Bomma - melting recommendations?

We've decided to give Bomma Cullet a whirl.

Does anyone have any recommendations for melting it in a Stadelman-style 300 lb. moly furnace?

Bomma's datasheet recommends a melting temp of between 2282 to 2336.

I know each furnace is different, just seeking advice if anyone has a similar setup.

Thanks,

Dana Smith
Reply With Quote
  #2  
Old 01-31-2020, 12:36 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,647
Pete VanderLaan is on a distinguished road
That sounds good. Bomma is not a borax base cullet. It needs that heat.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 01-31-2020, 02:24 PM
Shawn Everette Shawn Everette is online now
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 487
Shawn Everette is on a distinguished road
I melt and use at 2100 in a wet dog natural. I've got 1.5-2 hours between charges and 12-16 hours after last charge before use. Doesn't fit everyone's schedule, but it can be done lower.
Reply With Quote
  #4  
Old 01-31-2020, 03:11 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,647
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Shawn Everette View Post
I melt and use at 2100 in a wet dog natural. I've got 1.5-2 hours between charges and 12-16 hours after last charge before use. Doesn't fit everyone's schedule, but it can be done lower.
****
I thought you weren't using the Bomma yet.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #5  
Old 01-31-2020, 04:26 PM
Eric Trulson Eric Trulson is offline
Young Turk
 
Join Date: Sep 2014
Location: Boston
Posts: 118
Eric Trulson is on a distinguished road
Quote:
Originally Posted by Shawn Everette View Post
I melt and use at 2100 in a wet dog natural. I've got 1.5-2 hours between charges and 12-16 hours after last charge before use. Doesn't fit everyone's schedule, but it can be done lower.
Seconding this approximate schedule in a canned heat 200# furnace. My friend's shop has been using Bomma for much of the past year. He just charges at working temp (2080F), waits about an hour and a half between charges, and leaves it overnight after the last charge. Sometimes still has a few small bubbles left the next morning, but it generally fines out before the end of the day.
Reply With Quote
  #6  
Old 01-31-2020, 06:45 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,647
Pete VanderLaan is on a distinguished road
I've done this sort of schedule and agree that the fining goes well, but running a good deal hotter seems to yield up a different glass when it comes to cording. Is that being considered?
It seems OK on small work but not on deep dives.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #7  
Old 02-01-2020, 12:17 PM
Dana Smith Dana Smith is offline
Registered User
 
Join Date: Dec 2008
Location: Carrboro, NC
Posts: 12
Dana Smith is on a distinguished road
Pete,

Novice question - are you implying that you would expect more cords or less cords at the higher temps?
Reply With Quote
  #8  
Old 02-01-2020, 02:18 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,647
Pete VanderLaan is on a distinguished road
well, if you get way too hot, more cords as the pot dissolves. Then, looking at the other end, cords when melted way too cold as a glass not well stirred.

I'm more comfortable with the hotter melt than the cold one but it's clearly an economic consideration. With the Bomma, 2300F is not too hot if it has 8 hours to cook after the last charge. It would be more aggressive on the pot but would make bettter glass. It depends on whether you need better glass.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #9  
Old 02-03-2020, 10:46 AM
Shawn Everette Shawn Everette is online now
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 487
Shawn Everette is on a distinguished road
Nope I'm on it, have been since about October. Done a couple posts about it.
Reply With Quote
  #10  
Old 02-03-2020, 10:49 AM
Shawn Everette Shawn Everette is online now
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 487
Shawn Everette is on a distinguished road
I'v tended to notice no cords until you are actually scraping the bottom with most cullets and my method. I've had pots sit for a considerable amount of time that were cord free. I tend to think that cooking it hotter promotes the cords as it bakes off some of the fluxes.
Reply With Quote
  #11  
Old 02-03-2020, 10:59 AM
Dana Smith Dana Smith is offline
Registered User
 
Join Date: Dec 2008
Location: Carrboro, NC
Posts: 12
Dana Smith is on a distinguished road
Shawn - Are you using the whole tank before melting any additional glass or are you "topping off" the tank nightly/as needed?

The Bomma notes state:

"When using Bomma Cullet continuously, it is recommended to charge again when there is a minimum of 1/3 of the furnace capacity remaining."

If I am interpreting that correctly, that seems to be saying that they don't recommend letting your tank go below 1/3 full.
Reply With Quote
  #12  
Old 02-03-2020, 11:21 AM
Shawn Everette Shawn Everette is online now
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 487
Shawn Everette is on a distinguished road
With our charging availability we're generally getting to about half a tank these days, charging about every 3-4 days. We used to charge once a week, and the only difference I noticed was the amount of complaining from people that don't want to gather out of a low tank.
Reply With Quote
  #13  
Old 02-03-2020, 12:43 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,647
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Shawn Everette View Post
I'v tended to notice no cords until you are actually scraping the bottom with most cullets and my method. I've had pots sit for a considerable amount of time that were cord free. I tend to think that cooking it hotter promotes the cords as it bakes off some of the fluxes.
****
I tend to think differently. I think the glass feels a bit shorter because alumina is sloughing off into the melt and that makes a stiffer glass. It's a funny call with methodology. You can do something one way, and for a while it works great. Then it stops working. I don't know why that is.

