Furnaces, Glory Holes , Burners

Correll Glass Studio
Charlie Correll
66 Hidden Ledge
Conway MA 01341
413-369-4283
413-369-4283 fax
www.correllglass.com
ccorrell@crocker,com

Charlie is a warhorse in Glass and an old friend. He builds very nice furnaces and has tinkered with recuperation systems for years. I like what he puts together and a lot of other people must as well since frequently when I sell a crucible, more often than not, it is for one of Charlies' units. They are all over the northeast US. Check it out.
***************************


Denver Glass Machinery
2800 South Shoshone St
Englewood Co 80110
303-0980
303-781-9067 fax
www.denverglass.com
info@denverglass.com

These guys build Kanthal wire element furnaces. They are the most inexpensive thing out there I think although Thumb may have them beat.
I don't like wire element furnaces since the elements don't last very long. Their replacement elements are expensive and are better purchased from Duralite Inc Their replacement crucibles are better replaced by Engineered Ceramics ( moi!)
There are people who absolutely love these things and get very frosty when I pan them. I respect them and don't get it. So, they sell a lot of them every year so they must be doing something right.
So if you need a glass furnace that sells for about four Grand, give them a call. It's instant gratification. I just can't get excited.
As for the other equipment, I have looked at it but never used it. Maybe someone can give their polishing stuff a product review?
***************************
Hub
690 Route 73
Orwell Vt 05161
802-948 2209
802-9482217 fax
www.hubglass.com
info@www.hubglass.com
HUB builds beautiful equipment. Every thing they do is excellent. Corning actually calls HUB when they want furnaces built. HUB will rent you his forms for casting furnaces if you don't have the cash for the completed product. Great stuff.
**********************
Pine Ridge Enterprises
P.O. Box 121
Paradise CA 95967
Tom Ash
530-877-9793
http://www.prburner.com/
sales@prburner.com

This is the guy who makes the burner that I won't explain to anyone how they are made. You gotta buy one from Tom and cut it up. ( then buy another one when you find out how much trouble you just got into). They are very quiet, sturdy ribbon burners. I like them. For furnaces and gloryholes. Support small businesses.
*********************
Wet Dog Glass
504-286-9529
504-283-9234 FAX
www.@wetdogglass.com
hotstuff@wetdogglass.com
Eddie Bernard
Manufacturers of tank furnaces, pot and invested pot furnaces, gloryholes, pipe warmers. garages, yokes and other stuff. Also handles flame safety equipment. I have not ever dealt with these guys and would welcome a review.
************************

Abell Combustion

Custom designed combustion systems. Control and Safety systems for furnaces and Gloryholes.

www.abellcombustion.com

************************
Reply With Quote
  #2  
Old 05-31-2002, 09:28 PM
Eben Horton Eben Horton is online now
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 2,272
Eben Horton is on a distinguished road
Wet Dog Glass
504-286-9529
504-283-9234 FAX
www.hotstuff@wetdogglass.com
hotstuff@wetdogglass.com
Eddie Bernard
Manufacturers of tank furnaces, pot and invested pot furnaces, gloryholes, pipe warmers. garages, yokes and other stuff. Also handles flame safety equipment. I have not ever dealt with these guys and would welcome a review.

Wet dog is great. Eddie has worked with Fred Metz of Spiral Arts for a few years now. He is an amazing fabricator, and it shows in the equipment he makes. He's also the Shop tech at New Orleans School of Glass.
The correct web aderess is....
www.wetdogglass.com

eben
Reply With Quote
  #3  
Old 05-31-2002, 11:15 PM
Tom Ash Tom Ash is offline
Registered User
 
Join Date: Apr 2002
Location: Northern California
Posts: 5
Tom Ash is on a distinguished road
Eben is right. Eddie builds first rate equipment. I have been doing business with him on and off for several years. When Fred quit making the "Spiral Arts" retention tip, Eddie took over production (with Fred's blessing).

I recently had a chance to visit with Eddie and his wife at their new shop (in New Orleans). They are great people.

If you need expertise in putting together a hot shop in a school or other public setting, Eddie is your man. He is expert in all the safety stuff that will make the "powers that be" happy. (Besides the NO School of Glass, Eddie has also done a lot of work at Tulane University, which, buy the way, has a great hot shop).

I can't say enough good stuff about Eddie.

Tom A

Last edited by Tom Ash; 06-04-2002 at 10:43 PM.
Reply With Quote
  #4  
Old 06-05-2002, 08:58 AM
Mark Wilson's Avatar
Mark Wilson Mark Wilson is offline
Registered User
 
Join Date: Apr 2002
Location: St. Paul, MN
Posts: 360
Mark Wilson is on a distinguished road
Evenheat curcible kilns and annealers

I have been using an Evenheat 1413 curcible kiln for over a year melting glass in a 38# EC crucible. it works great, and runs off of 15 Amps at 220/240 volt. I also have the GT22, which is a front loading annealer from Evenheat. Both kilns are equipped with Rampmaster II digital controlers.

For more information, follow the link to their web site.

http://www.evenheat-kiln.com/

Last edited by Mark Wilson; 06-05-2002 at 09:04 AM.
Reply With Quote
  #5  
Old 01-15-2003, 01:28 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 13,918
Pete VanderLaan is on a distinguished road
Refractories

Hi Temp
2250 North Clark
Fenton MO 63026
Phone 636-677-2200
FAX 636-677-2235
Tom

Home of Morcocast refractories. Tom sells all sorts of stuff and specializes in buying out end runs when large furnaces are being built. His soft brick prices can't be beat on IFB26 and 28's. My favorite thing he sells is Morcocast 95, a 95% alumina castable made up fresh locally in very small quantities. It runs about 65 cents a lb which also makes it very inexpensive. I am about to try the Morocast 99 and will report back.
Reply With Quote
  #6  
Old 02-07-2003, 12:01 AM
Parker Stafford Parker Stafford is offline
Registered User
 
Join Date: Apr 2002
Posts: 254
Parker Stafford is on a distinguished road
Re: Furnaces, Glory Holes , Burners

Quote:
Originally posted by Pete VanderLaan


Denver Glass Machinery
2800 South Shoshone St
Englewood Co 80110
303-0980
303-781-9067 fax
www.denverglass.com
info@denverglass.com

These guys build Kanthal wire element furnaces. They are the most inexpensive thing out there I think although Thumb may have them beat.

