Can get very very expensive to dispose of.
Reply With Quote
  #3  
Old 09-10-2017, 07:24 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,098
Pete VanderLaan is on a distinguished road
I had an ammonium bifluoride vat in my old Santa Fe SHop in the early 1980's. At one point I wanted to neutralize that mix and dumped some soda Ash in and it jumped right out of the booth at me and I mean jumped- several feet.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #4  
Old 09-11-2017, 04:53 AM
Mike McCain
Guest
 
Posts: n/a
Exclamation

use at your own risk. if you've really got a hard on for this kind of thing, best either leave it to the cogs... or your own bone marrow.

http://warmglass.com/phpBB3/viewtopic.php?t=4631
....
Don't have the structure, but sugar acid is a mild form of hydrofluoric, used extensively in Oz.
Last edited by Brock on Tue Mar 16, 2004 11:19 pm, edited 1 time in total.
...
Postby Bert Weiss Wed Mar 17, 2004 10:46 am

Mild hydrofluoric will still dissolve your eyeballs, remove the paint from a car, dissolve glass... overexposure can be fatal. It is a wetting solution so once it is on it's way through your skin, water is not an effective diluter.


....

I was taught to use HF with simple safety equipment outdoors, so it is possible. On the other hand, after mastering the technique, I vowed not to do it again. At least not without an OSHA approved acid booth, which is not in the budget any time soon.

...
me<---> quoting me, as I write this, right now

Myself, I've seen HF used casually, via the bucket ( its in a bucket[in Mexico]) system,

and as a staple part of the shop via the bath ( there's a Whole crane, bath, rinse, Re-Rinse dilution, and then professional dispenser... The bath was in a dedicated room the size of your entire shop that,BTW, smelled like nuclear cancer) system.
Neither of which I feel comfortable with as a professional art bum.

Last edited by Mike McCain; 09-11-2017 at 04:57 AM.
Reply With Quote
  #5  
Old 09-19-2017, 09:42 AM
Henry Halem Henry Halem is offline
Registered User
 
Join Date: Apr 2002
Location: Kent, OH
Posts: 1,418
Henry Halem is on a distinguished road
Sugar Acid

Here is the link to Sugar Acid. http://www.glassnotes.com/downloads.html
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 06:06 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2018, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.