Removing glass stuck on blowpipe steel?

Hi, just thinking yesterday while working that it'd be nice to be able to remove some crusty glass that never fully popped-off of one or two of my pipes that were gathered on too deep at one point. (one was an assistant, and the other I take the blame for..) Anyway, it's just an annoyance when rolling on the bench rail as they don't roll smoothly unless I scootch them a bit farther to the right while rolling. So wondering if there's a good way to smooth that area down to steel again (or stainless in this case)? Just to be clear, I'm talking about 4-5" from the head of these pipes. The regular heat/quench cycles have removed most, but there's still this thin coverage of glass that is only an annoyance when rolling on the bench rail. Thanks in advance as always.
__________________
www.jmbglass.com
instagram.com/joshbernbaum_glass
Reply With Quote
  #2  
Old 10-05-2017, 09:49 AM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,240
Eben Horton is on a distinguished road
Rotate it on a belt sander if you have one. 120 belt works well.
Reply With Quote
  #3  
Old 10-05-2017, 06:24 PM
Josh Bernbaum Josh Bernbaum is online now
Registered User
 
Join Date: Feb 2009
Location: Brattleboro, VT
Posts: 548
Josh Bernbaum is on a distinguished road
Ah, sounds like a good idea, thanks Eben.
__________________
www.jmbglass.com
instagram.com/joshbernbaum_glass
Reply With Quote
  #4  
Old 10-05-2017, 09:29 PM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is offline
(((0)))
 
Join Date: Jan 2007
Location: Charlotte, NC
Posts: 1,942
Greg Vriethoff is on a distinguished road
I've had some luck in the past with a wire wheel on a bench grinder. Less aggressive option before moving on to the belt sander.
__________________
"It's such a fine line between stupid and clever." - David St. Hubbins
Reply With Quote
  #5  
Old 10-06-2017, 06:08 AM
Josh Bernbaum Josh Bernbaum is online now
Registered User
 
Join Date: Feb 2009
Location: Brattleboro, VT
Posts: 548
Josh Bernbaum is on a distinguished road
Cool, thanks Greg, I'll try that first.
__________________
www.jmbglass.com
instagram.com/joshbernbaum_glass
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 06:00 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2018, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.