Copper Blue Phosphate

Hello all, Im a student at Alfred and we have a class taught half by the glass faculty and half by engineering faculty. The main goal is to experiment with coloring glass. I spent the first semester doing 100 gram melts testing basic colors with spruce color base.

This semester Im looking into opals created by Stp and Bone ash. Friend of mine sent me over to this forum, and I really appreciate all the knowledge that is shared. So thank you to everyone! Especially Dave Bross, Jordan Kube, and Pete Vanderlaan. (sorry if i missed someone who also contributed to the phosphate discussions)

Here is my first test in the direction I was looking for. After more testing I hope to melt in our 50 lb crucible, but we can only send it up to 2275 F. Curious if there was anything I could try to lower the melting point of the stp. Would love to mix from scratch but using what is available at school.

Formula is
Melted at 1300 c
%91.5 Sp color base.
%.5 copper oxide
%4 Stp
%4 boric acid

I had to pick up the chunk and strike it before I overlayed it but found the color became more vibrant after annealing for the second time.
Attached Images
File Type: jpg IMG_0755.jpg (29.5 KB, 38 views)
Reply With Quote
  #2  
Old 03-06-2019, 06:28 PM
Jacob Willcox Jacob Willcox is offline
Registered User
 
Join Date: Jan 2019
Location: Tacoma, Wa/Alfred, NY
Posts: 2
Jacob Willcox is on a distinguished road
Heres a few pics after its been blown out.
Attached Images
File Type: jpg IMG_0764 (1).jpg (25.1 KB, 35 views)
File Type: jpg IMG_0757 (1).jpg (23.6 KB, 36 views)
Reply With Quote
  #3  
Old 03-06-2019, 08:10 PM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,659
Jordan Kube is on a distinguished road
Looks great, what's the problem?
__________________
WWUD? Think for yourself.
Reply With Quote
  #4  
Old 03-07-2019, 07:13 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,770
Pete VanderLaan is on a distinguished road
SP Color base does have a lot of calcium in it and it would be better to get it out and replace it with Strontium which can be had from Universal Pigment. As I recall, it has a similar expansion coefficient so it can fit reasonably. .5 copper is a lot of copper given the capacity of the metal to really change the working characteristics of the glass. Gets sloppy fast. Consider the base formula that Dave Bross put out. SP color base has it's limits.
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 06:58 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.