In castings, there's always some difficult getting the glass to run down into the very thinnest spots. I think the glass rolls over the alumina mold and gets stiffer from it. Mark thinks I have a good point. In mine, I'm going to try painting a bit of lithium carb onto the thinnest spots to see if the skids can be greased with fluxes.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #14  
Old 02-03-2020, 01:25 PM
Shawn Everette Shawn Everette is online now
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 487
Shawn Everette is on a distinguished road
How thin are you trying to go? You may have a solution with the added flux in the mold, pesky surface tension. Generic rule of thumb for most of the classroom situations was to not try and cast thinner than 1/8".
Reply With Quote
  #15  
Old 02-03-2020, 02:32 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,647
Pete VanderLaan is on a distinguished road
Coming out of Liuli Gongfang, Mr Bai was doing some stuff that defies all the conventions. Dan Clayman and I were talking about it as an issue but I think it can be done. What you can't do is to stick to the commercially available cullets.For casting, they pretty much all suck. The conventional mold materials contribute to the problem. Surface tension is one thing, viscosity is another. I'm learning fast. You need to make your own goop.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #16  
Old 02-03-2020, 02:48 PM
Shawn Everette Shawn Everette is online now
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 487
Shawn Everette is on a distinguished road
I'm curious about the Gaffer goop. It's anneal temp is so low that I'd think it have a low viscosity/surface tension in normal casting conditions. BE is really a fusers glass, but it gets real thin past a certain heat threshold. I think it'd sand cast beautifully, if it wasn't so yellow.

Normal molds really don't help things in terms of flow, and I don't really know of anyone doing anything that ground breaking. It's gotta stick to the mold, but not the glass, and that's a big order to fill. The boron nitride spray has been real hit or miss for me, but some people swear buy it.
Reply With Quote
  #17  
Old 02-03-2020, 03:28 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,647
Pete VanderLaan is on a distinguished road
Omce it gets to the terminal point in the mold, it will back up as long as the sprews are right. In China, I saw stuff as thin as the harvard flowers.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #18  
Old 02-03-2020, 04:09 PM
Shawn Everette Shawn Everette is online now
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 487
Shawn Everette is on a distinguished road
That is the theory, but most glasses I've used weren't ever brought to temperatures that would thin out enough to move up the sprew. When things when thermo nuke and the mold failed, it would flow into the thinnest flashing without fail.
Reply With Quote
  #19  
Old 02-03-2020, 04:39 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,647
Pete VanderLaan is on a distinguished road
the point of what I'm suggesting is to change the glass itself, midstream. If one uses the commercial glasses available, it won't happen.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #20  
Old 02-03-2020, 06:18 PM
Larry Cazes Larry Cazes is offline
Registered User
 
Join Date: Feb 2006
Location: San Jose, CA
Posts: 958
Larry Cazes is on a distinguished road
Quote:
Originally Posted by Pete VanderLaan View Post
****
It's a funny call with methodology. You can do something one way, and for a while it works great. Then it stops working. I don't know why that is.
I tend to think thats just the world telling you that you really didn't understand why you were using a particular methodology over others.
Reply With Quote
  #21  
Old 02-03-2020, 07:17 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,647
Pete VanderLaan is on a distinguished road
or... something changed in the formula, or the mine run. They don't tell you that either.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #22  
Old 02-14-2020, 12:36 PM
Pringle Teetor's Avatar
Pringle Teetor Pringle Teetor is online now
Registered User
 
Join Date: Jul 2003
Location: Chapel Hill, NC
Posts: 649
Pringle Teetor is on a distinguished road
Nothing but seeds.
Reply With Quote
  #23  
Old 02-14-2020, 12:49 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,647
Pete VanderLaan is on a distinguished road
I am assuming you saw my PM to you.
Tell me how you melted, blah blah blah...

I've had a lot of conversations with a lot of people over the last few days on this and I'm hearing some doing fine, others having nothing but cords. One indicated they are doing fine melting at 2100F but topping up the pot when half full. Others, nothing helps at all.
What was most disquieting was the observation that sometimes it looked great, then a later load would actually be short and cordy. I think beginning to nail down batch runs from the pallets may suggest something new. Both SP and Olympic have had these issues. Charlie Parriot is substantially more distant from this process than I expected he would be. I am a lot less certain that the cullet wars/shortages are over. Cristalica continues to go down and from my understanding, the furnace is shot with no plans to rebuild. Writing a formula isn't really all that difficult but proper mixing and melting consistently require diligence. It would be ironic if Oceanside was left as last man standing with sys96, a cullet incompatible with a fair amount of color when last produced.

Spruce Pine 87 is looking far more attractive today than anything else at .81 lb. I don't really know why there are so many objections to a pelletized batch that is so reliable. It's not really dusty. Mine? Mine is more dusty and I just throw on a respirator.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #24  
Old 02-14-2020, 06:39 PM
Pringle Teetor's Avatar
Pringle Teetor Pringle Teetor is online now
Registered User
 
Join Date: Jul 2003
Location: Chapel Hill, NC
Posts: 649
Pringle Teetor is on a distinguished road
we've melted at 2100, 90 minutes between scoops - seeds. People said melt hotter and longer. Did that - waited 90 minutes between scoops (cooked @2285 for 9 hours), still seeds. trying a squeeze today and will check in the morning but not holding my breath. Only charging 1/2 pot. Stad moly furnace 250 lb crucible. I did blow a clear piece with a thick bottom and yes, there were cords.

has anyone seen seeds seeds this bad in bomma?
Attached Images
File Type: jpg IMG_9831.jpg (25.8 KB, 16 views)
Reply With Quote
  #25  
Old 02-14-2020, 10:39 PM
Shawn Everette Shawn Everette is online now
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 487
Shawn Everette is on a distinguished road
General rule of thumb is electric takes longer. When I was running electric, it was a minimum of 3 hours between charges, they just take longer to regenerate the heat. On my WD gas it's less than 20 minutes, on my old stad moly it was over an hour back to temp.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 01:52 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.