Study of bone ash

Not all bone ashes are created equal.

Someone is doing a study to determine if the bone ash obtained from grass-fed cows makes a better porcelain. Apparently, it does.

https://www.fastcompany.com/90460845...aGosC0_LUcKaKg
__________________
I loves Dale gilhooly
Reply With Quote
  #2  
Old 02-08-2020, 07:00 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,648
Pete VanderLaan is on a distinguished road
Bone ash has always been flakey. The bone ash we all loved in 1970 was called bone ash 21, a rather greasy material that indeed did make a beautiful opal if you could get the mess hot enough to not cause stones. Once it was gone it was gone and Calcium polyphosphates were the only thing available. They never worked for me once.

Mark Peiser has persisted in finding calcium monophosphate but good luck locating it. If one uses strontium as a substitute for calcium as much as possible, it certainly performs better and strikes best on re annealing.

As to the "whole Cow" being used. I'm sure it's thrilled.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 02-10-2020, 05:43 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,603
Eben Horton is on a distinguished road
Well shit. I canít call my glass vegan if I use bone ash.
__________________
<eben epoiese>
Reply With Quote
  #4  
Old 02-10-2020, 06:25 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,648
Pete VanderLaan is on a distinguished road
just use the synthetic.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #5  
Old 02-10-2020, 06:31 PM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,704
Jordan Kube is on a distinguished road
Batch composition seems to me to be the biggest factor when using a similar phosphate sources. When using STPP in Dave's formula I get a "long" striking result. So gorgeous and beautiful in big solid sections like the old Daum and Lalique stuff. Terrible for goblets. STPP added to Spruce Pine gives a lovely quick striking glass that is great for cups. They are pretty different formulas.
__________________
WWUD? Think for yourself.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 02:16 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.