Mothballing a Molly

I'm taking a break from glass which may turn into full-blown retirement from it or only temporary.

My studio is in a small bank barn with a tendency to be, if anything, more humid than the outside ambient air (if you know bank barns, only one end, the entrance is really above grade).
I don't want the Control panel/transformer to suffer from this humid air (oxidation of contacts etc.) so should I just hang a 25 watt bulb in the control cabinet to chase down the humidity or should I bite the bullet and leave the thing on with the set point somewhere around 100-125 so some heat is generated to reduce humidity in the cabinet?

I expect the mothball period to be roughly 6-7 months and the summers here in Michigan are quite humid.
__________________
Dave Hilty
Reply With Quote
  #2  
Old 04-28-2018, 08:31 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,598
Pete VanderLaan is on a distinguished road
the lightbulb and about a pound of dry rice in a bowl. Check the rice regularly.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 04-28-2018, 09:57 AM
Steve Stadelman Steve Stadelman is offline
Registered User
 
Join Date: Jun 2002
Location: Portland oregon area
Posts: 3,738
Steve Stadelman is on a distinguished road
Quote:
Originally Posted by Pete VanderLaan View Post
the lightbulb and about a pound of dry rice in a bowl. Check the rice regularly.
I agree 100% with this. the transformer can sit without worry.
__________________
If all you wanted to do was express yourself artistically, you should have obtained a field watercolor set and a pad of acid-free paper. You chose a media with INFRASTRUCTURE baby!
Reply With Quote
  #4  
Old 04-28-2018, 10:55 AM
Eben Horton Eben Horton is online now
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,402
Eben Horton is on a distinguished road
I was going to suggest a bunch of silica gel packets and a light bulb.
__________________
<eben epoiese>
Reply With Quote
  #5  
Old 04-28-2018, 11:43 AM
Larry Cazes Larry Cazes is offline
Registered User
 
Join Date: Feb 2006
Location: San Jose, CA
Posts: 872
Larry Cazes is on a distinguished road
All great advice. If you go to a store that sells safes they sell very large desiccant canisters that turn colors based on their saturation level. When it saturates all you have to do it is put it in a low oven for a few hours to re activate it.
Reply With Quote
  #6  
Old 04-28-2018, 12:21 PM
Lowell Duell Lowell Duell is offline
Registered User
 
Join Date: Jan 2006
Location: Glide, Oregon
Posts: 42
Lowell Duell is on a distinguished road
Dri-Z-air.
Reply With Quote
  #7  
Old 04-28-2018, 12:22 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,598
Pete VanderLaan is on a distinguished road
Dave, look for a PM.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #8  
Old 04-28-2018, 02:25 PM
Rich Samuel's Avatar
Rich Samuel Rich Samuel is online now
Registered User
 
Join Date: Apr 2002
Location: Seattle, WA
Posts: 2,402
Rich Samuel is on a distinguished road
Lowell, Dri-Z-Air is great for closets, storage lockers, and the like, but it creates liquid so may not be good near electricity. They can also be a hassle to maintain over time. And then you're always buying more packets, too.
Reply With Quote
  #9  
Old 04-28-2018, 02:51 PM
Jordan Kube Jordan Kube is online now
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,647
Jordan Kube is on a distinguished road
I keep my tools in a suitcase and they tend to sit for months at a time. I put one if these in there and check it every once and awhile:

https://www.amazon.com/Improved-Eva-...D5J3YWFM0XEHSG

Just plug it in to dry it out again.

This is a larger one:

https://www.amazon.com/Improved-Eva-...8WFJPWBRCWR2S9
__________________
WWUD? Think for yourself.
Reply With Quote
  #10  
Old 05-05-2018, 07:55 AM
Dave Hilty's Avatar
Dave Hilty Dave Hilty is online now
Registered User
 
Join Date: Apr 2002
Location: Oxford, MI
Posts: 625
Dave Hilty is on a distinguished road
Thanks guys, all good suggestions!
__________________
Dave Hilty
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 10:54 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.