Coating cast glass

I've heard and/or read about coating castings (Gaffer in this case), especially after sandblasting to protect from finger prints, oils, and what not. Obviously there's Liquid Lust'er and I've had a thin coating of Hextal suggested. Years back I read on this forum (I believe) of a common clear bathroom sealant being used.

While I may take my current casting to a polish, I'm interested to hear others experiences, whats good and what not.
Reply With Quote
  #2  
Old 03-21-2020, 09:27 AM
Eric Trulson Eric Trulson is offline
Young Turk
 
Join Date: Sep 2014
Location: Stanwood, WA
Posts: 137
Eric Trulson is on a distinguished road
I've been playing around with a new (for me) substance, Liquin. It's a lacquer-type outer coating for oil paintings, a lot of online art suppliers stock it.

Has worked well so far the handful of times I've used it on sandblasted glass pieces, but it needs to be applied carefully - I messed up one piece by trying to use a paper towel to wipe off some excess and getting little paper particles stuck on the surface (Going to need to re-sandblast that piece to fix it).

Going forward I am planning to heat up the liquin a bit in a double boiler beforehand to thin it out, and use a soft brush to apply it, to try and get a more even coverage


Edit: Link to another useful thread on this topic from 2011 that Dave unearthed: Sandblasted surface coatings

Last edited by Eric Trulson; 03-22-2020 at 08:10 AM.
Reply With Quote
  #3  
Old 03-21-2020, 08:38 PM
Dave Bowers's Avatar
Dave Bowers Dave Bowers is offline
Registered User
 
Join Date: Feb 2010
Location: Pataskala, OH
Posts: 7
Dave Bowers is on a distinguished road
After figuring out the right search terms, I found the thread from 2011 under "Sandblasted surface coatings".
Reply With Quote
  #4  
Old 03-23-2020, 09:03 AM
Shawn Everette Shawn Everette is online now
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 617
Shawn Everette is on a distinguished road
Here ya go, https://www.bullseyeglass.com/method...?articleid=766 .

Bought it, but have yet to use it. Personally I like Hxtal thinned with acetone and air bushed. It's kind of a huge pain, but the results are perminant.
Reply With Quote
  #5  
Old 03-23-2020, 11:45 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,034
Pete VanderLaan is on a distinguished road
Air spraying Hxtal gives me the willies. Only do that with superb ventilation. If I say what I really think, I hear from their lawyer.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #6  
Old 03-23-2020, 12:30 PM
Shawn Everette Shawn Everette is online now
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 617
Shawn Everette is on a distinguished road
Agreed. I haven't done it in some time, but always under a hood and with a respirator. You can apply thinned by brush and still get a lot of detail, but spraying lets you retain the blasted texture, if that's what you're after.
Reply With Quote
  #7  
Old 03-23-2020, 01:07 PM
Marty Kremer Marty Kremer is offline
Registered User
 
Join Date: May 2004
Location: North Yarmouth ME
Posts: 501
Marty Kremer is on a distinguished road
Quote:
Originally Posted by Shawn Everette View Post
Here ya go, https://www.bullseyeglass.com/method...?articleid=766 .

Bought it, but have yet to use it. Personally I like Hxtal thinned with acetone and air bushed. It's kind of a huge pain, but the results are perminant.
I use it all the time on sandblasted bullseye. Good stuff. And surprisingly, BE's price is ok.
Reply With Quote
  #8  
Old 03-23-2020, 08:10 PM
Nick Delmatto Nick Delmatto is offline
Registered User
 
Join Date: Feb 2010
Location: Logan, OH
Posts: 55
Nick Delmatto is on a distinguished road
Has the Clean Shield withstood the test of time? How old is it?
Reply With Quote
  #9  
Old 03-23-2020, 09:42 PM
Marty Kremer Marty Kremer is offline
Registered User
 
Join Date: May 2004
Location: North Yarmouth ME
Posts: 501
Marty Kremer is on a distinguished road
If you're talking about shelf life, I don't know.
It's not permanent. I'd say it's good for a couple of years before needing another application (but that's a guess).
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 02:44 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.