Hot torch knobs

Is it ok if my torch knob get warm.
Hope it does not explode
Franklin
Attached Images
File Type: jpg 3BDEFB17-2749-4DE7-A5EC-C9B3D2F19614.jpg (31.7 KB, 28 views)
Reply With Quote
  #2  
Old 06-17-2020, 06:45 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 4,001
Franklin Sankar is on a distinguished road
Sorry, not only the knobs but the body of the torch. Also the knobs are really levers. An oLd torch used for scientific framework.
Thanks
Franklin
Reply With Quote
  #3  
Old 06-18-2020, 09:27 AM
Tom Fuhrman Tom Fuhrman is offline
Registered User
 
Join Date: Apr 2002
Location: hills of Tennessee
Posts: 1,449
Tom Fuhrman is on a distinguished road
that torch may have been designed for natural gas and not propane so it may be running hotter than it was designed to run. you may have to see if you can change the orifice.
Reply With Quote
  #4  
Old 06-18-2020, 10:25 AM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 4,001
Franklin Sankar is on a distinguished road
Can I run it like that . Would it be dangerous.
Franklin
Reply With Quote
  #5  
Old 06-18-2020, 10:31 AM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 4,001
Franklin Sankar is on a distinguished road
Running it out of spec is not recommended but glassblower’s work on the edge so I am not worried
Franklin
Reply With Quote
  #6  
Old 06-18-2020, 10:37 AM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 4,001
Franklin Sankar is on a distinguished road
Tom the older you get the wiser you get. It may be nat gas. You are right.
It’s a beautiful torch. No nat gas here.
Franklin
Reply With Quote
  #7  
Old 06-18-2020, 11:37 AM
Larry Cazes Larry Cazes is offline
Registered User
 
Join Date: Feb 2006
Location: San Jose, CA
Posts: 997
Larry Cazes is on a distinguished road
Quote:
Originally Posted by Franklin Sankar View Post
Running it out of spec is not recommended but glassblower’s work on the edge so I am not worried
Franklin
Of course it depends on how hot but in general it is NOT a good idea.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 12:40 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.