Spreadsheet additions?

I've just put together a spread sheet for calculating L.E.C. (I know; its a guide not gospel) Is anyone willing to share any additional expansion values for things like strontium, or any other potentially useful ingredients, beyond what's listed in 'Modern Glass Practice' and 'Glass Notes IV'? Or have a suggestion of where to look for such additional values? Thanks in advance.
P.S. the original E&T values were published in 1927 in the Journal of the American Ceramic Society volume 10, pg. 551. It's a well written piece of history.
Reply With Quote
  #2  
Old 11-09-2019, 11:19 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,177
Pete VanderLaan is on a distinguished road
Look at Appen.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 11-09-2019, 10:15 PM
Josh Bernbaum Josh Bernbaum is offline
Registered User
 
Join Date: Feb 2009
Location: Brattleboro, VT
Posts: 716
Josh Bernbaum is on a distinguished road
I think Dave Bross mentioned here somewhere that strontium and barium were very similar on expansion factor. So I've been entering the strontium in the barium line of the spreadsheet. How accurate that is, I'm not sure yet but is what I've been doing on the spreadsheet for these phosphates I'm doing now which have a decent amt. of strontium.
__________________
www.jmbglass.com
instagram.com/joshbernbaum_glass
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 06:31 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.