Stopped Stadelman Furnace

On my 300# Stadelman furnace I seem to have lost all power to my control panel...no lights at all. There is still a dim hum from the transformer when I turn it on so I know I have power. Replaced the ice cube fuses and still no power. Electrician coming tomorrow for what thats worth but i would love to get a handle on the situation now. All suggestions welcome
Reply With Quote
  #2  
Old 08-03-2017, 06:42 AM
Peter Bowles Peter Bowles is offline
Registered User
 
Join Date: Sep 2002
Location: Breadalbane, Tasmania
Posts: 621
Peter Bowles is on a distinguished road
tryin to help an aussie out while the rest of the world sleeps...anything in this thread ring any bells?

http://talk.craftweb.com/showthread....ght=loss+power
Reply With Quote
  #3  
Old 08-03-2017, 08:16 AM
Steve Stadelman Steve Stadelman is offline
Registered User
 
Join Date: Jun 2002
Location: Portland oregon area
Posts: 3,737
Steve Stadelman is on a distinguished road
Check the breaker on the circuit that the control panel is plugged/wired into. Check the internal fuses for the controls and later models had a breaker inside the panel as well for control circuitry.
__________________
If all you wanted to do was express yourself artistically, you should have obtained a field watercolor set and a pad of acid-free paper. You chose a media with INFRASTRUCTURE baby!
Reply With Quote
  #4  
Old 08-03-2017, 08:38 AM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,327
Eben Horton is on a distinguished road
I won't give up names but a glass blower was in a panic for a whole month becauae their controller died. They lost thousands of dollars in potential profit from lost production time... finally when the person that they hired to come and install the new co triller that they bought, it was discovered that it was just a popped breaker.

Talk about a face palm moment.
Reply With Quote
  #5  
Old 08-03-2017, 09:55 AM
Scott Novota's Avatar
Scott Novota Scott Novota is offline
AbbyNormal User
 
Join Date: Jan 2004
Location: Pensacola Florida
Posts: 2,104
Scott Novota is on a distinguished road
I had this happen to me on my ST-Moly last month.

Checked all the breakers in line to the furnace. All good.

Went home and got my multi-meter and started to check each fuse. Three of the smaller fuses and the 60amp fuse had also blown. You could not visually inspect them and tell the difference.

I suspect power outage from a thunderstorm and then the power popping back on caused the fuses to all go at the same time but did not clip my breaker. That breaker has since been replaced as well just because I no longer trust it.

I had about dozen spare small fuses and 2 of the 60amp fuses on the shelf so I was back in business. Hope it is something simple like that.

Last edited by Scott Novota; 08-03-2017 at 11:25 AM.
Reply With Quote
  #6  
Old 08-03-2017, 10:12 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,320
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Eben Horton View Post
I won't give up names but a glass blower was in a panic for a whole month becauae their controller died. They lost thousands of dollars in potential profit from lost production time... finally when the person that they hired to come and install the new co triller that they bought, it was discovered that it was just a popped breaker.

Talk about a face palm moment.
*******
Occam's razor
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #7  
Old 08-03-2017, 11:12 AM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,621
Jordan Kube is on a distinguished road
Not to beat the breaker thing to death but I just last week went over to troubleshoot my friend's moly furnace and it was indeed the breaker. Opened and closed the breaker two more times and it worked. We got it coming up on schedule and he is going to replace the breaker.
__________________
WWUD? Think for yourself.
Reply With Quote
  #8  
Old 08-03-2017, 11:43 AM
John Riepma John Riepma is offline
Registered User
 
Join Date: Apr 2003
Location: Grand Haven, MI
Posts: 478
John Riepma is on a distinguished road
I've heard recommendations about "exercising" circuit breakers by turning them off and then back on at least once a year. This is meant to ensure that that breaker isn't locked in the "On" position by any oxidation that may in fact increase it's duty rating. I've also heard that switching a breaker on and off too many times can damage it, but it's hard to imagine that they aren't meant for at least occasional switching. Some electrician forums even recommend changing breakers out every 20 years. You can look this up on the Googles.

I turn my furnace off at least twice a year at the breaker and have not experienced any fuses blowing. I have had semiconductor fuses blow on the Watlow Din-A-Mite that could be tracked back to a loosened element lead.
Reply With Quote
  #9  
Old 08-03-2017, 02:35 PM
Art Freas Art Freas is offline
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 495
Art Freas is on a distinguished road
I had to replace a breaker last year on my annealer. One of the symptoms was that even when it was working it was hotter than the other breaker running the same load.
Reply With Quote
  #10  
Old 08-03-2017, 06:26 PM
David Russell David Russell is offline
Registered User
 
Join Date: Jul 2008
Location: South Carolina
Posts: 198
David Russell is on a distinguished road
Never ignore the faint smell of burning plastic
Reply With Quote
  #11  
Old 08-05-2017, 03:42 PM
Steve Stadelman Steve Stadelman is offline
Registered User
 
Join Date: Jun 2002
Location: Portland oregon area
Posts: 3,737
Steve Stadelman is on a distinguished road
Follow up and feedback on this Tim?
__________________
If all you wanted to do was express yourself artistically, you should have obtained a field watercolor set and a pad of acid-free paper. You chose a media with INFRASTRUCTURE baby!
Reply With Quote
  #12  
Old 08-05-2017, 06:55 PM
Tim Bassett Tim Bassett is offline
Registered User
 
Join Date: Jun 2006
Location: melbourne australia
Posts: 76
Tim Bassett is on a distinguished road
All the fuses in the control panel were good. Located blown fuse at the transformer which is inside its own cabinet underneath the control panel. We lost one day of production waiting for the glass to come back up to working temp but at least now all my canes and stringers have been colour coded.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 03:38 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2018, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.