CraftWEB Hot Glass Talk  

Go Back   CraftWEB Hot Glass Talk > Hot Glass > General Hot Glass Discussion

Reply
 
Thread Tools Display Modes
  #1  
Old 01-28-2020, 06:45 AM
Victor Chiarizia Victor Chiarizia is offline
Registered User
 
Join Date: Sep 2005
Location: fairview, NC
Posts: 568
Victor Chiarizia is on a distinguished road
drying castables

i'm casting a new burner and gas forge and want to speed the drying of the econocast. parts are up tp 4" thick. is there a recommended temp and time to dry the parts before use?

i suppose it would be below the 212deg boil point of water. vic
Reply With Quote
  #2  
Old 01-28-2020, 08:24 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,648
Pete VanderLaan is on a distinguished road
You don't say how physically big the thing is Vic, but when I want to dry such things as crowns or gloryhole doors, I put the thing in a cardboard box with a 60-100 watt lightbulb for a number of days. The closed box usually gets up to about 140-150F which works well. If it's big enough, it might take two bulbs.

Don't let the lightbulb touch the box.
You may still have to drive off chemically bound water so when you fire it, use a bench torch to heat at first.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 01-28-2020, 02:50 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,603
Eben Horton is on a distinguished road
I slide doors under my furnace to dry over a week ... works great
__________________
<eben epoiese>
Reply With Quote
  #4  
Old 01-29-2020, 09:22 AM
Victor Chiarizia Victor Chiarizia is offline
Registered User
 
Join Date: Sep 2005
Location: fairview, NC
Posts: 568
Victor Chiarizia is on a distinguished road
i think ill just stick them in the annealer at ~ 150 for a while 1-2 days then give them a slow firing when the unit is put together. slow fluffy flame for another day. v
Reply With Quote
  #5  
Old 01-29-2020, 02:00 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,603
Eben Horton is on a distinguished road
Can’t wait to see what you make with the forge Vic!!
__________________
<eben epoiese>
Reply With Quote
  #6  
Old 01-29-2020, 04:24 PM
Victor Chiarizia Victor Chiarizia is offline
Registered User
 
Join Date: Sep 2005
Location: fairview, NC
Posts: 568
Victor Chiarizia is on a distinguished road
damascus kitchen knives and wrought copper/bronze sculpture and lighting. v
Reply With Quote
  #7  
Old 01-29-2020, 10:43 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,603
Eben Horton is on a distinguished road
Nice. Don’t forget the cheese knives
__________________
<eben epoiese>
Reply With Quote
  #8  
Old 01-30-2020, 02:11 PM
Larry Cazes Larry Cazes is offline
Registered User
 
Join Date: Feb 2006
Location: San Jose, CA
Posts: 958
Larry Cazes is on a distinguished road
Blacksmithing is the new go to for established glass artists it seems.
Reply With Quote
  #9  
Old 02-02-2020, 09:06 AM
Lawrence Duckworth Lawrence Duckworth is offline
Registered User
 
Join Date: Mar 2010
Location: Gainesville, GA
Posts: 669
Lawrence Duckworth is on a distinguished road
I’ve got a big blue power hammer and a 42”x8” gas forge that would make a good setup for those extra long Damascus kitchen knives......
They don’t get used much anymore......

4 set of dies

Last edited by Lawrence Duckworth; 02-02-2020 at 09:08 AM.
Reply With Quote
  #10  
Old 02-02-2020, 09:07 AM
Lawrence Duckworth Lawrence Duckworth is offline
Registered User
 
Join Date: Mar 2010
Location: Gainesville, GA
Posts: 669
Lawrence Duckworth is on a distinguished road
......Just saying 👍
Reply With Quote
  #11  
Old 02-02-2020, 09:15 AM
Victor Chiarizia Victor Chiarizia is offline
Registered User
 
Join Date: Sep 2005
Location: fairview, NC
Posts: 568
Victor Chiarizia is on a distinguished road
mighty big forge. mine is 16x8x6.
built a 24ton press, have an anyang 15kilo hammer and upgraded my lathe, bridgeport and band saw.

glass and metals has always fascinated me so we'll see where this all goes.
i'm with pete and let the exploration continue!

fyi i took 12 years off from sculpture to build my house and now that it's finished i can spend more time having fun' and pete i'm doing my first bourbon runs starting today. trying to get 4-5 10gallon kegs filled in the next 4 or so months.
Reply With Quote
  #12  
Old 02-02-2020, 09:32 AM
Lawrence Duckworth Lawrence Duckworth is offline
Registered User
 
Join Date: Mar 2010
Location: Gainesville, GA
Posts: 669
Lawrence Duckworth is on a distinguished road
How bout a cnc plasma table...��

Need to here more about the bourbon.....are you making it?

Last edited by Lawrence Duckworth; 02-02-2020 at 09:37 AM.
Reply With Quote
  #13  
Old 02-02-2020, 03:31 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,648
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Lawrence Duckworth View Post
How bout a cnc plasma table...��

Need to here more about the bourbon.....are you making it?
***
We both make it. I do single malts.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #14  
Old 02-03-2020, 08:04 AM
Victor Chiarizia Victor Chiarizia is offline
Registered User
 
Join Date: Sep 2005
Location: fairview, NC
Posts: 568
Victor Chiarizia is on a distinguished road
im a corn/rye/malt kind of guy. v
Reply With Quote
  #15  
Old 02-03-2020, 05:47 PM
Lawrence Duckworth Lawrence Duckworth is offline
Registered User
 
Join Date: Mar 2010
Location: Gainesville, GA
Posts: 669
Lawrence Duckworth is on a distinguished road
Here in the foot hills of n.e.ga. they call homemade corn whiskey “Moonshine” or “white lightning”......
I was a little reluctant at first to try some of it, especially the peach flavored.


Here’s a tune you guys might want to listen to while making your stuff. Seriously, it’s a good song, one of my favorites.

https://m.youtube.com/watch?v=yQY1TtqVhxQ
Reply With Quote
  #16  
Old 02-03-2020, 07:19 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,648
Pete VanderLaan is on a distinguished road
"White lightning", because it was never aged in a charred oak barrel which gives color to it. White is really raw.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #17  
Old 02-07-2020, 02:58 PM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is offline
rEgisturd Spelunker
 
Join Date: Jan 2007
Location: USSA
Posts: 2,149
Greg Vriethoff is on a distinguished road
This song always jumps to mind for me whenever the subject comes up:

https://youtu.be/4y8fMHJ0zt0
__________________
I loves Dale gilhooly
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 02:46 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.