So if you need a glass furnace that sells for about four Grand, give them a call. It's instant gratification.
Denver makes three electric units, and they are all invested. One is a 60 lb capacity, the next is the unit I have used for the last 5 yrs, the EF 240 (130 lb capacity), then the larger unit that melts 200 lbs. I have found that the smaller unit runs through elements very quickly due to tight element windings and probably some watt loading issues. The thinking here on the part of the maker is that this is really a unit for the weekend warrior or hobbyist, so element life shouldn't matter too much (it should always matter folks).......except some people interested in using the smaller unit in a production studio find that they are having to change elements on a quarterly basis (I know a couple of people who did this and had to get rid of the unit since it was a bit like trying to get a lawn mower to do the job of a bush hog).

The two larger units don't have near the problems associated with element life. 9 months is not unusual. I recommend using the elements for the 200 lb unit in the 130 lb unit and sizing up the relay and the service at the panel. This will result in quicker melts, and temp rebounds after squeezing or idling. If I start charging at 3:00 p.m., I am finished by about midnight, ready to blow the next day.
Reply With Quote
  #7  
Old 10-24-2004, 12:33 PM
Donovan Brooke's Avatar
Donovan Brooke Donovan Brooke is offline
Registered User
 
Join Date: Sep 2004
Location: Oregon, WI
Posts: 696
Donovan Brooke is on a distinguished road
Re: Re: Furnaces, Glory Holes , Burners

Quote:
Originally posted by Parker Stafford
Denver makes three electric units, and they are all invested.

The two larger units don't have near the problems associated with element life. [snip]

I blew a little with these furnaces and my major gripe was the combination door position and radiant heat blasting at you. Seems like it was a hot gather compared to the other furnaces I've used.

I agree though that the price combined with instant gratification is tempting.

Donovan
Reply With Quote
  #8  
Old 05-24-2005, 01:14 PM
Jay Holden's Avatar
Jay Holden Jay Holden is offline
Registered User
 
Join Date: May 2003
Location: Tyrone,Ny
Posts: 1,173
Jay Holden is on a distinguished road
Refractories

For those of you on the north east coast who need castables including Kast-o-lite 30 and Mizzou.


Refractory Maintenence Corperation,
4524, Rt 104,
Williamson, Ny,
14589

No website.

Ph# 315-589-4441

Kast-o-lite 30 is $31.35 a 55" bag

Mizzou is $29.15 a 55# bag.

Jay.
__________________
"Many of lifes failures are experienced by people who didn't realize how close they were to success when they gave up".

Thomas Edison
Reply With Quote
  #9  
Old 05-24-2005, 01:31 PM
Donovan Brooke's Avatar
Donovan Brooke Donovan Brooke is offline
Registered User
 
Join Date: Sep 2004
Location: Oregon, WI
Posts: 696
Donovan Brooke is on a distinguished road
Just for a comparison, I just paid $28.00 for 55 lb bags of Mizzou at Hi Temp... However, I'm sure that $1.15 can easily be saved in shipping if you are closer to Jay's resource.

Donovan
Reply With Quote
  #10  
Old 05-26-2005, 08:15 PM
Jay Holden's Avatar
Jay Holden Jay Holden is offline
Registered User
 
Join Date: May 2003
Location: Tyrone,Ny
Posts: 1,173
Jay Holden is on a distinguished road
Quote:
Originally posted by Donovan Brooke
Just for a comparison, I just paid $28.00 for 55 lb bags of Mizzou at Hi Temp... However, I'm sure that $1.15 can easily be saved in shipping if you are closer to Jay's resource.

Donovan

For me it's great because it only takes me about 45 min to get there so no shipping.
Jay.
__________________
"Many of lifes failures are experienced by people who didn't realize how close they were to success when they gave up".

Thomas Edison
Reply With Quote
  #11  
Old 01-23-2006, 01:31 PM
katiemoe's Avatar
katiemoe katiemoe is offline
Administrator
 
Join Date: Feb 2002
Posts: 62
katiemoe is on a distinguished road
bump
Reply With Quote
  #12  
Old 06-22-2012, 10:11 PM
David Palmer
Guest
 
Posts: n/a
Hi Pete. There's a new technology for glass blowing, instead of recuperation I opted for heat exchangers in cascade fashion to use all the heat. 6 pieces of gear from 1. 11/2" burner & 20 amps.
http://www.pozible.com/index.php/archive/index/5706
Website coming soon, these are a DIY build, with online support.
Reply With Quote
  #13  
Old 06-26-2012, 05:48 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 13,918
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by David Palmer View Post
Hi Pete. There's a new technology for glass blowing, instead of recuperation I opted for heat exchangers in cascade fashion to use all the heat. 6 pieces of gear from 1. 11/2" burner & 20 amps.
http://www.pozible.com/index.php/archive/index/5706
Website coming soon, these are a DIY build, with online support.
*****************
I would note here that this post is the only one in the thread which is recommended by the guy who made the equipment. The other posts are all recommendations from actual users of the equipment recommended. To me, that's worth noticing.
__________________
Never do anything you wouldn't want to explain to a paramedic.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 04:12 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2013, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.